For the example of PRFBKh6-2 alloy and P6M5 steel powders, the structure of plasma coatings after electromechanical treatment is investigated by scanning probe microscopy. After such treatment, ultradisperse and nano hardening phases are formed in the coating. These phases are formed by the decomposition of the coating’s initial fast-quenched structure in high-speed treatment. The formation of characteristic structural zones hardened by nanoparticles and ultradisperse particles is analyzed; the proportions of nanoparticles and ultradisperse particles are determined by the parameters of the sprayed powder and the conditions of plasma spraying and subsequent electromechanical treatment.
1 February 2018 in Surface and Coatings Technology
Changes of structure, phase composition and microhardness in high-strength α + β titanium alloy were investigated after electromechanical treatment (EMT) and subsequent aging. The EMT was performed with alternating current density (j of 300 and 600 A/mm2). The aging was performed upon heating at 600 °C and exposure for 14 h. Methods of scanning electron microscopy, X-ray phase structure, micro X-ray spectral and durometric analyses were used. Modified layers (up to 200–250 µm in depth) on the surface of α + β titanium alloy were formed due to intensive thermo-deformation during the EMT and the following aging. The structure of the surface layer was characterized by high dispersivity (with particle sizes of about 30–500 nm), significant concentration heterogeneity (due to redistribution of the alloying elements and changes in the volume ratio of α- and β-phases), distortions in the crystal structure, increased levels of microstrain and microstress (2–2.5 times as compared to the initial) and increases in microhardness (by 30–40%).