Laser remelting is being explored as a viable technique for obtaining a graphite-free, defect-free surface layer on cast iron EN GJS 400-15. The goal is to obtain a large remelted layer along with a low surface roughness to enable a subsequent manual high-gloss surface finish. The impact of the laser remelting process parameters is evaluated by using samples with three different cooling rates, resulting in different graphite microstructures. By utilizing four passes and a laser power of 300 W, the smallest roughness and largest remelting depth are achieved. The remelted layer is mostly devoid of graphite particles. Subsequent manual polishing is performed to evaluate the potential for achieving a high-gloss finish with a roughness of Sa < 0.05 µm. Laser remelting alone does not improve visual appearance or reduce roughness. However, after manual polishing, the roughness of the laser-remelted surfaces with Sa = 0.018 µm is one order of magnitude smaller than the manually polished initial state. Graphite removal during laser remelting therefore makes it possible to achieve a conventional and high-gloss polish, overcoming the previous limitations of GJS materials.
11 February 2026 in International Journal of Metalcasting
This study investigates the microstructural evolution, mechanical performance, and residual stress distribution of AlSi11Mg alloy wheels produced by low-pressure die casting (LPDC) under various heat treatment conditions. Unlike conventional practice, where AlSi11Mg is often used without heat treatment, this work applied T6 and alternative heat treatments to assess their influence on critical wheel regions. Microstructural observations showed that the as-cast condition contained coarse dendrites and sharp Si particles, leading to low hardness and brittle behavior. Artificial aging alone produced limited precipitation hardening, whereas T6-treated samples exhibited refined and spheroidized Si morphologies, resulting in significantly higher yield strength, ultimate tensile strength, elongation, and hardness. Among the tested scenarios, Option #3 achieved the most balanced and consistent properties across all wheel regions. Residual stress simulations confirmed stress accumulation in hub and hub–spoke areas, a potential source of cracking. While T6 treatment maximized the strength, it also increased the residual stress; in contrast, limited heat treatments reduced the stress but compromised the mechanical performance. Complementary numerical simulations were conducted using Magmasoft and its Magmastress module to model both casting and heat treatment processes. Residual stress analyses highlighted that the highest residual stresses occur after quenching in T6-treated specimens. Long artificial aging time (Option #2) gives the lowest residual stress under T6-treated specimen groups. Stress relief annealing (Option #5) significantly reduced the residual stresses by 56–68%, reducing the risk of crack initiation. Overall, the study demonstrates that T6 heat treatment optimizes the mechanical performance in AlSi11Mg wheels, while stress relief annealing effectively decreases the residual stresses. These findings provide critical insights for the design, heat treatment, and quality assurance of aluminum alloy castings in automotive applications and potentially other thin-walled, complex components. Graphical Abstract
30 December 2025 in Dicle Üniversitesi Mühendislik Fakültesi Mühendislik Dergisi
Bu çalışma, döküm alüminyum alaşımlarında üretim sürecinde ortaya çıkan kalıntı gerilmelerin nedenlerini, ölçüm yöntemlerini ve önleme stratejilerini incelemektedir. Kalıntı gerilmeler; ısıl işlem, talaşlı imalat, kaynak gibi işlemlerden sonra, dış yük olmadan malzeme içinde oluşan elastik gerilmelerdir. Bu gerilmeler, parçanın yorulma ömrünü, mekanik performansını ve boyutsal doğruluğunu doğrudan etkiler. Özellikle T6 gibi ısıl işlem süreçlerinde, su verme sırasında meydana gelen ani sıcaklık değişimleri ciddi kalıntı gerilmeler yaratabilir. Çalışmada delik delme, halka çekirdek ve kontur gibi tahribatlı; X-ışını kırınımı, ultrasonik ve nötron kırınımı gibi tahribatsız yöntemler detaylı şekilde incelenmiş, bunların avantaj ve dezavantajları karşılaştırılmıştır. Ayrıca, sonlu elemanlar analizleriyle yapılan analitik ölçüm yöntemlerine de yer verilmiştir. Yorulma ömrü açısından, çeki kalıntı gerilmeleri zararlı olurken, bası gerilmeleri ömrü artırabilir. Bu nedenle kalıntı gerilmelerin ölçümü kadar kontrolü de önemlidir. Gerilme giderme tavlaması, düşük sıcaklıkta yaşlandırma ve yüzey işlemleri gibi yöntemlerle bu gerilmeler azaltılabilir. Sonuç olarak, kalıntı gerilmelerin dikkatli yönetimi, daha dayanıklı ve güvenilir mühendislik parçaları üretimini mümkün kılar.
24 May 2021 in Dokuz Eylül Üniversitesi Mühendislik Fakültesi Fen ve Mühendislik Dergisi
In this study, the natural frequencies of Solaris 10 Solar Car’s 2018 and 2019-Model wheels were determined experimentally by the impact hammer test under free-free boundary conditions and the results were compared with the natural frequency results obtained using ANSYS FEA software. Comparing the numerical and experimental vibration analysis, a maximum percent error of 7.46% was observed. The 7th and upper mode frequencies of 2018 and 2019 wheel models were shown to be above 200 Hz and the experimental results were validated. After expressing the mode shapes in the ANSYS-Modal Analysis, a parametric study was performed for the 2019 wheel model using the ANSYS- Parametric Design. As a result of the parametric design, the mass of the 2019 wheel model was decreased by 6.5% while maximum equivalent von Mises stress was decreased by 2%. Thus, a lighter wheel design was obtained with ANSYS FEA software and maximum equivalent von Mises stress value was achieved to be below pre-defined limit of 120 (MPa).