This study investigated the influence of process-induced surface features, porosity, and microstructure on the corrosion behavior of Ti-6Al-4V alloy produced by different additive manufacturing (AM) technologies, including emerging sinter-based material extrusion (MEX), well-established electron beam melting (EBM) and laser powder bed fusion (LPBF), and wrought reference material. The investigated manufacturing routes produced sensibly different surfaces, porosity, and microstructures. Potentiodynamic and potentiostatic polarization tests in phosphate-buffered saline (PBS) revealed stable passivity and excellent corrosion performance for all AM alloys, both in the as-built and polished conditions. After polishing, modest variations were detected among manufacturing technologies, suggesting a possible deleterious effect of the intrinsic porosity once exposed to the environment. Immersion tests performed in neutral and acidified isotonic solutions highlighted the onset of selective corrosion phenomena between the α and β phases under deoxygenated acidic conditions, consistent with Volta potential measurements. Long-term immersion in acidified isotonic solution confirmed the detrimental influence of porosity on the corrosion behavior of Ti-6Al-4V, especially for the MEX-produced alloy, where the presence of a macro-defect network promoted localized corrosion propagation.
The high emissions of carbon dioxide (CO2) into the atmosphere have driven the development of carbon capture, transport, and storage (CCTS) technologies. These focus on capturing CO2 from industrial exhaust gases and transporting it through existing pipeline networks. Although various capture techniques are available, they may introduce impurities such as O2, N2, Ar, H2O, NH3, and others into the CO2 stream. These contaminants can significantly alter the thermophysical behaviour of the fluid, making the phase behaviour predictions, reliable for pure CO2, much more complex. Pressure and temperature variations along pipelines can induce unexpected phase transitions, affecting fluid composition and potentially triggering corrosion. This review examines the formation of condensates within pipelines and their role in initiating corrosion phenomena, with a focus on top of the line corrosion (TLC) and conventional CO2-induced corrosion (sweet corrosion). The main literature findings highlight how phase changes and altered fluid composition due to corrosion processes can significantly intensify degradation mechanisms during CO2 transport.
The aim of this study is to comprehensively investigate and quantify the effect of strain rate (SR) and environmental parameters on the stress corrosion cracking (SCC) behavior of a high-strength, aluminum–copper alloy. Slow strain rate (SSR) tests were carried out in air at 25 °C, over a SR range from 10−4 to 10−7 s−1 and controlled relative humidity (RH) between 40% and 80%. The influence of the pre-soaking period in 3.5 wt.% NaCl solution was also assessed. A major effect of pre-soaking was identified, as it was necessary for the onset of SCC. Increasing RH over 40% and decreasing SR below 10−5 s−1 significantly intensified SCC susceptibility, leading to ductility loss up to 84%. SSR test results were supported by microstructural investigations, with particular emphasis on the role of second phases. Their electrochemical activity was examined by scanning Kelvin probe force microscopy (SKPFM), while intergranular corrosion (IGC) susceptibility was evaluated according to the ISO 11846 standard. The pronounced IGC susceptibility of the alloy led to predominantly intergranular fracture morphologies in cross-section peripheral areas after SSR testing. The results confirmed the synergistic effect among microstructure, IGC susceptibility and SCC behavior, identifying a critical window of mechanical and environmental parameters governing SCC.