In this work, a series of Al2O3–SiO2/water hybrid nanofluid with different volume fractions and surfactant types were prepared. The Al2O3 and SiO2 were synthesized using the sol-gel method, and ultrasonic vibration was used to disperse the powders into the DI water to form nanofluids. The effects of anionic (SDS), cationic (CTAB) and nonionic (PVP) surfactants toward the stability, electrical conductivity, and viscosity of the nanofluid were then investigated. Zeta potential analysis, spectral analysis method, sedimentation method, and centrifugation method were used to compare the stability of the nanofluids. The obtained results indicated that the surfactant played an important role in dispersing the nanoparticles (NPs) and forming stable nanofluids. Nanofluids with low concentration of Al2O3 showed good dispersion in water, but it tended to aggregate when the amount used was higher. The viscosity of nanofluids increased slightly when the surfactant was added due to the increase of solid-phase concentration in the nanofluids. SDS positively affected the dispersion and stability of the nanofluids, and the best ratio of Al2O3:SiO2 was at 30:70. The electrical conductivity increased with temperature, and nanofluid containing CTAB and SDS had a higher increment in conductivity.
Iron Oxide Nanoparticles (IONPs) have received unprecedented interest in various applications. The main challenges in IONPs are fluid stability due to agglomeration in a saline condition. This paper aims to investigate the colloidal stability of citric acid (CA), sodium dodecyl sulphate (SDS) and polyvinyl alcohol (PVA) under various molar ratios and levels of salinity. Firstly, the IONPs were synthesized using a facile co-precipitation approach. Secondly, the IONPs were coated using a simple dip-coating method by varying the molar ratio of CA, SDS and PVA. Next, the coated IONPs were characterized by using an X-ray Diffractometer (XRD), Fourier transform infrared spectroscopy (FTIR), and a Field Emission Scanning Electron Microscope (FESEM) for the morphological and crystallographic study of coated IONPs. Finally, the coated IONPs were characterized for their zeta potential value and hydrodynamic size using a Zetasizer and their turbidity was measured using a turbidity meter. It was found that at a low salinity level, 0.07 M of CA-IONPs, a high zeta potential value, a smaller hydrodynamic size, and a high turbidity value of −40.9 mV, 192 nm and 159 NTU were observed, respectively. At a high salinity level, 1.0 M SDS-IONPs recorded a high zeta potential value of 23.63 mV, which corresponds to a smaller hydrodynamic size (3955 nm) and high turbidity result (639 NTU). These findings are beneficial for delivering cutting-edge knowledge, especially in enhanced oil recovery (EOR) applications.
Many studies have investigated natural convection heat transfer from the outside surface of horizontal and vertical cylinders in both constant heat flux and temperature conditions. However, there are poor studies in natural convection from inclined cylinders. In this study, free convection heat transfer was examined experimentally from the outside surface of a cylinder for glycerol and water at various heat fluxes. The tests were performed at 10 different inclination angles of the cylinder, namely, φ = 0°, 10°, 20°, 30°, 40°, 50°, 60°, 70°, 80°, and 90°, measured from the horizon. Our results indicated that the average Nusselt number reduces with the growth in the inclination of the cylinder to the horizon at the same heat flux, and the average Nusselt number enhanced with the growth in heat flux at the same angle. Also, the average Nusselt number of water is greater than that of glycerol. A new experimental model for predicting the average Nusselt number is suggested, which has a satisfactory accuracy for experimental data.
In this study, ZnO nanoparticles were synthesized using a sol-gel method for oil upgrading and wax deposition control. The synthesized ZnO nanoparticles were used to measure viscosity and wax deposition in the heavy crude oil and to investigate the effectiveness of the nanoparticles in the reduction of viscosity and wax deposition control of the heavy crude oil. This study investigated the effect of calcination temperature on ZnO nanoparticles during synthesis towards viscosity reduction and wax deposition control. ZnO nanoparticles were calcined at different temperatures ranging from 300 to 900 °C. The calcined ZnO nanoparticles were characterized using X-ray diffraction (XRD), Field Emission Scanning Electron microscope (FESEM), and Energy-dispersive X-ray spectroscopy (EDX) for its structure, size, shape, and morphology. The characterization results showed a hexagonal wurtzite structure of ZnO nanoparticles. The physical properties and rheology of heavy crude oil were characterized by using Electronic Rheometer and cold finger method to analyze the viscosity, shear rate, and wax deposition of the heavy crude oil for performance study. Decreased in crystallite size from 15.59 to 12.84 nm was observed with increasing calcination temperature from 300 to 400 °C, and a further increase of calcination temperature from 400 to 900 °C, the crystallite size increased from 12.84 to 41.58 nm. The degree viscosity reduction (DVR %) of heavy crude oil was observed to increase by 41.7%, with decreasing ZnO nanoparticles size from 30.11 nm to 12.84 nm. The optimum calcination temperature was 400 °C. Wax deposition decreases by 32.40% after the addition of ZnO nanoparticles into heavy crude oil.
In the current paper, fundamental aspects of heavy oil and wax deposition problems are defined. Wax or in another term is cloud point occur when the oil starts to precipitate. When it’s started to precipitate, it can cause major problem to industry of oil and gas. In this study, ZnO nanoparticles were chosen to study the effect of varying molar ratio from 1:1, 1:2, 1:3 to the morphology and size of the nanoparticle. The structures and properties were recognized with energy dispersive X-ray (EDX), field emission scanning electron microscopy (FE-SEM), and X-ray diffraction (XRD) methods. EDX and FE-SEM is to study the morphology of ZnO structure while XRD is to determine the purity and size of the nanoparticle. From the study, 1:1 ratio has the smallest size of nanoparticle with 10.37 nm while 1:2 and 1:3 give the size of 12.3 nm and 16.37 nm respectively. As the molar ratio is increases, the size of nanoparticle become bigger. The influenced of ZnO nanoparticles on rheological behaviour of model oils and the wax content is reported. From the study, the addition of ZnO nanoparticle reduced the rheology behaviour of crude oil by varying nanoparticle sizes, temperature and shear rate. ZnO nanoparticle can reduce the deposition of wax up to 50% with influenced of smaller nanoparticle size. Effect of size of nanoparticle highly impact the viscosity and wax content. This prove that, by introducing nanoparticle into crude oil, wax content can be reduced thus decrease the chance for crude to precipitate.