Juan Manuel Manuel González Carmona

Dr. Juan Manuel Manuel González Carmona

orcid

Research Focus & Metrics

Academic Career Length

25Years (2002-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 September 2019 in Surface and Coatings Technology
Verified
Journal Article
Closed access
AMA. Moreno-Bárcenas
A. Moreno-Bárcenas
JJuan Manuel Alvarado Orozco
Juan Manuel Alvarado Orozco
JCJ.M. González Carmona
J.M. González Carmona
GMG.C. Mondragón-Rodríguez
G.C. Mondragón-Rodríguez
Juan Manuel Manuel González CarmonaJuan Manuel Manuel González Carmona
Juan Manuel Manuel González Carmona
AGAlejandra Garcia-Garcia
Alejandra Garcia-Garcia

19 September 2022 in Ceramics International
Verified
Journal Article
Closed access
DZD.F. Zambrano
D.F. Zambrano
RHR. Hernández-Bravo
R. Hernández-Bravo
ARA. Ruden
A. Ruden
DED.G. Espinosa-Arbelaez
D.G. Espinosa-Arbelaez
Juan Manuel Manuel González CarmonaJuan Manuel Manuel González Carmona
Juan Manuel Manuel González Carmona
VMV. Mujica
V. Mujica

2 July 2024 in Coatings
Verified
Journal Article
Open access
PDF file
COCarolina Ortega-Portilla
Carolina Ortega-Portilla
AGAndrea Giraldo
Andrea Giraldo
Jorge Andrés Cardona HernándezJorge Andrés Cardona Hernández
Jorge Andrés Cardona Hernández
ARAlexander Ruden-Munoz
Alexander Ruden-Munoz
G.C. Mondragón RodríguezG.C. Mondragón Rodríguez
G.C. Mondragón Rodríguez
Edgar FrancoEdgar Franco
Edgar Franco
Monolayers of Ti and TiN coatings, as well as a Ti/TiN bilayer coating, were deposited on AISI M2 steel substrates using the PVD cathodic arc technique. The coatings had a thickness close to 5 μm and an average roughness between 98.6 and 110.1 μm due to the presence of microdroplets on the surface. The crystalline structure of the materials was analyzed using Grazing Incidence X-ray Diffraction (GIXRD) with an increase in temperature to study the dynamics of oxide formation. A phase composition study was conducted using the Rietveld refinement method. At the temperatures where critical growth of titanium oxides, both anatase and rutile, was observed, pin-on-disk tests were performed to study the tribological properties of the materials at high temperatures. It was determined that the oxidation temperature of Ti is around 450 °C, promoting the formation of a combination of anatase and rutile. However, the formation of rutile inhibits the formation of anatase, which is stable above 600 °C. In contrast, TiN showed an oxidation temperature of 550 °C, with an exclusive growth of the rutile phase. The Ti/TiN bilayer exhibited mixed behavior, with the initial growth of anatase promoted by Ti, followed by the formation of rutile. Oxidation and tribo-oxidation dominated the wear behavior of the surfaces, showing a transition from mechanisms related to abrasion at low and medium temperatures to a combination of abrasion and adhesion mechanisms at high temperatures (800 °C).

20 November 2023 in Journal of Vacuum Science & Technology A
Verified
Journal Article
Open access
PDF file
ICI. Campos-Silva
I. Campos-Silva
LCL. E. Castillo-Vela
L. E. Castillo-Vela
IMI. Mejía-Caballero
I. Mejía-Caballero
JRJ. L. Rosales-Lopez
J. L. Rosales-Lopez
MOM. Olivares-Luna
M. Olivares-Luna
Juan Manuel Manuel González CarmonaJuan Manuel Manuel González Carmona
Juan Manuel Manuel González Carmona
In this study, novel findings were obtained regarding the influence of current intensity and electrode distance on the growth of the FeB-Fe2B layer during pulsed-DC powder pack boriding (PDCPB). Boride layer formation was carried out on AISI 1018 and AISI 4140 steels at 900 °C for 2700 s, considering current intensities ranging from 2.5 to 7.5 A and electrode distances of 10, 15, and 20 mm for each current intensity. The growth of the FeB-Fe2B layer was enhanced as the current intensity/electrode distance increased. This was related to the contribution of electromigration, the amount of powder mixture (used during the PDCPB) between electrodes, and Joule heating. Analysis of variance was performed on borided steels to assess the impact of the current intensity/electrode distance on the boride layer growth. The results revealed weight coefficients of approximately 50% for current intensity, around 40% for electrode distance, and a combined contribution of both variables of no more than 3.5%. Finally, multiple regression analyses were conducted to estimate boride layer thickness expressions as a function of the independent variables. The model results demonstrated a 5% error when compared to the experimental boride layer thickness.

22 June 2023 in Materials
Verified
Journal Article
Open access
PDF file
Juan Manuel Manuel González CarmonaJuan Manuel Manuel González Carmona
Juan Manuel Manuel González Carmona
CMClaudia Mambuscay
Claudia Mambuscay
COCarolina Ortega-Portilla
Carolina Ortega-Portilla
AHAbel Hurtado-Macias
Abel Hurtado-Macias
JPJeferson Fernando Piamba
Jeferson Fernando Piamba
This study focused on investigating the adhesion and tribological properties of niobium-doped titanium nitride (TiNbN) coatings deposited on D2 steel substrates at various substrate temperatures (Ts) under simulated cutting conditions. X-ray diffraction confirmed the presence of coatings with an FCC crystalline structure, where Nb substitutes Ti atoms in the TiN lattice. With increasing Ts, the lattice parameter decreased, and the crystallite material transitioned from flat-like to spherical shapes. Nanoindentation tests revealed an increase in hardness (H) with Ts, while a decrease in the elastic modulus (E) resulted in an improved elastic strain limit for failure (H/E) and plastic deformation resistance (H3/E2), thereby enhancing stiffness and contact elasticity. Adhesion analysis showed critical loads of ~50 N at Ts of 200 and 400 °C, and ~38 N at Ts of 600 °C. Cohesive failures were associated with lateral cracking, while adhesive failures were attributed to chipping spallation. The tribological behavior was evaluated using a pin-on-disk test, which indicated an increase in friction coefficients with Ts, although they remained lower than those of the substrate. Friction and wear were influenced by the surface morphology, facilitating the formation of abrasive particles. However, the absence of coating detachment in the wear tracks suggested that the films were capable of withstanding the load and wear.

1 February 2017 in Ceramics International
Verified
Journal Article
Closed access
ABA.F. Baron
A.F. Baron
JGJ. Guerrero
J. Guerrero
Juan Manuel Manuel González CarmonaJuan Manuel Manuel González Carmona
Juan Manuel Manuel González Carmona
AGA. Gómez
A. Gómez
AJA. Jurado
A. Jurado
HSH.Sánchez Sthepa
H.Sánchez Sthepa