The paper studies the properties of brass workpieces for antifriction rings under severe plastic deformation by high-pressure torsion. The evolution of microstructure and mechanical properties of deformed workpieces after six cycles of deformation by high-pressure torsion at 500 °C have been studied. All metallographic studies were performed using modern methods: transmission electron microscopy (TEM) and analysis electron back scatter diffraction patterns (EBSD). The deformation resulted in an ultrafine grained structure with a large number of large-angle boundaries. The strength properties of brass increased compared to the initial state almost by three times, the microhardness also increases by three times, i.e., increased from 820 MPa in the initial state to 2115 MPa after deformation. In this case, the greatest increase in strength properties occurs in the first two cycles of deformation.
The article presents the results of obtaining a composite material by sintering nickel-containing raw materials mixed with carbon-containing materials, namely using coke and semi-coke. The sintering process was performed at a charge layer height of 240 mm and the temperature of the lower layer was T = 1200 °C. The results of the sieve analysis showed (a fraction of 10 mm) that the yield of a suitable composite material using coke was 68.3% and with semi-coke 67.0%. The average nickel and chromium content in the composite materials was 1.42% and 3.07%, accordingly. As a result of determining the strength characteristics of the obtained composite materials with various reducing agents by dropping from a height of 2 m onto a steel pallet, it was found that the obtained composite materials have high mechanical properties in terms of strength of 81% and 89.2%. The results of the elemental composition at the studied points and the thermal analysis of the studied composite material are presented. The mineralogical composition of the composite material is presented in the form of serpentine and nontronite, and the empty rock is made of quartz and talc. The activation energy of thermal analysis by the method of non-isothermal kinetics were calculated. The results of experiments on the production of composite materials from nickel-containing raw materials will be recommended for obtaining the optimal composition of composite materials at the stage of pilot tests and industrial development of the developed technology for processing nickel ores of the Republic of Kazakhstan. For the processing of nickel-poor nickel ores, it is of great importance to obtain optimal technological and technical and economic indicators that ensure low cost of nickel in the resulting product.