The effect of sintering aids of SiO2, ZrO2, B2O3, and MgO oxides on the optimum sintering temperature, ceramics grain growth, total volume of residual pores, and optical quality of obtained ceramics is studied. The best combinations of sintering aids are found; as a result, YAG:Nd (1 at%) samples of ceramics of high optical quality are obtained. An original method for characterizing laser properties of ceramics is developed. Comparative measurements of main laser characteristics of the obtained ceramics and ceramics of the Konoshima Chemical Corp. Ltd wellknown in the world practice, are performed.
Lasing in a solid-state inhomogeneously diode end-pumped Nd : KGW/Cr4+ : YAG laser is obtained at wavelengths of 1067 and 1181 nm (Stokes shift 901 cm−1) under conditions of frequency degeneracy of cavity modes. In this case, the radiation has a characteristic ring spatial structure, which testifies to transverse mode locking of the fundamental and Stokes components. The possibility of controlling the Raman conversion efficiency by changing the position of an undoped KGW crystal additionally installed in the cavity is demonstrated. It is shown that the transverse mode locking is accompanied by the total longitudinal mode locking at λ = 1067 and 1181 nm.