Pyrolysis of raw pine bark, pine, and Douglas-Fir bark was examined. The pyrolysis oil yields of raw pine bark, pine, and Douglas-Fir bark at 500 °C were 29.18%, 26.67%, and 26.65%, respectively. Both energy densification ratios (1.32–1.56) and energy yields (48.40–54.31%) of char are higher than pyrolysis oils (energy densification ratios: 1.13–1.19, energy yields: 30.16–34.42%). The pyrolysis oils have higher heating values (~25 MJ/kg) than bio-oils (~20 MJ/kg) from wood and agricultural residues, and the higher heating values of char (~31 MJ/kg) are comparable to that of many commercial coals. The elemental analysis indicated that the lower O/C value and higher H/C value represent a more valuable source of energy for pyrolysis oils than biomass. The nuclear magnetic resonance results demonstrated that the most abundant hydroxyl groups of pyrolysis oil are aliphatic OH groups, catechol, guaiacol, and p-hydroxy-phenyl OH groups. The aliphatic OH groups are mainly derived from the cleavage of cellulose glycosidic bonds, while the catechol, guaiacol, and p-hydroxy-phenyl OH groups are mostly attributed to the cleavage of the lignin β–O-4 bond. Significant amount of aromatic carbon (~40%) in pyrolysis oils is obtained from tannin and lignin components and the aromatic C–O bonds may be formed by a radical reaction between the aromatic and aliphatic hydroxyl groups. In this study, a comprehensive analytical method was developed to fully understand and evaluate the pyrolysis products produced from softwood barks, which could offer valuable information on the pyrolysis mechanism of biomass and promote better utilization of pyrolysis products.
The pyrolysis behavior of corn stover and polypropylene during co-pyrolysis was studied using a tube furnace reactor. The effects of mixing ratio of corn stover and polypropylene, pyrolysis temperature, addition amount of catalyst (HZSM-5) and reaction atmosphere (N2 and CO2) on the properties of pyrolysis products were studied. The results showed that co-pyrolysis of corn stover and polypropylene can increase the yield of pyrolysis oil. When corn stover:polypropylene = 1:3, the yield of pyrolysis oil was as high as 52.1%, which was 4.5% higher than the theoretical value. With the increase of pyrolysis temperature, the yield of pyrolysis oil increased first and then decreased, and reached the optimal yield at 550 °C. The addition of catalyst (HZSM-5) reduced the proportion of oxygenates and promoted the generation of aromatic hydrocarbons. CO2 has a certain oxidation effect on the components of pyrolysis oil, which promoted the increase of oxygen-containing aromatics and the reduction of deoxy-aromatic hydrocarbons. This study identified the theoretical basis for the comprehensive utilization of plastic and biomass energy.