In this study, two types of single polymer films have been inserted in a composite laminate to examine their toughening effects on mechanical properties. The first is a thermoplastic polyurethane (PU) film, and the second is an adhesive epoxy film featuring a polyester net. The laminates were manufactured either using a co-curing (CC) process or a secondary bonding (SB) process used for the epoxy film. Mode I and mode II interlaminar fracture toughness were measured for laminates manufactured by both processes and compared with the corresponding reference laminate toughness. A significant increase in both mode I and mode II toughness resulted when introducing a single PU film, approximately 290% and 50%, respectively. Similarly, the epoxy film improved the interlaminar fracture properties; the CC process produced an increase of 175% for mode II toughness, while the SB adhesive film showed an increase of 75% for mode II toughness.
21 February 2022 in Composites Part B: Engineering
In this study, carbon fiber/epoxy composites (CFRP) were fabricated by vacuum‐assisted resin infusion molding (VARIM) with polyphenylene ether (PPE) as a toughening agent. The PPE contained hydroxyl end groups that facilitated chemical bonding with epoxy during curing. PPE was incorporated into the epoxy matrix by dissolution, and spreading in the interlaminar regions. The presence of PPE as a toughener exhibited significant improvement in the Mode‐I fracture toughness of the composites. The CFRP samples, which were toughened with 5 wt.% and 10 wt.% PPE, showed about 191% to 380% enhancement, respectively, in the critical energy release rate (GIC) compared to the unmodified sample. Dynamic mechanical analysis (DMA) showed about a 6°C increase in the glass transition temperature of the toughened composites, which is an interesting aspect of this work. These results indicate the potential of using PPE as a toughening agent in CFRP composites.
This paper presents repair methods for in-situpolymerised acrylic (Elium®)/glass composites focusing on mode-I fracture toughness recovery. Acrylic/glass composites were first subjected to double cantilever beam (DCB) tests to measure their Mode-I fracture toughness. The delaminated samples after DCB tests were repaired and rejoined. Two repair methods were performed: liquid resin injection and press moulding at two different temperatures (130°C and 160°C). The repaired samples were subjected to a second set of DCB tests. The fracture behaviours of the four specimen groups (virgin, resin-injected, pressed at 130°C, and pressed at 160°C) were evaluated in terms of strain energy release rates (G IC ) during crack initiation and propagation. The results showed that specimens repaired by resin injection exhibited highest G IC values, about 30% higher than the virgin state, due to the formation of a semi-interpenetrating polymer network (semi-IPN) at the joining interface. Scanning electron microscopy images provided insight into distinctive fracture behaviours for each test group.
An investigation into the inspection capabilities of in-field advanced ultrasound detection for use on ultra-thick (20 to 100 mm) glass fibre-reinforced polyester composites is presented. Plates were manufactured using custom moulding techniques, such that delamination flaws were created at calibrated depths. The full matrix capture technique with an on-board total focussing method was used to detect flaws scanned by a 0.5 MHz linear array probe. Flaw through-thickness dimensions were altered to assess the threshold for crack face separation at which delaminations could be identified. Furthermore, part thickness and in-plane flaw dimensions were varied to identify the inspection capability limitations of advanced ultrasonics for thick composites. The results presented in this study demonstrate an inverse relationship between the ability to find delaminations and plate thicknesses, with inspections successful at depths up to 74 mm. When the delamination thickness exhibited surface-to-surface contact, the inspection capability was reduced to 35 mm. There was an exponential decay relationship between the accuracy of the flaw depth measurement and plate thickness, likely due to the necessity of low probe frequencies. The effective inspection depth was determined to be in the range of 1 to 20 times the wavelength. It is speculated that the accuracy of measurements could be improved using probes with novel coupling solutions, and detectors with optimised signal processing/filtration algorithms.