This research highlights the critical role that entrepreneurial capital (EC) plays in organizational development and resilience by examining the connections between EC and the success of new joint ventures (NJVs) in developing nations. Corporate social responsibility (CSR) is becoming more popular in the early phases of a company’s growth because of its capacity to improve credibility and competitive differentiation. Traditionally associated with well-established corporations. This study uses a mediated-moderation model to explore theories on how EC affects the disruptive innovation, economic, social, legal, and environmental sustainability of NJVs. Using quantitative survey data from 270 NJVs, this paper highlights the strategic interdependencies influencing NJV trajectories, as well as the functions of disruptive innovation and CSR. The findings demonstrate that EC greatly enhances NJVs performance in every category, promoting CSR and innovative projects. NJVs benefit from early CSR participation because it reduces risks and boosts entrepreneurial vitality. Disruptive innovation transforms EC into measurable performance advantages. This study has important policy and management implications because it shows that NJVs can stay ahead of the competition and improve their performance by strategically using EC for CSR and innovation projects. Overall, this study emphasizes how crucial CSR is to the startup environment, supporting resilient and long-term growth in emerging economies.
This work presents ANSYS Workbench simulations analyzing fatigue crack propagation in high-performance aluminum alloys 2524-T3, 2024-T42, and 2024-T351 under stress ratios R = 0.1, 0.3, and 0.5 using pre-meshed crack tools and SMART Fracture automation. Key simulation outputs include crack length evolution, cycle count, equivalent stress intensity factor ranges (ΔK), and crack resistance curves (Kr). At R = 0.1, 2524-T3 exhibited the highest crack growth rate (da/dN = 3.20×10⁻⁸ mm/cycle, ΔK = 7.28 MPa√m, Nf ≈ 459×10⁶ cycles), while 2024-T351 showed the lowest rate (da/dN = 2.76×10⁻⁹ mm/cycle, ΔK = 1.65 MPa√m, Nf ≈ 5.27×10⁹ cycles) — a 10.4-fold reduction in da/dN and 11.5-fold increase in fatigue life. At R = 0.5, 2024-T351 achieved da/dN < 1.0×10⁻⁸ mm/cycle with Nf > 6×10⁹ cycles, outperforming 2024-T42 (da/dN = 3.82×10⁻⁹ mm/cycle, Nf ≈ 2.92×10⁹) and 2524-T3 (da/dN = 2.76×10⁻⁹ mm/cycle, Nf ≈ 5.27×10⁹). Kr curve analysis revealed steep resistance decay for 2524-T3 (R = 0.1), stable plateau behavior for 2024-T42 (R = 0.3–0.5), and rising Kr trends for 2024-T351 across all R-ratios, indicating active crack-tip shielding mechanisms. SEM fractography validated simulation trends: 2524-T3 showed brittle trans granular features with secondary crack density of 12.3 ± 2.1 cracks/mm²; 2024-T42 exhibited mixed-mode fracture with moderate dimple density (8.7 ± 1.4 μm⁻²); 2024-T351 displayed ductile dimple morphology with the highest dimple density (18.4 ± 2.6 μm⁻²) and minimal secondary cracking (2.1 ± 0.8 cracks/mm²). These microstructural metrics confirm 2024-T351 as the optimal candidate for fatigue-critical aerospace and automotive applications.