Automotive manufacturers are increasingly using ultra-high-strength steels in vehicle components to facilitate mass reduction via downgauging. Unfortunately, as the strength of steels increases, so does susceptibility to ‘hydrogen embrittlement’, a process in which ductility is significantly impaired by ingress of hydrogen. Mechanisms and environmental conditions by which this degradation occurs are not fully understood. In this work, 2 fully-ferritic, 2 fully-martensitic boron, and 2 ferrite-martensite dual-phase, ultra-high-strength steels, were assessed for susceptibility to hydrogen embrittlement via 3 key characteristics: firstly, with particular regard to hydrogen evolution under corrosion conditions, through well-established open circuit potential and potentiodynamic polarisation experiments. Exacerbation of hydrogen evolution through galvanic corrosion of a zinc coating was assessed by scanning vibrating electrode technique (SVET), and an attempt made to quantify increased risk of hydrogen evolution during crevice corrosion through a novel time-lapse photography experiment. Secondly, hydrogen diffusivity was assessed via permeation experiments. Finally, degradation in mechanical properties due to diffusing hydrogen was evaluated through slow strain rate tests (SSRT), whereby susceptibility to embrittlement was equated to reduction in ductility of hydrogen-charged test specimens. The fully-ferritic steels showed the greatest resistance to mechanical degradation, attributed to micro-alloy nano-precipitates within their microstructure acting as ‘traps’, leading to lower diffusivity compared to dual-phase steels of equivalent strength. Indeed, lower diffusivity showed a strong correlation with lower levels of embrittlement across all steels. 1000 MPa dual-phase steel showed the greatest degradation in mechanical properties, with fully-martensitic boron steels also found to be particularly susceptible. 1000 MPa dual-phase steel also showed the largest increase in hydrogen evolution reaction in response to polarisation, thought to result from the inherent potential difference between ferrite and martensite phases. Galvanic corrosion of a damaged zinc coating was found to polarise the exposed steel substrate, triggering sufficient hydrogen evolution to reach critical concentrations for embrittlement.
The adoption of advanced high-strength steels (AHSS) in the automotive industry has significantly increased in recent years driven by weight reduction and enhanced crashworthiness. Hot dip galvanised sacrificial coatings are regularly applied to these steels for corrosion protection. In this investigation, the scanning vibrating electrode technique (SVET) demonstrated that hydrogen evolution on the steel substrate is taking place when these sacrificial coatings are damaged during service, increasing the risk of hydrogen embrittlement. The hydrogen embrittlement susceptibility of a new generation of nano-precipitate ferritic, FNP, AHSS have been studied and compared against conventional dual phase ferritic-martensitic, FM, AHSS at equivalent strength levels. Hydrogen permeation tests have shown that FNP AHSS have lower effective diffusion coefficients, Deff, than FM AHSS at equivalent strength levels. At 800 MPa strength levels Deff were 1.68 × 10−7 cm2/s and 1.87 × 10−7 cm2/s for FNP800 and FM800, respectively. At higher strength levels, 1000 MPa, Deff were 7.45 × 10−8 cm2/s and 1.45 × 10−7 cm2/s for the FNP1000 and FM1000, respectively. Slow strain-rate tests (SSRT) showed that FNP AHSS displayed over 35% higher resistance to hydrogen embrittlement than conventional FM AHSS. Quantitative fractographic analyses confirmed that the new ferritic nano-precipitate microstructure retains much more ductile behaviour than conventional martensitic-ferritic even under the most severe hydrogen charging conditions tested.
The adoption of advanced high-strength steels (AHSS) in the automotive industry have significantly increased in recent years driven by weight reduction and enhanced crashworthiness. Hot dip galvanised sacrificial coatings are regularly applied to these steels for corrosion protection. In this investigation, the scanning vibrating electrode technique (SVET) demonstrated that hydrogen evolution on the steel substrate is taking place when these sacrificial coatings are damaged during service, increasing the risk of hydrogen embrittlement. The hydrogen embrittlement susceptibility of a new generation of nano-precipitate ferritic, FNP, AHSS have been studied and compared against conventional dual phase ferritic-martensitic, FM, AHSS at equivalent strength levels. Hydrogen permeation tests have shown that FNP AHSS have lower effective diffusion coefficients, Deff, than FM AHSS at equivalent strength levels. At 800 MPa strength level Deff were 1.68×10-7 cm2/s and 1.87×10-7 cm2/s for FNP800 and FM800 respectively. At higher strength levels, 1000 MPa, Deff were 7.45×10-8 cm2/s and 1.45×10-7 cm2/s for the FNP1000 and FM1000, respectively. Slow strain rate tests (SSRT) showed that FNP AHSS displayed over 35% higher resistance to hydrogen embrittlement than conventional FM AHSS. Quantitative fractographic analyses confirmed that the new ferritic nano-precipitate microstructure retains much more ductile behaviour than conventional martensitic-ferritic even under the most severe hydrogen charging conditions tested.
About Me
Steel researcher with 15 years' experience across industry and academia.
Steel researcher with 15 years' experience across industry and academia.