This work investigates the suitability of supercritical fluid technology for designing a safe, efficient and sustainable consolidation treatment for a pair of heavily degraded goalkeeper gloves. Traditional methods have revealed themselves as unsafe and inefficient, leading to material loss and a minimal enhancement of surface cohesion. To overcome these limitations, the use of supercritical carbon dioxide (scCO2) was explored in a treatment, where scCO2 behaves as a green solvent and consolidant carrier. In-depth and homogeneous application of the consolidant, without the need for direct contact with the foam material, was sought. As a proof of concept, the procedure was tested on samples that mimic the synthetic latex-based foam composition and condition of the object. Poly(vinyl acetate) was selected as a consolidant because its behaviour and solubility in scCO2 are known. Several experimental conditions were explored to assess the impact and feasibility of the scCO2-assisted consolidation procedure. Empirical observations, optical microscopy, scanning electron microscopy and infrared spectroscopy were used to monitor potential modifications in the samples and assess the treatment efficacy. The results highlighted the advantages and pitfalls of scCO2-assisted consolidation, paving the way for fine-tuning the process. It neither damaged the fragile surfaces of the foam samples nor increased material loss, which is an advantage compared to traditional treatments. The performed analysis suggested that homogeneous impregnation of the foams was achieved. This study might be a turning point in the conservation of foam-based museum objects, as the results indicate the suitability of the scCO2-assisted consolidation process as a non-toxic and more efficient alternative, being safer for the object.
Coated fabrics featuring plasticised poly(vinyl chloride) (p-PVC) and thermoplastic polyurethane (TPU) coatings are widespread in fashion collections. These materials pose significant conservation challenges due to their production and chemical variability, coupled with issues of rapid deterioration. Despite their prevalence and instability, systematic research on their composition and ageing behaviour remains limited, as most studies rely mainly on infrared spectroscopy and cover a small number of cases, which cannot fully capture their chemical complexity. This knowledge gap represents a pressing issue, as it hampers the development of well-informed conservation strategies. This research addresses this gap by investigating a representative set of twenty-five historical and contemporary fabrics from the 1990s onwards, coated with aromatic and aliphatic polyester-based TPUs, as well as phthalate- and terephthalate-plasticised PVCs. Samples were characterised using a multi-analytical approach combining optical microscopy, infrared spectroscopy, pyrolysis–gas chromatography/mass spectrometry, and X-ray fluorescence spectroscopy. This integrated strategy provided unprecedented detail on the chemical variability of p-PVC and TPU-coated fabrics, enabling the identification of primary components, additives, degradation products, and mixed compositions. This study underscores the value of multi-technique analysis to capture the complexity of such coated fabrics, providing essential knowledge for further research and development of effective conservation strategies for fashion collections.
Coated fabrics with thermoplastic polyurethane (TPU) are largely found in fashion and design collections in imitation leathers and glossy-look fabrics. Unfortunately, blooming is a common damage in aged TPU, appearing as white crystalline deposits at the surface. These deposits have been generally identified as adipic acid and mainly affect ester-based aromatic TPU. The white colour of adipic acid often leads to the complete unrecognition of the cultural item, highly decreasing its values. Strategies to remove blooming are still absent in the literature, resulting in a lack of action by conservators. The Glossy Surfaces project addressed this issue through preliminary research on cleaning strategies to remove adipic acid. Dry and wet methods were tested on two fabrics showing blooming and different surface cohesion. Non-confined and confined liquids in hydrogels were included and assessed by digital microscopy, colourimetry, and infrared spectroscopy. The best results were achieved with agar-agar, but limitations were also recognized.
Synthetic-coated fabrics, often made of short-life expectancy coatings, namely plasticised poly(vinyl chloride) (p‑PVC) and thermoplastic polyurethane (TPU), are challenging to preserve. These materials are poorly studied within the conservation field, and there is a lack of research and solutions for their preservation. This study aimed to provide insight into the yet unknown variability of p-PVC and TPU-coated fabrics in fashion collections. The subtle differences in layer construction and morphology were investigated in a selected set of materials to unveil production methods and better understand delamination damages, namely peeling and flaking. Optical microscopy provided primary material assessment, complemented by ATR-FTIR for molecular identification. A wide variability of synthetic-coated fabrics was reported and connections between morphology, production methods and delamination damages were suggested. Optical microscopy proved to be a powerful tool in the study of the stratigraphy of coated fabrics, enhancing material knowledge for more informed conservation decisions.
In the 19th century, significant linen and leather imitation products were invented using cellulose nitrate-coated fabrics, including celluloid detachable collars and Fabrikoid artificial leather, now preserved in the Hagley Museum and Library, USA. Using optical microscopy, µRaman, and µFourier Transformed Infrared spectroscopies, this study highlights the need for characterizing the heterogeneity of these materials at the microscale. While the detachable collars have well-preserved fabric coatings composed of cellulose nitrate, camphor, anatase (TiO2), and carbon-based particles, Fabrikoid’s pigmented cellulose nitrate-castor oil systems show problems. Our molecular data align with a 1922 report on Fabrikoid degradation, revealing free fatty acids and carboxylates formed due to oil oxidation. This is concerning as these materials were used until the 1960s, demonstrated by the analysis of objects from the National Museum of Costumes in Portugal. Future studies should address the compatibility of cellulose nitrate with fatty acids and the reactivity of additives in these systems.
Synthetic-coated fabrics, often made of short-life expectancy coatings, namely plasticised poly(vinyl chloride) (p‑PVC) and thermoplastic polyurethane (TPU), are challenging to preserve. These materials are poorly studied within the conservation field, and there is a lack of research and solutions for their preservation. This study aimed to provide insight into the yet unknown variability of p-PVC and TPU-coated fabrics in fashion collections. The subtle differences in layer construction and morphology were investigated in a selected set of materials to unveil production methods and better understand delamination damages, namely peeling and flaking. Optical microscopy provided primary material assessment, complemented by ATR-FTIR for molecular identification. A wide variability of synthetic-coated fabrics was reported and connections between morphology, production methods and delamination damages were suggested. Optical microscopy proved to be a powerful tool in the study of the stratigraphy of coated fabrics, enhancing material knowledge for more informed conservation decisions.