The use of electric arc furnace slag (EAFS) as sole precursor to produce alkali-activated mortars has been experimentally investigated. EAFS, a by-product of the steel recycling industry, is a coarse material with unevenly distributed and size-extensive particles. Milling of EAFS was required to achieve a cement-like sized powder before it could be used as precursor. Different combinations of sodium hydroxide (NaOH) and sodium silicate (Na2SiO3) were used, by varying the Na2O/binder concentration (4%, 6%, 8%, 10%, 12%) and SiO2/Na2O ratio (0, 0.5, 1.0, 1.5, 2.0, 2.5) to maximize the mechanical performance. The alkaline solutions were prepared 24 h prior to mixing to unify temperatures for all mixes. The results showed that the SiO2/Na2O ratio and strength development are directly proportional. The maximum 28-day compressive strength obtained, after being subjected to an initial 24 h thermal curing at 80 °C, was 9.1 MPa in mixes with 4% Na2O/binder and 2.5 SiO2/Na2O. However, after an additional 28 days of accelerated carbonation, the maximum compressive strength (i.e., 31 MPa compared to 3.9 MPa in uncarbonated mixes, corresponding to an 800% increase) was obtained in mixes with 12% and 1.0 for Na2O/binder and SiO2/Na2O, respectively, thus showing an alteration in the optimal alkaline activator contents.
This research focuses on the utilization of recently investigated aluminosilicate industrial wastes as precursors to produce non-structural precast alkali-activated concrete pavement blocks. For this purpose, conventional blocks (200 mm × 100 mm × 80 mm) were produced using electric arc furnace slag and municipal solid waste incineration bottom ashes as the sole binders. Portland cement and fly ash blocks were produced as references. The blocks underwent a curing regimen comprising thermal, dry, and carbonation curing stages. Control uncarbonated specimens were subjected to dry curing instead of CO2-based curing to evaluate the influence of carbonation on the blocks’ strength development. The specimens were subsequently examined following EN 1338, which is the European standard for assessing and ensuring the conformity of conventional concrete pavement blocks. The carbonated blocks revealed improved mechanical and physical properties in relation to the uncarbonated ones. All blocks met standard dimensions, showed minimal skid potential (most indicating extremely low potential for slip for reporting unpolished slip resistance values exceeding 75), and had enhanced abrasion resistance due to carbonation, showing 30% and 11% less volume loss due to abrasion for fly ash and bottom ash, respectively. Carbonated blocks performed better than non-carbonated ones, displaying lower water absorption (0.58% and 0.23% less water absorption for bottom ash and slag, respectively) and higher thermal conductivity (20%, 13%, and 8% increase in values for fly ash, slag, and bottom ash, respectively). These results confirm the effectiveness of the accelerated carbonation curing technique in improving the block’s performance. Despite the promising outcomes, further optimization of the alkaline solution and carbonation curing conditions is recommended for future research.