The high emissions of carbon dioxide (CO2) into the atmosphere have driven the development of carbon capture, transport, and storage (CCTS) technologies. These focus on capturing CO2 from industrial exhaust gases and transporting it through existing pipeline networks. Although various capture techniques are available, they may introduce impurities such as O2, N2, Ar, H2O, NH3, and others into the CO2 stream. These contaminants can significantly alter the thermophysical behaviour of the fluid, making the phase behaviour predictions, reliable for pure CO2, much more complex. Pressure and temperature variations along pipelines can induce unexpected phase transitions, affecting fluid composition and potentially triggering corrosion. This review examines the formation of condensates within pipelines and their role in initiating corrosion phenomena, with a focus on top of the line corrosion (TLC) and conventional CO2-induced corrosion (sweet corrosion). The main literature findings highlight how phase changes and altered fluid composition due to corrosion processes can significantly intensify degradation mechanisms during CO2 transport.
This article presents the data collected during experimental solubility tests in University of Bergamo lab and the developed code to estimate the principal parameters for hydrogen uptake. The experimental approach proposed involves in two-step process: the first phase consists of electrochemical charging to saturate the metallic sample via cathodic polarization at potentials lower than the equilibrium potential for hydrogen evolution, followed by a second phase of discharging under anodic polarization at potentials higher than the equilibrium potential. During the discharging phase, the time-dependent anodic current is influenced by the flux of diffusible hydrogen exiting the sample. This flux is governed by the initial concentration of diffusible hydrogen in the material, the diffusion coefficient, and the time elapsed between the end of the charging step and the beginning of the discharging phase. Via a data-driven optimisation it is possible to obtain the characteristic parameter of hydrogen diffusion in the material (apparent diffusion coefficient, hydrogen uptake and waiting time) using the MATLAB code. The data permit to elaborate the cylindrical geometry, however it is possible to modify the target curve via a simulation on a specific geometry (not included in the data) and use the same method to elaborate the experimental data of a specific geometry.
The aim of this study is to comprehensively investigate and quantify the effect of strain rate (SR) and environmental parameters on the stress corrosion cracking (SCC) behavior of a high-strength, aluminum–copper alloy. Slow strain rate (SSR) tests were carried out in air at 25 °C, over a SR range from 10−4 to 10−7 s−1 and controlled relative humidity (RH) between 40% and 80%. The influence of the pre-soaking period in 3.5 wt.% NaCl solution was also assessed. A major effect of pre-soaking was identified, as it was necessary for the onset of SCC. Increasing RH over 40% and decreasing SR below 10−5 s−1 significantly intensified SCC susceptibility, leading to ductility loss up to 84%. SSR test results were supported by microstructural investigations, with particular emphasis on the role of second phases. Their electrochemical activity was examined by scanning Kelvin probe force microscopy (SKPFM), while intergranular corrosion (IGC) susceptibility was evaluated according to the ISO 11846 standard. The pronounced IGC susceptibility of the alloy led to predominantly intergranular fracture morphologies in cross-section peripheral areas after SSR testing. The results confirmed the synergistic effect among microstructure, IGC susceptibility and SCC behavior, identifying a critical window of mechanical and environmental parameters governing SCC.
The decarbonisation of the energy sector is driving increasing interest in the use of hydrogen as an energy carrier, with existing natural gas networks representing a potential infrastructure for its distribution. Before hydrogen can be widely introduced into these systems, the compatibility of the materials currently employed in gas networks must be thoroughly evaluated. While the behavior of carbon steels in hydrogen environments has been extensively investigated, considerably less information is available for the non-ferrous metallic materials that are widely used in low-pressure gas distribution systems. Distribution networks, which typically operate at pressures below 16 bar, include a broader range of materials and components than high-pressure transmission pipelines and are generally subject to fewer standardization requirements. Within this context, the Horizon Europe CANDHy project (Grant Agreement No. 101111893) aims to assess the suitability of non-steel metallic materials currently used in European gas distribution infrastructures for future hydrogen service. A survey carried out during the project identified cast irons as the most widespread non-steel metallic materials in these networks. This paper reviews the current understanding of hydrogen interaction with cast irons, including hydrogen dissociation, adsorption, solubility and diffusion, together with the principal mechanisms responsible for hydrogen embrittlement. The available literature indicates that exposure to high-pressure gaseous hydrogen at ambient temperature generally has little influence on the mechanical performance of cast irons. In contrast, hydrogen uptake during electrochemical charging or exposure to high-temperature hydrogen environments may lead to embrittlement. Under cathodic polarization, the susceptibility of cast irons appears to depend strongly on microstructural features, particularly the morphology, size and distribution of graphite within the alloy.
Hydrogen–steel interactions remain a critical concern for the safe deployment of hydrogen–natural gas mixtures in pipeline infrastructures. Thermally grown iron oxides may be a good barrier to hydrogen ingress into the crystalline lattice of pipeline steels, but their actual effectiveness depends strongly on their composition and stability under service conditions. Several experimental approaches have been proposed to investigate the correlation between thermally grown oxides and hydrogen permeation. Among these, electrochemical permeation testing offers a more complex but safer methodology compared to pressurized hydrogen gas tests. However, when the oxide is directly exposed to the charging side (cathodic charging conditions), permeation behaviour often appears comparable to that of bare steel, and rapid oxide degradation occurs. This study introduces an alternative permeation testing configuration that enables direct assessment of thin thermally grown oxides while preserving their structural integrity. By deliberately placing the oxide on the anodic detection side, mechanical removal during hydrogen evolution is suppressed, allowing the intrinsic resistance of the oxide to hydrogen transport to be evaluated. Carbon steel samples were thermally oxidized at 250 °C for controlled exposure times, and the resulting oxide scales were characterized by Raman spectroscopy, revealing variations in hematite and magnetite fractions. Hydrogen permeation was evaluated using a Devanathan–Stachurski cell by positioning the oxidized surface either on the cathodic charging side or on the anodic detection side. Under these conditions, significant variations in apparent steady-state permeation current density were observed as a function of oxidation time and oxide composition.