The principle of wood impregnation entails treating wood with a monomer/impregnating agent that diffuses into the cell walls, often followed by polymerization to change desired properties. Numerous studies related to this matter have been reported and continue to attract more interest, as wood impregnation can significantly improve wood properties. These processes can be grouped into two approaches: active modification involves the chemical alteration of wood structure by cross-linking, and passive modification features filling of cell cavities and/or cell walls with impregnating agents without any chemical reaction taking place. Wood impregnations could have resulted in an increase in its weight gain due to impregnating agents filling its cavities. It will diminish the utilization of wood as an engineering material in selected application fields. Owing to the extensive literature available, this article summarizes the representative achievements of wood impregnation. The mechanisms, benefits, and drawbacks of various impregnating agents on wood properties, along with grouping the impregnating agents that cause greater or lesser weight gain of wood were analyzed, compared, and evaluated. Thus, according to the application state of wood impregnations, the problems existing in those processes and the developmental trends in the future are also discussed in this review.
Cross-laminated timber (CLT) has become a popular engineered wood product due to its innovative properties and rapid development, which involves the use of various wood species and adhesives. This study aimed to assess the effect of glue application on the bonding strength, delamination, and wood failure of CLT made from jabon wood and bonded with a cold-setting melamine-based adhesive at three different rates: 250, 280, and 300 g/m2. The adhesive was composed of melamine–formaldehyde (MF) by adding 5% citric acid, 3% polymeric 4,4-methylene diphenyl diisocyanate (pMDI), and 10% wheat flour. Adding these ingredients increased the adhesive viscosity and decreased the gelation time. The CLT samples, made using cold pressing in the melamine-based adhesive at a pressure of 1.0 MPa for 2 h, were evaluated as per the standard EN 16531:2021. The results revealed that a higher glue spread resulted in a greater bonding strength, lower delamination, and a higher wood failure. The glue spread was shown to have a more significant influence on wood failure compared with delamination and the bonding strength. The application of 300 g/m2 glue spread (MF-1) on the jabon CLT led to a product that met the standard requirements. The use of modified MF in cold-setting adhesive produced a potential product that could be a feasible option for future CLT production in terms of its lower heat energy consumption.
High demand for Agarwood (Gaharu) from natural forest causes the decreasing of their population. In 2004, Indonesia proposed that all natural Agarwood from Gyrinops and Aquilaria generas should be included in the Appendix II CITES (Convention on International Trade in Endangered Species) list, which could be internationally traded but in certain quota. This paper deals with anatomical observation and characterization on basic properties to find out the difference between Gyrinops and Aquilaria for classification and standardization. Explorations have been conducted at community forests in Flores, East Nusa Tenggara for Gyrinops versteegii (Gilg) Domke; while A. malaccensis Benth., A. microcarpa Baill., A. beccariana Tiegh., and Aquilaria sp. were extracted from Sangau and Ketapang Regencies, West Kalimantan. Wood samples were taken by drilling the trees stem by using a Drill tool to get a pencil-shaped sample of about 20 cm in length and 0.5 cm in diameter. Another sample in form of chips contain bark and wood were also extracted. The results showed that the average specific gravity of Gyrinops and Aquilaria was between 0.31 – 0.35, therefore it was included in the Strength Class IV. Chemical components of injured G. versteegii contained 50.74% holocelullose, 30.50% α-cellulose, 31.98% lignin, and 16.69% extractives. The composition of ray cells in G. versteegii was more complex than Aquilaria generas.
1 November 2019 in IOP Conference Series: Earth and Environmental Science
Sonokeling (Dalbergia latifolia Roxb) stands are widely lost throughout the world. Sonokeling is currently classified as an Appendix II CITES (Convention on International Trade in Endangered Species of Wild Fauna and Flora) wood. Therefore, a study on the existence and characteristics of Sonokeling were expected to contribute in providing population data and basic properties of the wood. Exploration was conducted in Plot No. 25, KPH (Forest Management Unit) Gundih, Perum Perhutani Cepu, Central Java. Sonokeling stands have been planted since 1975 (more than 40 years-old) in an area of 54.20 ha, which was not productive for Teak and mixed with Mahogany. Sample was taken from upper part of stem with around 30 cm in diameter and 30 cm in length. The sample was further cutted into 2 x 2 x 2 cm for physical, 30 x 2 x 2 cm for Modulus of Elasticity (MOE) and Modulus of Rupture (MOR), and 4 x 2 x 2 cm for Compression Strength Parallel to the Grain (CSPG) tests. The results showed that specific gravity of sapwood dan heartwood were 0.79 and 0.82, respectively. The average values of MOE, MOR, and CSPG were 117,722, 1122.19, and 1022.93 kgf/cm2, respectively. Therefore, Sonokeling can be classified into Strength Class II.
The effect of NaOH, succinic acid and their combination used as pretreatments on selected properties of densified wood samples of pisang putih (Mezzettia spp.), nyatoh (Palaquium spp.) and sepetir (Sindora spp.) has been studied. The properties of these samples were then compared with those of untreated wood (control) and densified wood samples without any pretreatment (HD wood). For alkali-pretreatment, after immersion in 10% NaOH (w/w) for 1, 2 and 3 h, the samples were immediately compressed; for acid-pretreatment, the sample was impregnated with 10% succinic acid (w/w) using a vacuum of −50 kPa for 30 min and a pressure of 7 bar for 2 h before pressing; while for the combination-pretreatment, the sample was initially immersed in 10% NaOH then impregnated with 10% succinic acid (w/w) and finally densified/compressed. Compression was applied in a radial direction and carried out in an open system using a hot press machine at 180 °C and 7 MPa specific pressure for 30 min with a 40% compression ratio. The results showed that densified wood with or without pretreatment had a higher specific gravity (SG) than the control, whereas sepetir wood showed the greatest increase in SG. The alkali- and combination-pretreatments resulted in a higher C-set value than in the control, HD and acid-pretreated samples. Acid-pretreatment resulted in the best improvement in dimensional stability compared to the other pretreatments. Increasing the immersion time in NaOH solution was proven to be able to increase dimensional stability both in alkali- and combination-pretreatments, although water absorption values varied.