In recent years, bio-based wood adhesives have gained an increased industrial and research interest as an environmentally friendly and renewable alternative to the commercial petroleum-based synthetic adhesives used in the wood-based industry. Due to its renewability, abundance, relatively low price, and good adhesion properties, starch is a promising natural feedstock for synthesizing bio-based adhesives for wood-based composites. This review aims to summarize the recent advances in developing sustainable starch-based wood adhesives for manufacturing non-toxic, low-emission wood composites with enhanced properties and lower environmental impact. Recent developments in starch modification, physical, and enzymatic treatments applied to improve the performance of starch-based wood adhesives, mainly in terms of improving their water resistance and bonding strength, are also outlined and discussed.
This study aimed to evaluate the effect of ammonium persulfate’s (APS) oxidation time on the characteristics of the cellulose nanocrystals (CNCs) of balsa and kapok fibers after delignification pretreatment with sodium chlorite/acetic acid. This two-step method is important for increasing the zeta potential value and achieving higher thermal stability. The fibers were partially delignified using acidified sodium chlorite for four cycles, followed by APS oxidation at 60 °C for 8, 12, and 16 h. The isolated CNCs with a rod-like structure showed an average diameter in the range of 5.5–12.6 nm and an aspect ratio of 14.7–28.2. Increasing the reaction time resulted in a gradual reduction in the CNC dimensions. The higher surface charge of the balsa and kapok CNCs was observed at a longer oxidation time. The CNCs prepared from kapok had the highest colloid stability after oxidation for 16 h (−62.27 mV). The CNCs with higher crystallinity had longer oxidation times. Thermogravimetric analysis revealed that the CNCs with a higher thermal stability had longer oxidation times. All of the parameters were influenced by the oxidation time. This study indicates that APS oxidation for 8–16 h can produce CNCs from delignified balsa and kapok with satisfactory zeta potential values and thermal stabilities.
25 July 2019 in Journal of the Korean Wood Science and Technology
The Journal of the Korean Wood Science and Technology (JKWST) launched in 1973 as an official publication of the Korean Society of Wood Science and Technology has been served as a core of knowledges on wood science and technology.
1 September 2020 in IOP Conference Series: Materials Science and Engineering
Chemical components content of seven Indonesian bamboo species were investigated. Bamboo species used in this study including Andong bamboo (Gigantochloa pseudoarundinacea), Tali bamboo (G.apus), Hitam bamboo (G. artoviolacea), Betung bamboo (Dendrocalamus asper), Sembilang bamboo (D. giganteus), Ampel bamboo (Bambusa vulgaris var. vulgaris), and Kuning bamboo (B. vulgaris var. striata). Holocellulose, alphacellulose, Klason lignin, acid-soluble lignin, extractives content, and pH value were determined. The highest holocellulose and alphacellulose content were found in Ampel and Hitam bamboo, respectively. Sembilang bamboo has the highest lignin content. Generally, Ampel bamboo has the highest extractives content. The pH value of the seven bamboo species showed that all bamboo species tend to be acidic.
Phenol-formaldehyde (PF) resin is one of the most well-known adhesives for exterior use. PF adhesive is one of the commercial thermoset polymers that is used extensively due to its many benefits. This study investigated the influence of different types and levels of catalysts, i.e., NaOH and CaCO3 at 1% and 5% based on the solids content of PF resin on the adhesive properties, adhesion, and cohesion strength of PF resin. The results show that the catalyst type significantly influenced the PF adhesive viscosity and pH. Furthermore, the catalyst level significantly affected the PF adhesive’s solids content, viscosity, and gelation time. The cohesion strength of PF-CaCO3-1% was more significant than the PF control at 75 °C. According to the DMA analysis, the mixed PF-NaOH-5% provided the highest storage modulus, followed by the PF-CaCO3-1%, with values that were not statistically different from one another. The adhesion strength of PF-CaCO3-1% was the highest, whereas the adhesion strength of the PF control was the lowest, as confirmed by the cohesion strength. According to the findings, adding CaCO3-1% as a catalyst of PF resin would result in better adhesive adhesion and cohesion properties for wood composites in the future.