This article provides a comprehensive overview of recent studies concerning laser heat treatment (LHT) of structural and tool steels, with particular attention to the 21NiCrMo2 steel used for carburized gear wheels. Analysis includes the influence of critical laser processing conditions—including power output, motion speed, spot size, and focusing distance—on surface microhardness, hardening depth, and microstructure development. The findings indicate that the energy density is the dominant factor that affects the outcomes of LHT. Optimal results, in the form of a high surface microhardness and a sufficient depth of hardening, were achieved within the energy density range of 80–130 J/mm2, allowing for martensitic transformation while avoiding defects such as melting or cracking. At densities below 50 J/mm2, incomplete hardening occurred with minimal microhardness improvement. On the contrary, densities exceeding 150–180 J/mm2 caused surface overheating and degradation. For carburized 21NiCrMo2 steel, the most effective parameters included 450–1050 W laser power, 1.7–2.5 mm/s scanning speed, and 2.0–2.3 mm beam diameter. The review confirms that process control through energy-based parameters allows for reliable prediction and optimization of LHT for industrial applications, particularly in components exposed to cyclic loads.
The article presents an analysis of the mechanical properties of S700MC steel, which represents advanced low-alloy high-strength steels. The influence of microstructure, shaped by a controlled thermo-mechanical rolling process, on the strength, ductility, and resistance to cracking and fatigue of the material is discussed. Particular attention is paid to the anisotropy of mechanical properties resulting from the orientation relative to the rolling direction, manifested by variations in yield strength, tensile strength, and total elongation of the specimens. The analysis also includes the material’s behavior under dynamic conditions, where the steel’s strength increases with the strain rate. Experimental investigations conducted using the digital image correlation (DIC) method enabled a detailed assessment of local strains and fracture characteristics of specimens subjected to both static and dynamic testing. The results showed that specimens cut along the rolling direction exhibited, on average, 6.4% higher tensile strength and 6.8% higher yield strength compared to those cut transversely. Moreover, dynamic loading led to an increase in load-bearing capacity of over 10% compared to static tests. The obtained data are highly relevant from the perspective of structural design, where the selection of material orientation and the consideration of strain rate effects are crucial for ensuring the reliability of components made from S700MC steel.