Pervious concrete provides a tailored surface course with high permeability properties which permit the easy flow of water through a larger interconnected porous structure to prevent flooding hazards. This paper reports the modeling of the flexural properties of quarry dust (QD) and sawdust ash (SDA) blended green pervious concrete for sustainable road pavement construction using Scheffe’s (5,2) optimization approach. The simplex mixture design method was adapted to formulate the mixture proportion to eliminate the set-backs encountered in empirical or trials and the error design approach, which consume more time and resources to design with experimental runs required to evaluate the response function. For the laboratory evaluation exercise, a maximum flexural strength of 3.703 N/mm2 was obtained with a mix proportion of 0.435:0.95:0.1:1.55:0.05 for water, cement, QD, coarse aggregate and SDA, respectively. Moreover, the minimal flexural strength response of 2.504 N/mm2 was obtained with a mix ratio of 0.6:0.75:0.3:4.1:0.25 for water, cement, QD, coarse aggregate and SDA, respectively. The test of the appropriateness of the developed model was statistically verified using the Student’ t-test and an analysis of variance (ANOVA), and was confirmed to be acceptable based on computational outcomes at the 95% confidence interval. Furthermore, the scanning electron microscopy (SEM) and energy dispersive X-ray (EDX) were used to evaluate the morphological and mineralogical behavior of green prior concrete samples with various additive mixture compositions. The addition of QD and SDA, on the other hand, aided the creation of porous microstructures in the concrete matrix due to fabric changes in the concrete mixture, potentially aided by the formation of cementitious compounds such as calcium aluminate hydrate and calcium silicate hydrate.
8 September 2022 in Sustainable Technology and Entrepreneurship
Management of waste glass is a huge environmental challenge in Nigeria and most developing countries. This study evaluates the influence of using Waste Glass Fines (WGF) as an asphalt filler to improve the Rigidity Ratio (RR) of asphaltic concrete. As stand-alone fillers in hot asphalt mixtures, the performances of quarry dust and waste glass powder were compared. The effect of waste glass as a partial replacement for quarry dust on the rigidity ratio of asphalt mixtures was then assessed using the Marshall Stability method. An optimum bitumen content (OBC) of 5.0% was established for the control specimens. Quarry dust (QD) was partially replaced with Waste Glass Fines (WGF) at 5% to 100% replacement levels. Results showed that while stability, Flow, and VMA at 5% OBC were found to satisfy the minimum requirement of typical Marshal Design Criteria for QD and WGF fillers, and Air Voids and VFB did not meet minimum specification. For QD+WGF samples, an optimum WGF content of 10% was found to give satisfactory results for both binders and wearing courses. The air voids were reduced, while VFB increased. The resistance of the mix against permanent deformations measured by the rigidity ratio or Marshal Quotient at this optimum WGF was 1.49KN/m2. This value is higher than those at 100% QD (1.33kN/m2) and 100% WGF (0.84kN/m2), Increased MQ values indicated a stiffer mix capable of spreading the applied load and resisting creep deformation. This indicates that Waste Glass Fines can improve asphalt resistance to permanent deformations.