Lithium-ion (Li-ion) batteries with Ni-based cathodes are leading storage technology in the fields of electric vehicles and power-grid applications. NCA (LiNiCoAlO2) batteries are known for their troublesome degradation tendencies, and this susceptibility to degradation raises questions regarding the safety of their usage. Hence, it is of vital importance to analyse the degradation of NCA batteries via methods which are applicable to onboard systems, so that the changes in the battery’s state of health can be addressed accordingly. For this purpose, it is crucial to study batteries stressed by various conditions which might induce degradation of different origins or magnitudes. Methods such as electrochemical impedance spectroscopy (EIS), galvanostatic intermittent titration technique (GITT), and incremental capacity analysis (ICA) have been used in battery research for years, however, there is a lack of published studies which would analyse the degradation of NCA batteries by simultaneous usage of these methods, which is essential for a comprehensive and confirmatory understanding of battery degradation. This study intends to fill this research gap by analysing the degradation of NCA batteries via simultaneous usage of EIS, GITT, and ICA methods for common stress-inducing operating conditions (over-charge, over-discharge, and high-current charging).
The paper presents fabrication and characterization of amorphous silicon carbide (a-SiC:H) based structures for photo-electrochemical (PEC) water splitting. The increase of the photocurrent of PEC upon the decreased of CH 4 flow during the deposition is associated with the decrease of the band gap and increased absorption of light in a-SiC:H. Photocurrent of 50 µ A/cm 2 is achieved for PEC structure prepared with the lowest CH 4 flow during the deposition. An ITO/a-SiC:H/Si silicon heterojunction structure forming a simple photovoltaic cell (PV) with efficiency of 9.66% was prepared to support additional voltage hereby forming a hybrid PEC-PV system. ASA simulation revealed that a photocurrent of 0.62 mA/cm 2 and solar to hydrogen efficiency of 0.76% can be achieved for hybrid a PEC-PV structure with 5 PVs connected in series behind the PEC cell. Further opportunities for increasing the performance are discussed and summarized.
As second‐life applications for used electric vehicle (EV) batteries receive growing attention, the need for accurate and efficient diagnostics of the state‐of‐health (SOH) of such battery modules becomes increasingly critical. Electrochemical impedance spectroscopy (EIS) stands out as one of the most promising techniques for this purpose, offering comprehensive and non‐destructive analysis of various SOH indicators. However, its pronounced sensitivity to temperature raises concerns regarding the influence of thermal conditions during measurements. This study investigates the thermal stabilisation behaviour of a first‐generation Nissan Leaf battery module subjected to step changes in ambient temperature and evaluates how internal thermal dynamics affect the accuracy and reliability of key EIS parameters. The results show that, at the point when the module casing appears thermally stabilised, the ROHM and Warburg impedance exhibit acceptable accuracy approaching the 2% error benchmark. In contrast, RSEI and RCHT demonstrate large relative errors and require significantly more time to reach thermal equilibrium. These findings highlight that, under the tested conditions, surface temperature monitoring alone is insufficient. This work provides practical insight into reliable EIS‐based SOH diagnostics of used battery modules, with particular emphasis on the impact of ambient temperature variations during the transition from storage to testing facilities.
Differential capacity (dQ/dV) analysis has emerged as a powerful diagnostic tool for lithium-ion battery characterization, yet large-scale statistical studies on fresh commercial cells remain limited. This work presents a comprehensive dQ/dV analysis of 134 fresh Molicel P45B 18650 cells to establish baseline electrochemical signatures and quantify manufacturing variability. Systematic peak characterization reveals that voltage positions are highly consistent across the batch, reflecting uniform material composition, while peak intensities exhibit moderate variability attributable to manufacturing-related differences in active material loading. Principal component analysis and hierarchical clustering identify two natural cell subpopulations with distinct electrochemical activity levels, motivating a three-tier grading framework for quality-based cell classification. Strong charge--discharge correlations in peak intensities indicate co-variation within the cell population, and minimal voltage hysteresis suggests low polarization resistance across the batch. This baseline characterization supports cluster-informed cell sorting for battery pack assembly and provides a reference dataset for future degradation studies, demonstrating that dQ/dV analysis can serve as a rapid, non-destructive screening method for commercial cell quality assessment.