1 July 2012 in Russian Metallurgy (Metally)
The formation of nickel and iron nanoparticles produced by a chemical—metallurgical method and steels made of composite iron powders with nanosized nickel additions is studied. A procedure is...
30 May 2022 in Inorganic Materials: Applied Research
The influence of various schemes of pressure treatment (pressing, rolling) and modes of heat treatment of powder mixtures on the service properties and adhesion strength of the working and current-carrying layers of electrical contacts with a conductivity of at least 75% of the copper conductivity was studied. The dependence of the permissible fraction of the working layer in the total contact thickness on its resistivity was established. It was calculated that, in the created contacts, the thickness of the working layer of two compositions 97% Cu + 1% CA + 2% PA (1) and 97.5% Cu + 1% CA + 0.5% PA + 1% Al2O3 (2), with the electrical resistivity of 3.20 and 3.28 μΩ cm, respectively, can be increased to the thickness of the copper layer (here, CA is activated carbon; PA is a (Fe–Cu) nanocrystalline pseudoalloy). Among the considered processes, we determined the optimum method to fabricate contacts that consists of combined rolling with a reduction of 50% of copper powder and the powder mixture for the working layer using the metering hoppers separated for the charge of each layer, reducing sintering at 600°C for 1 h, and re-compacting rolling with strain of 85% and sintering at 800°С for 1 h. This technique was used to obtain samples of contacts with working layers of two compositions with a relative density of 0.99 and 0.98, hardness HB of 990 and 830 MPa, and electrical resistivity of 2.57 and 2.61 μΩ cm, respectively. The adhesion strength of contact layers is more than 200 MPa (breaking stress for copper).
1 September 2016 in Metallurgist
1 January 2017 in AIP Conference Proceedings
Aluminium, copper and their compounds are used in common as basis for antifriction coatings of plain bearings. Antifriction testing of plain bearings (based on Al and Cu) made by leading automotive manufacturers from Germany, Japan, USA, United Kingdom and Russia were carried out to make judicious selection of basis for development of new antifriction material. Testing was carried out using friction machine. It was defined that materials based on Cu provide better durability and robustness of plain bearings in comparison with Al based ones. The new antifriction composite coatings based on copper were developed taking into account the requirements specified for plain bearings of internal-combustion engine. Pilot samples of plain bearings with antifriction coatings of Cu-Fe-Al-Pb system were produced. The antifriction composite having Cu-5Fe-5Al5Fe2-10Pb (mass %) composition has demonstrated low friction factor and high wear-resistance. Metallographic analysis of pilot samples was carried out by means of optical and scanning electron microscopy.
1 May 2020 in Inorganic Materials: Applied Research
This paper proposes a method for rapid cladding of copper powder with aluminum. The optimal parameters (frequency and amplitude of oscillations) of the experimental setup and the dispersity and volume fraction of the interacting powders are determined. The most productive cladding mechanism is considered. Dependences of the coating thickness (from 5 to 25 μm) on copper particles on the temperature (18–600°C) and the time of heating (5–30 s) the powder mixture are determined. It is shown that the highest rates of the coating growth on copper particles and the formation of Al–Cu intermetallic compounds are achieved at the temperatures of Al and Cu recrystallization.
30 September 2022 in Inorganic Materials: Applied Research
A composite material (CM) based on a copper powder clad with a Fe–Cu pseudo alloy (PA) for a working layer of two-layer interrupting electrical contacts was created using pressing, rolling, and sintering. The powder of activated carbon (CA) with the specific surface area of 1000 m2/g served as an arc quenching component, and highly dispersed powders of Al2O3, Fe2Al5, and Fe were used as additional components. The experimental linear dependences of the conductivity and hardness of copper-based composites on the concentration of particular functional additives of CA, PA, Al2O3, and Fe2Al5 were established. The addition of mixtures of these components was used to obtain CMs for the working contact layer of the following compositions (in wt %): 97% Cu + 1% СА + 2% PA and 97.5% Cu + 1% СA + 0.5% PA + 1% Al2O3 with the electrical resistivity of 3.20 and 4.5 μΩ cm and hardness HB of 1030 and 790 MPa, respectively. The dependence of the maximum allowable resistivity of the working layer (ρCM) on the ratio of its thickness to that of the copper layer was calculated for a given conductivity of a two-layer contact at a level of at least 75% of the copper conductivity. The characteristics of the CM with the composition 97% Cu + 1% СА + 2% PA make it possible to create an electrical contact for which the ratio of thicknesses of the working and copper layers is 1 : 1.