In this study, we investigate the dielectric, electric, and pyroelectric properties of Ba1−xCaxTiO3 (BCT) ceramics with compositions of x = 0.2, 0.25, and 0.3. The ceramics were synthesized using the solid-state reaction method. A microstructural analysis was performed using scanning electron microscopy (SEM), revealing that calcium concentration influences grain size and morphology, with BCT20 showing larger, hexagonal grains, while BCT25 and BCT30 exhibited smaller, irregular grains. Phase composition and crystalline structure were characterized via X-ray diffraction (XRD), which confirmed the absence of secondary phases and a predominantly tetragonal P4mm structure for BCT20 and BCT25. However, BCT30 showed an additional orthorhombic (Pbam) phase at 5.9 wt. % alongside the dominant tetragonal phase. Dielectric measurements revealed that increasing the calcium concentration shifts the temperature of dielectric permittivity maximum to lower values, correlating with a shift in the ferroelectric–paraelectric phase transition. Pyroelectric measurements indicated the highest pyroelectric current for BCT25, while BCT30 showed the maximum thermally stimulated depolarization current.
Novel phenylamine-substituted derivatives, possessing different photochromic groups, were investigated. The electrochemical activity of the monomers and polymers were studied by usage of the electrochemical and spectroelectrochemical measurements. Heterocyclic side rings influence on the oxidation potential of monomers, decreasing its value below oxidation potential in comparison to parent phenylamine units. The removal of electron is easier for diphenylamine derivatives than for the triphenylamine ones. Electroactivity of monomers allows to polymerize them into macromolecule chains. Triphenylamine-based polymers are more stable as a result of the enlarged conjugated systems. Furthermore, the energy gap value of the final polymer can be reduced by introduction of additional branch into the monomer structure.
Ba0.75Ca0.25TiO3 ceramics were successfully synthesized by a simple solid-state reaction method. This study examined the influence of sintering temperature on the structure, microstructure, dielectric properties and electrical behavior of the material. The XRD analysis reveals that the tetragonal phase (P4mm) is dominant in all the synthesized materials, with those sintered at T = 1400 °C and T = 1450 °C being single-phase, while others exhibit a minor orthorhombic phase (Pbnm). Higher sintering temperatures promoted better grain boundary formation and larger grain sizes. The electric permittivity increased with temperature up to T = 1400 °C, followed by a sharp decline at T = 1450 °C. Additionally, the Curie temperature decreased with increasing sintering temperature, indicating changes in phase transition characteristics. Thermal analysis showed that higher sintering temperatures led to sharper heat capacity peaks, while pyroelectric and thermally stimulated depolarization currents were maximized at T = 1400 °C due to oxygen vacancies. These findings highlight the significant impact of sintering temperature on the material’s structural and functional properties.
1 August 2017 in Spectrochimica Acta Part A: Molecular and Biomolecular Spectroscopy