Aim: Total knee arthroplasties have reached a high grade of quality and safety, but most often fail because of aseptic implant loosening caused by polyethylene wear debris. Wear is generated at the articulating surfaces, e.g. caused by third-body particles. The objective of this experimental study was to determine the wear of tibial polyethylene inserts combined with metallic and ceramic femoral components under third-body wear conditions initiated by bone cement particles. Methods and Materials: Wear testing using a cemented unconstrained bicondylar knee endoprosthesis (Multigen Plus CR knee system) was performed in a knee wear simulator. Tibial polyethylene inserts were combined with the identical femoral component design, but made of two different materials (cobalt-chromium and ceramic). Bone cement debris including zirconium oxide particles was added every 500,000 cycles between the articulating surfaces. After 5 million load cycles, the amount of wear was determined gravimetrically and compared with results from standard wear test conditions. The surfaces of tibial inserts were also analyzed. Results: The average gravimetrical wear of the tibial polyethylene inserts in combination with cobalt-chromium and ceramic femoral components under third-body wear conditions amounted to 31.88 ± 4.53 mg and 13.06 ± 1.88 mg after 5 million cycles, respectively, and was higher than under standard wear test conditions in both cases. Conclusions: The wear simulator test demonstrates that wear of polyethylene inserts under third-body wear conditions, in combination with ceramic femoral components, was significantly lower than with metallic femoral components.
By means of plasma polymerization, positively charged, nanometre-thin coatings can be applied to implant surfaces. The aim of the present study was to quantify the adhesion of human bone cells in vitro and to evaluate the bone ongrowth in vivo, on titanium surfaces modified by plasma polymer coatings. Different implant surface configurations were examined: titanium alloy (Ti6Al4V) coated with plasma-polymerized allylamine (PPAAm) and plasma-polymerized ethylenediamine (PPEDA) versus uncoated. Shear stress on human osteoblast-like MG-63 cells was investigated in vitro using a spinning disc device. Furthermore, bone-to-implant contact (BIC) was evaluated in vivo. Custom-made conical titanium implants were inserted at the medial tibia of female Sprague-Dawley rats. After a follow-up of six weeks, the BIC was determined by means of histomorphometry. The quantification of cell adhesion showed a significantly higher shear stress for MG-63 cells on PPAAm and PPEDA compared to uncoated Ti6Al4V. Uncoated titanium alloyed implants showed the lowest BIC (40.4%). Implants with PPAAm coating revealed a clear but not significant increase of the BIC (58.5%) and implants with PPEDA a significantly increased BIC (63.7%). In conclusion, plasma polymer coatings demonstrate enhanced cell adhesion and bone ongrowth compared to uncoated titanium surfaces.
20 May 2017 in Knee Surgery, Sports Traumatology, Arthroscopy
Purpose The objective of this study was to evaluate the in vivo wear resistance of cobalt-chromium femoral components coated with titanium nitride (TiN). Our null hypothesis was that the surface damage and the thickness of the TiN coating do not correlate with the time in vivo. Methods Twenty-five TiN-coated bicondylar femoral retrievals with a mean implantation period of 30.7 ± 11.7 months were subjected to an objective surface damage analysis with a semi-quantitative assessment method. A visual examination of scratches, indentations, notches and coating breakthroughs of the surfaces was performed. The roughness and the coating thickness of the TiN coating were evaluated in the main articulation regions. Results Narrow scratches and indentations in the range of low flexion angles on the retrieval surfaces were the most common modes of damage. There was no evidence of delamination on the articulation surface but rather at the bottom of isolated severe indentations or notches. An analysis of three retrievals revealed a coating breakthrough in the patellofemoral joint region, resulting from patella maltracking and a dislocation. The arithmetical mean roughness of the TiN surface slightly increased with the implantation period. In contrast, the maximum peak height of the roughness profile was reduced at the condyles of the retrieved components in comparison with new, unused surfaces. No significant association between the coating thickness and implantation period was determined. Moreover, the measured values were retained in the range of the initial coating thickness even after several years of in vivo service. Conclusions As was demonstrated by the results of this study, the surface damage to the TiN coating did not deteriorate with the implantation period. The calculated damage scores and the measured coating thickness in particular both confirmed that the TiN coating provides low wear rates. Our findings support the use of wear-resistant TiN-coated components in total knee arthroplasty with the objective of reducing the risk of aseptic loosening. However, in terms of TiN-coated femoral components, particular attention should be paid to a correct patellar tracking in order to avoid wear propagation at the implant.
25 April 2013 in Journal of Materials Science: Materials in Medicine
The aim of the present study was to evaluate the biotribology of current surface modifications on femoral heads in terms of wettability, polyethylene wear and ion-release behavior. Three 36 mm diameter ion-treated CoCr heads and three 36 mm diameter TiNbN-coated CoCr heads were articulated against sequentially cross-linked polyethylene inserts (X3) in a hip joint simulator, according to ISO 14242. Within the scope of the study, the cobalt ion release in the lubricant, as well as contact angles at the bearing surfaces, were investigated and compared to 36 mm alumina ceramic femoral heads over a period of 5 million cycles. The mean volumetric wear rates were 2.15 ± 0.18 mm3·million cycles−1 in articulation against the ion-treated CoCr head, 2.66 ± 0.40 mm3·million cycles−1 for the coupling with the TiNbN-coated heads and 2.17 ± 0.40 mm3·million cycles−1 for the ceramic heads. The TiNbN-coated femoral heads showed a better wettability and a lower ion level in comparison to the ion-treated CoCr heads. Consequently, the low volumes of wear debris, which is comparable to ceramics, and the low concentration of metal ions in the lubrication justifies the use of coated femoral heads.