19 February 2025 in Engineering Failure Analysis
Verified
Journal Article
Open access
RWRashiga Walallawita
Rashiga Walallawita
MHMatthew C. Hinchliff
Matthew C. Hinchliff
DSDimitry Sediako
Dimitry Sediako
JQJohn Quinn
John Quinn
VCVincent Chou
Vincent Chou
KWKim Walker
Kim Walker

4 October 2024 in Metals
Verified
Journal Article
Open access
PDF file
RWRashiga Walallawita
Rashiga Walallawita
MHMatthew C. Hinchliff
Matthew C. Hinchliff
DSDimitry Sediako
Dimitry Sediako
JQJOHN QUINN
JOHN QUINN
VCVincent Chou
Vincent Chou
MHMatthew Hill
Matthew Hill
This study employs a custom hollow specimen setup to investigate the HE in API 5L X60 pipeline base and welded materials exposed to pure hydrogen and a 20% hydrogen–natural gas blend at 2.07 MPa. Results indicate embrittlement with increasing hydrogen concentration. The base material showed a hydrogen embrittlement index (HEI) of 11.6% at 20% hydrogen and 12.4% at 100% hydrogen. For the welded material, the HEI was 14.6% at 20% hydrogen and 18.0% at 100% hydrogen. Fractography analysis revealed that the base and welded materials exhibited typical ductile fracture features in the absence of hydrogen, transitioning to a mixture of quasi-cleavage and micro-void coalescence (MVC) features in hydrogen environments. Additionally, with hydrogen, increased formation of secondary cracks was observed. Notably, the study identified the Hydrogen-Enhanced Localized Plasticity (HELP) mechanism as a probable contributor to hydrogen-assisted fracture.


21 July 2026 in Metals
Verified
Journal Article
Open access
PDF file
MSMatthew Scott
Matthew Scott
RWRashiga Walallawita
Rashiga Walallawita
MHMatthew C. Hinchliff
Matthew C. Hinchliff
DSDimitry Sediako
Dimitry Sediako
Hydrogen diffusion plays a central role in the susceptibility of steels to hydrogen embrittlement, yet reported diffusivity values often exhibit significant variability due to differences in experimental methodology. Gaseous hydrogen permeation experiments, while more representative of service conditions, are highly sensitive to surface boundary conditions and trapping effects, which can bias the diffusivity obtained from analysis. In this work, a gaseous hydrogen permeation methodology was developed at the High-Performance Powertrain Materials Laboratory (HPPM) at the University of British Columbia, Okanagan. A dedicated gas management system (GMS) was implemented to enable controlled pressure step transients, allowing partial permeation transients to be collected under gaseous charging conditions. This approach was applied to commercially pure iron and API 5L X60 pipeline steel to evaluate diffusion and trapping behaviour across materials with differing microstructural complexity. The results demonstrate that diffusivity obtained from transients spanning the full charging–discharging range (0–2 MPa) reflects an effective parameter influenced by reversible hydrogen trapping, whereas transients measured over incremental pressure steps (1–2 MPa) provide a more consistent estimate of lattice-controlled diffusion. The application of palladium coatings to the charging surface was found to promote hydrogen entry, reducing surface impedance effects and further improving agreement with Fickian diffusion behaviour.