1 July 2013 in Applied Surface Science
24 March 2025 in Nature Communications
Information technology has a great demand for magnetoresistance (MR) sensors with high sensitivity and wide-temperature-range operation. It is well known that space charge inhomogeneity in graphene (Gr) leads to finite MR in its pristine form, and can be enhanced by increasing the degree of spatial disorder. However, the enhanced MR usually diminishes drastically as the temperature decreases. Here, by stacking a van der Waals ferromagnet Fe3GeTe2 (FGT) on top of graphene to form an FGT/Gr heterostructure, we demonstrate a positive MR of up to ~9400% under a magnetic field of 9 T at room temperature (RT), an order of magnitude larger MR compared to pure graphene. More strikingly, the giant MR of the FGT/Gr heterostructure sustains over a wide temperature range from RT down to 4 K. Both control experiments and DFT calculations show that the enhanced MR originates from spin-dependent orbital coupling between FGT and graphene, which is temperature insensitive. Our results open a new route for realizing high-sensitivity and wide-temperature-range MR sensors.
7 March 2013 in Materials Research Bulletin
10 January 2026 in Nature Communications
Efficient and reliable spin injection at room temperature with scalability is crucial for spintronic applications but remains challenging. Direct ferromagnetic metal deposition on two-dimensional materials often leads to inefficient transparent contacts. Here, we introduce an indium buffer layer between ferromagnetic cobalt (Co) and graphene to establish high-efficiency van der Waals (vdW) tunnel contacts. This buffer layer facilitates a physisorption interface between Co and graphene with a well-defined vdW gap, which functions as an effective spin tunnel barrier. Through buffer layer thickness optimization, we achieved a room-temperature spin injection efficiency of approximately 25% in graphene, comparable to the best single-crystalline oxide-tunnel-barrier-based devices, alongside explicit nonlocal spin valve signals and Hanle spin precession. We further demonstrate the scalability of our approach through uniform performance across multi-channel graphene spin valves and its versatility by achieving efficient spin injection in semiconducting MoS2 with an average efficiency of about 19.7%. Our strategy offers a simple, cost-efficient, and industry-compatible method for future large-scale and efficient spintronic applications.
10 June 2024 in Applied Physics Letters
Semiconductor spintronics has brought about revolutionary application prospects in future electronic devices. The tunnel junction plays a key role in achieving efficient spin injection in semiconductors. This work employed the GaN semiconductor as a room-temperature spin injection system, taking advantage of its weak spin–orbit coupling and spin scattering. By introducing a lattice-matched AlN barrier layer to improve the tunneling interface, advanced spin injection and transport were realized compared with traditional oxide barriers. The spin polarization was further improved by modulating the applied bias, and a bias-controlled tunneling enhancement mechanism was revealed. Consequently, we demonstrated a high record of spin polarization of 20.5%. This work paves a feasible route for achieving efficient spin injection and transport in GaN, which will further promote the development of room-temperature and high-performance spintronic devices.
14 July 2020 in IEEE Transactions on Nuclear Science
Lu2O3:Eu3+ nanowire arrays were synthesized by sol-gel immersion method using anodic aluminum oxide (AAO) templates. The influence of annealing temperature on the morphology, crystallinity, luminescence, and transmittance of the Lu2O3:Eu3+ nanowire arrays in AAO templates was studied. The results show that the nanowires in AAO templates are dense and orderly. Their diameters are uniform and defined by the templates. As annealing temperature increases from 500 °C to 900 °C, the shape of the nanowires remains substantially unchanged, but the crystallinity is greatly improved. When the annealing temperature reaches 1000 °C, the AAO template begins to crystallization and the samples begin to deform or even crack. In view of the fact that a scintillation screen for X-ray imaging requires not only high luminous intensity but also high transparency, no deformation, and no crack, the suitable annealing temperature for synthesizing the screen of Lu2O3:Eu3+ nanowire array in AAO template was obtain.