The leaching of copper from industrial copper ore with 4.8 wt % chalcopyrite by acidified nitrate with seawater based media was investigated. Water quality (pure water and seawater), temperature (25–70 °C), reagent concentration, and nitrate type (sodium and potassium) were studied variables. Leaching conditions were: 100 g ore/1 L solution; P80 of 62.5 µm; 400 rpm and leaching time, varying between 3 and 7 days. Nitrates in sulfuric acid are known to be good oxidants for sulfide ores. This study showed that up to 80 wt % copper could be extracted at 45 °C in 7 days. In the absence of nitrate, under the same leaching conditions, only a 28 wt % copper extraction was achievable. The extraction rate increased to 97.2 wt % when leach temperature was increased to 70 °C in nitrate-chloride-acid media. The presence of chloride ions also increased the copper extraction rate. The copper extraction achieved in seawater systems were higher than in water systems under the same leaching conditions (increased by an average of 18 wt %). This effect can be attributable to the contribution of chloride that increases proton (H+) activity.
21 July 2021 in Journal of Material Cycles and Waste Management
The aim of this study was to improve the dissolution of copper sulfide ore composed mainly of chalcopyrite (1.21 wt %) and bornite (0.54 wt %) using a pretreatment before leaching. The effect of the pretreatment on copper sulfide dissolution was investigated using different types of leaching. Three sets of experimental tests were performed (flask, reactor and mini-column). Using experimental design, three operational variables in the ore pretreatment were evaluated: chloride concentration (20, 50 and 90 kg/t), repose time (7, 20 and 40 days) and repose temperature (20 and 50 °C). A maximum of 93% copper dissolution was obtained when the ore was treated with 90 kg Cl−/t ore, 40 d of repose time and 50 °C in flask leaching. Without any ore pretreatment, 53% copper dissolution was achieved. Using reactor leaching, an 85% copper dissolution was obtained using pretreatment stage. Without this pretreatment, only 55% copper dissolution was obtained. The final test, which involved leaching a pretreated ore in a mini-column at room temperature, yielded 49% copper dissolution. The data showed that repose time and temperature were the most important variables affecting copper extraction in the pretreatment stage. This study indicates that pretreatment has a positive effect on copper dissolution from primary copper sulfide ore in an acid-chloride medium. It also provides a feasible alternative for treating primary copper sulfide ores at the industrial level.
This work investigates the effect of an agglomeration and curing pretreatment on leaching of a copper sulfide ore, mainly chalcopyrite, using mini-columns in acid-nitrate-chloride media. Ten pretreatment tests were conducted to evaluate different variables, namely the addition of nitrate as NaNO3 (11.7 and 23.3 kg/ton), chloride as NaCl (2.1 and 19.8 kg/ton), curing time (20 and 30 days) and repose temperature (25 and 45 °C). The optimum copper extraction of 58.6% was achieved with the addition of 23.3 kg of NaNO3/ton, 19.8 kg of NaCl/ton, and after 30 days of curing at 45 °C. Under these pretreatment conditions, three samples of ore were leached in mini-columns. The studied parameters were temperature (25 and 45 °C) and chloride concentration (20 and 40 g/L). The optimum copper extraction of 63.9% was obtained in the mini-column leaching test at 25 °C, with the use of 20 g/L of chloride. A higher temperature (45 °C) and a higher chloride concentration (40 g/L) negatively affected the extraction. The pretreatment stage had favorable effects, in terms of accelerating copper dissolution and improving leaching of copper sulfide ore in acid-nitrate-chloride media. Waste salts from caliche industry and waste brine from reverse osmosis can be used for providing the nitrate and chloride media.
In this paper, the effect of the cupric and chloride ions concentrations on copper dissolution from chalcopyrite concentrate was studied in acidified media. Variables included three different concentrations of Cu2+ (0.5, 1.5, and 2.5 g L−1), four different concentrations of Cl− (0, 5, 7, and 10 g L−1), two different pH values of 1 and 2, and a constant temperature of 60 °C. Results indicated that addition of Cl− to the system improves copper extractions, especially at higher concentrations of Cu2+. Initial copper concentrations in the leaching solution did not significantly affect the copper extraction when Cl− was not present. Better copper extractions were obtained at pH 1 as compared with pH 2. As the Cu2+ and Cl− concentrations were increased, higher values of redox potential were obtained. According to the formation constants of the chloro-complexes, the predominant species in the Cu2+/Cl− system in the studied interval were CuCl+ and Cu2+. Using a model of copper speciation in the experimental range predicted for a single copper concentration with increasing Cl− concentration, the Cu2+ concentration decreased significantly while the concentration of the chloro-complex species CuCl+ increased. In the leached residue, evidence of sulfur formation was found using SEM and corroborated by XRD analysis. When chloride is present in the medium, the amounts of copper and iron in the residue decrease, confirming a positive effect of chloride on the extraction of copper from concentrate for the studied conditions.