Third-generation advanced high-strength steels (AHSS) containing metastable retained austenite are being developed for the structural components of vehicles to reduce vehicle weight and improve crash performance. The goal of this work was to compare the effect of temperature on austenite stability and tensile mechanical properties of two steels, a quenched and partitioned (Q&P) steel with a martensite and retained austenite microstructure, and a medium manganese transformation-induced plasticity (TRIP) steel with a ferrite and retained austenite microstructure. Quasi-static tensile tests were performed at temperatures between −10 and 85 °C for the Q&P steel (0.28C-2.56Mn-1.56Si in wt.%), and between −10 and 115 °C for the medium manganese TRIP steel (0.14C-7.14Mn-0.23Si in wt.%). X-ray diffraction measurements as a function of strain were performed from interrupted tensile tests at all test temperatures. For the medium manganese TRIP steel, austenite stability increased significantly, serrated flow behavior changed, and tensile strength and elongation changed significantly with increasing temperature. For the Q&P steel, flow stress was mostly insensitive to temperature, uniform elongation decreased with increasing temperature, and austenite stability increased with increasing temperature. The Olson–Cohen model for the austenite-to-martensite transformation as a function of strain showed good agreement for the medium manganese TRIP steel data and fit most of the Q&P steel data above 1% strain.
The strain-induced diffusionless shear transformation of retained austenite to martensite during straining of transformation induced plasticity (TRIP) assisted steels increases strain hardening and delays necking and fracture leading to exceptional ductility and strength, which are attractive for automotive applications. A novel technique that provides the retained austenite volume fraction variation with strain with improved precision is presented. Digital images of the gauge section of tensile specimens were first recorded up to selected plastic strains with a stereo digital image correlation (DIC) system. The austenite volume fraction was measured by synchrotron X-ray diffraction from small squares cut from the gage section. Strain fields in the squares were then computed by localizing the strain measurement to the corresponding region of a given square during DIC post-processing of the images recorded during tensile testing. Results obtained for a QP980 steel are used to study the influence of initial volume fraction of austenite and the austenite transformation with strain on tensile mechanical behavior.
2 April 2019 in SAE International Journal of Advances and Current Practices in Mobility
Adiabatic heating during plastic straining can slow the diffusionless shear transformation of austenite to martensite in steels that exhibit transformation induced plasticity (TRIP). However, the extent to which the transformation is affected over a strain rate range of relevance to automotive stamping and vehicle impact events is unclear for most third-generation advanced high strength TRIP steels. In this study, an 1180MPa minimum tensile strength TRIP steel with carbide-free bainite is evaluated by measuring the variation of retained austenite volume fraction (RAVF) in fractured tensile specimens with position and strain. This requires a combination of servo-hydraulic load frame instrumented with high speed stereo digital image correlation for measurement of strains and ex-situ synchrotron x-ray diffraction for determination of RAVF in fractured tensile specimens. Specifically, the potentially competing effects of strain rate on austenite transformation to martensite were investigated to determine which predominate at nominal strain rates of 0.5 s-1, 5 s-1, 50 s-1 and 500 s-1. A corresponding decrease in austenite volume fraction at a fixed true strain with strain rate suggests that austenite transformation to martensite with strain is accelerated with increased strain rate despite potential energetic inhibition of the transformation due to adiabatic heating. Increased transformation rate to martensite results in increased work hardening rates, strengths, and elongations with strain rate increases to 500 s-1. Observations are discussed in the context of contributing mechanisms both favoring and inhibiting the strain-assisted transformation of austenite to martensite.