Xingui Zhou

Prof. Dr. Xingui Zhou

National University of Defense Technology

Research Focus & Metrics

Academic Career Length

7Years (2020-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
25 February 2024 in Nanomaterials
Verified
Journal Article
Open access
PDF file
XZXiangzhe Zhang
Xiangzhe Zhang
BLBowen Lv
Bowen Lv
HWHaitao Wei
Haitao Wei
XZXingui Zhou
Xingui Zhou
GPGang Peng
Gang Peng
SQShiqiao Qin
Shiqiao Qin
Violet phosphorus (VP), a novel two-dimensional (2D) nanomaterial, boasts structural anisotropy, a tunable optical bandgap, and superior thermal stability compared with its allotropes. Its multifunctionality has sparked widespread interest in the community. Yet, the VP’s air susceptibility impedes both probing its intrinsic features and device integration, thus making it of urgent significance to unveil the degradation mechanism. Herein, we conduct a comprehensive study of photoactivated degradation effects on VP. A nitrogen annealing method is presented for the effective elimination of surface adsorbates from VP, as evidenced by a giant surface-roughness improvement from 65.639 nm to 7.09 nm, enabling direct observation of the intrinsic morphology changes induced by photodegradation. Laser illumination demonstrates a significant thickness-thinning effect on VP, manifested in the remarkable morphological changes and the 73% quenching of PL intensity within 160 s, implying its great potential for the efficient selected-area etching of VP at high resolution. Furthermore, van der Waals passivation of VP using 2D hexagonal boron nitride (hBN) was achieved. The hBN-passivated channel exhibited improved surface roughness (0.512 nm), reduced photocurrent hysteresis, and lower responsivity (0.11 A/W @ 450 nm; 2 μW), effectively excluding adsorbate-induced electrical and optoelectrical effects while disabling photodegradation. Based on our experimental results, we conclude that three possible factors contribute to the photodegradation of VP: illumination with photon energy higher than the bandgap, adsorbed H2O, and adsorbed O2.

Verified
Journal Article
Open access
PDF file
HWHaitao Wei
Haitao Wei
BLBowen Lv
Bowen Lv
MZMengya Zhang
Mengya Zhang
XZXiangzhe Zhang
Xiangzhe Zhang
XZXingui Zhou
Xingui Zhou
TYTongcheng Yu
Tongcheng Yu
The near-infrared photodetection of monolayer MoS2 can be achieved using upconverted nanoparticles (UCNPs). Herein, we demonstrated that gold nanorods (Au NRs) further enhanced the near-infrared photoresponsivity of a hybrid device via the surface plasmon enhancement of the localized field. We synthesized a three-layer device comprising Au NRs, UCNPs (NaYF4:Yb3+, Er3+), and monolayer MoS2, and examined its photoelectric characteristics using laser irradiation with varying power densities at 980 nm, the excitation wavelength of UCNPs. Compared with a device without Au NRs, the photoelectric response of the three-layer device was greatly improved at 5 V bias, and photoresponsivity was increased at visible wavelengths (450, 532, and 635 nm). This study contributes to the knowledge of two-dimensional materials for the development of hybrid photoelectronic devices.

12 May 2022 in Multidiscipline Modeling in Materials and Structures
Verified
Journal Article
Closed access
CLChang Li
Chang Li
XZXingui Zhou
Xingui Zhou
QGQuanchao Gu
Quanchao Gu
XZXingui Zhou
Xingui Zhou
HWHonglei Wang
Honglei Wang
Purpose: A continuous chemical vapor deposition (CVD) method has been used to fabricate pyro-carbon (PyC) coating on continuous silicon carbide (SiC) fibers. The paper aims to evaluate these coated fibers by testing filament tensile and using microstructure characterization.Design/methodology/approach: The continuous SiC fiber-reinforced SiC matrix (SiC/SiC) composite is widely studied in aerospace and nuclear applications. The PyC is the probable option in fusion and fast reactor. However, the conventional fabrication method of PyC coating has some drawbacks influencing performance and efficiency.Findings: The results showed that PyC-coated SiC fibers with continuous CVD method are more straight than conventional ones and residual deformations could not be observed, and these PyC coatings have complete geometry and uniform thickness. In different process conditions, the thickness of PyC coating could control from ∼100 to ∼1,000 nm.Originality/value: The coated SiC fibers in a lower gas ratio (1:7 to 1:3), lower pressure (500–1,000 Pa) and appropriate winding speed (3 to 5 rpm) have relative high filament tensile strength (∼3.5 to ∼3.9 GPa). And the strength of coated SiC fibers has a negative correlation with the measured thickness of PyC coating. A distinctive growth process was discovered in the continuous CVD method. In a certain range, the quicker growing rate of PyC is obtained in shorter deposition time which means an efficient and quality method could be applied to fabricate coatings.

22 September 2020 in Research Square
Verified
Preprint
Open access
PDF file
XZXingui Zhou
Xingui Zhou
XZXingui Zhou
Xingui Zhou
HWHonglei Wang
Honglei Wang
B4C-TiB2 composite ceramics with ultra-high fracture toughness were successfully prepared via spark plasma sintering at 1900℃ using B4C and Ti3SiC2 as raw materials. The results show that compared with pure B4C ceramics sintered by SPS, the hardness of B4C-TiB2 composite ceramics is decreased, but the flexural strength and fracture toughness are significantly improved, especially the fracture toughness has been improved by leaps and bounds. When the content of Ti3SiC2 is 30vol.%, the B4C-TiB2 composite ceramic has the best comprehensive mechanical properties: hardness, bending strength and fracture toughness are 27.28 GPa, 405.11 MPa and 18.94 MPa·m1/2, respectively. The fracture mode of the B4C-TiB2 composite ceramics is a mixture of transgranular fracture and intergranular fracture. Two main two reasons for the ultra-high fracture toughness are the existence of lamellar graphite at the grain boundary, and the formation of a three-dimensional interpenetrating network covering the whole composite.

7 October 2020 in Research Square
Verified
Preprint
Open access
PDF file
XZXingui Zhou
Xingui Zhou
XZXingui Zhou
Xingui Zhou
HWHonglei Wang
Honglei Wang
B4C-TiB2 composite ceramics with ultra-high fracture toughness were successfully prepared via spark plasma sintering using B4C and 30 vol.% Ti3SiC2 as raw materials at different sintering temperatures. The results show that compared with pure B4C ceramics sintered by SPS, the flexural strength and fracture toughness are significantly improved, especially the fracture toughness has been improved by leaps and bounds. When the sintering temperature is 1900 ℃, the B4C-TiB2 composite ceramic has the best comprehensive mechanical properties: hardness, bending strength and fracture toughness are 27.28 GPa, 405.11 MPa and 18.94 MPa·m1/2, respectively. The main two reasons for the ultra-high fracture toughness are the formation of TiB2 three-dimensional network covering the whole composites, and the existence of lamellar graphite at the grain boundary.