The steelmaking industry requires coke as a reducing agent, as an energy source, and for its ability to hold slag in a blast furnace. Coking coal as raw coke material is very limited. Studying the use of biomass as a mixture of coking coal in the synthesis of biocoke is necessary to reduce greenhouse gas coal emissions. This research focuses on biomass and heating temperature through the coal blending method to produce biocoke with optimal mechanical properties for the blast-furnace standard. The heating temperature of biomass to biochar was evaluated at 400, 500, and 600 °C. The blending of coking coal with biochar was in the compositions of 95:5, 85:15, and 75:25 wt.%. A compacting force of 20 MPa was employed to produce biocoke that was 50 mm in diameter and 27 mm thick using a hot cylinder dye. The green sample was heated at 1100 °C for 4 h, followed by quenching with a water medium, resulting in dense samples. Increasing heating temperature is generally directly proportional to an increase in fixed carbon and calorific value. Biocoke that meets several blast-furnace criteria is a coal mixture with coconut-shell charcoal of 85:15 wt.%. Carbonization at 500 °C, yielding fixed carbon, calorific value, and compressive strength, was achieved at 89.02 ± 0.11%; 29.681 ± 0.46 MJ/kg, and 6.53 ± 0.4 MPa, respectively. This product meets several criteria for blast-furnace applications, with CRI 29.8 and CSR 55.1.
A research goal to create a coating material that conforms to the shape of the product up to 99.99% radar-absorbing, even at minimum thickness. The novelty of this study is the control of the BaFe12O19 : MnO2 mass ratio and hydrothermal holding time, which has not been explored until now.
14 April 2020 in International Journal of Technology
Barium hexaferrite (BHF) with the chemical formula BaFe12O19 is a well-known permanent magnet and is still primarily used in various electrical devices. Because of its excellent magnetic properties, BHF is potentially one of the best candidates as a microwave absorber. For this investigation, the magnetic and microwave absorption characteristics of nanostructured BHF and BaFe9Mn1.5Ti1.5O19 were study. The high coercivity of BHF was substantially reduced through Mn-Ti partial substitution for Fe atoms with a minor reduction of its saturation magnetization. Nanostructured Mn-Ti–doped BHF was obtained through particle size reduction with high-powered ultrasonic irradiation. After 12 h of ultrasonic irradiation, the mean particle of BHF reduced to 61 nm from 380 nm, and the Mn-Ti–doped BHF reduced from 545 nm to 95 nm. The mean crystallite size of the two samples was 15 and 18 nm, respectively. Hence, the particles of both samples contained only a few crystallites. The characterization of reflection loss revealed that the highest absorption value achieved by the nanostructured BaFe9Mn1.5Ti1.5O19 sample was 19.75 dB at 13.6 GHz, and approximately 90% of the intensity of incoming electromagnetic waves was reduced by the material.
4 April 2022 in International Journal of Renewable Energy Development
Biomass-based materials have the potential to replace conventional cokes for blast furnaces in the steel manufacturing study. Biomass as a renewable energy source can reduce the consumption of coking coal. The current challenge is saving fossil energy and waste management. The steelmaking industry with environmentally friendly processes and high energy efficiency is expected today. Many researchers have partially developed biomass as an alternative renewable resource to replace fossil fuels. This study aimed to determine the effect of composition the blending ratio of wood tar and molasses as a binder on the calorific value and compressive strength of bio-coke. The carbonization of redwood waste to produce high-quality charcoal was carried out at 500 °C with a kiln rotation speed of 20 rpm and a slope of 5°. The resulting charcoal showed a promising result with a 23.87 MJ/kg calorific value. The carbonization process of the redwood increased the fixed carbon value by up to 130% and the calorific value by 40%. The second part of this study focuses on bio-coke production by blending coking coal with redwood charcoal at 90:10 wt%. The coking coal and the redwood charcoal particle sizes were 40 and 50 mesh, respectively. A 15 wt% binder was added to increase the compressive strength of the bio-coke. The binder composition ratios of molasses: wood tar were 15:0, (12.5:2.5), and 10:5 wt%. The briquette was pressed using a cylinder die with a height: diameter ratio of 2.7:5.0 cm, then compacted up to 20 MPa followed by heating at 1100 °C for four hours. The bio-coke with a binder composition of 2.5 wt% wood tar + 12.5 wt% molasses produced a compressive strength of up to 5.57 MPa with a sulfur content of 0.8 wt% and produced a calorific value of 31.25 MJ/kg with an ash content of 9.6%. The study showed that the bio-coke produced meets some requirements for steelmaking industry.
29 October 2016 in International Journal of Technology
This paper reports the particle and crystallite size characterizations of mechanically alloyed Ba(1-x)SrxTiO3 (BST) with x = 0.3 and 0.7 prepared with the assistance of a high-power sonicator. Analytical grade BaCO3, TiO2 and SrCO3 precursors with a purity of greater than 99 wt.% were mixed and milled using a planetary ball mill to a powder weight ratio of 10:1. Powders obtained after 20 hours of milling time were then sintered at 1200°C for 4 hours to form crystalline powders.These powders were further treated ultrasonically under a fixed 6.7 gr/l particle concentration in demineralized water for 1, 3, 5, 7 hours and a fixed ultrasonic irradiation time of 1 hour to the dispersion of 6.7; 20; 33.3 gr/l concentrations. As to the results of crystallite size characterization, it is demonstrated that the mean crystallite size of BST with x = 0.3 and 0.7 undergo a slight change after the first 1 hour irradiation time and then remain almost unchanged. This was in contrary to the particle size in which the mean particle size of BST with x = 0.3 increased from 765 nm to 1405 nm after 7 hours irradiation time, while that of x = 0.7 increased from 505 nm to 1298 nm after 3 hours and then reduced back to the initial size after 7 hours ultra sonication time. The increase in particle size was due to large of cohesive forces among fine particles. It is also demonstrated that the concentration of particles in a dispersion with anionic surfactant do not effective to reduce the particle sizes ultrasonically. Nanoparticles with the mean size respectively 40 and 10 times larger than their respective crystallite size were successfully obtained respectively in x = 0.3 and x = 0.7.