In the production of catalyst‐coated membranes (CCMs) for proton‐exchange membrane fuel cells and electrolyzers, the ink formulation and its processing are key factors in determining the resulting catalyst layer. Catalyst inks often contain a multicomponent solvent mixture. Selective drying, which can occur with solvent mixtures, changes the composition in the solidifying film and thus influences the microstructure of the layer that forms. The selectivity depends on the material‐specific thermodynamics of the solvents and the process‐related drying parameters. Different 1‐propanol/water mixtures serve as the state of the art material system considered and commonly used for CCM inks. Typical solvent mixtures can be dried selectively or non‐selectively, depending on the initial ink composition and humidity of the drying air. In mixtures that contain more 1‐propanol than the azeotropic or arheotropic composition, the 1‐propanol content accumulates in the remaining liquid; if there is less, it decreases. Increasing the preloading of the drying air with water leads to a relative water enrichment and shifts the tipping point to higher initial alcohol fractions. This behavior can be transferred to the real CCM production.
15 January 2024 in International Journal of Hydrogen Energy
The formulation and production of catalyst coatings significantly impact the porous microstructure and the performance of electrodes in polymer electrolyte membrane (PEM) fuel cells and electrolyzers. The critical step in the microstructure formation is the drying. Experimental studies have shown that the drying changes the solvent composition, affecting particle‐ and ionomer (self‐)interactions, as well as ink properties, which influence the drying‐induced stress build‐up within the layers. This study provides a theoretical analysis of the drying of binary 1‐propanol/water mixtures, and the transfer to the drying of catalyst inks. On the basis of selective drying, considering thermodynamic selectivity and gas‐phase kinetics, the accumulation and depletion of solvents during the drying process is described. The influence of different ink formulations (initial solvent compositions) and drying conditions (air temperature, heat transfer coefficient, and air pre‐loading) on ink composition during drying is studied. The selectivity is particularly influenced by the air pre‐loading, for example, relative humidity, which inhibits the evaporation kinetics of water. Theoretical predictions from the drying simulations are experimentally validated via gravimetric drying curves using different catalyst ink formulations. The results suggest that the catalyst layer drying can be effectively modeled by focusing solely on the evaporation dynamics of the solvent mixture.
The processing of catalyst‐coated membranes (CCM) is a major challenge in the production of efficient fuel cells and electrolyzers. In addition to the material properties and the formulation, the processing of the ink has a decisive effect on the crack pattern of the resulting electrodes. In this work, the influence of milling time in a ball mill on ink and electrode properties is investigated. Prolonged milling results in a reduction in large agglomerates, particularly. The pore diameter distribution of the membrane direct coatings exhibits a strong correlation with the particle size distribution (PSD) of the inks. With regard to the proportion of cracks, an optimum milling time exists. With very long milling time and thus small and narrow PSD, a continuous crack network is created. This phenomenon is explained by the large specific surface area of the dispersed particles and the distribution of the ionomer in the ink. Ionomer adsorbed to the particles is no longer available as a stress‐absorbing binder during solidification. A higher ionomer to carbon ratio can compensate for small PSD, enabling low‐crack coatings.