6 May 2020 in Materials
Verified
Journal Article
Open access
PDF file
MGMin Ge
Min Ge
LXLv Xiaoxu
Lv Xiaoxu
HZHao Zhang
Hao Zhang
SYShouquan Yu
Shouquan Yu
ZLZhenxi Lu
Zhenxi Lu
WZWeigang Zhang
Weigang Zhang
Continuous ceramic fiber comprising silicon carbide–zirconium carbide (SiC–ZrC) binary phases was obtained through melt spinning, electron-beam curing and pyrolysis of a pre-ceramic precursor of polyzirconocenecarbosilanes (PZCS). After pyrolysis and heat treatment, ZrC particles with mean diameters of 15–20 nm were formed and homogeneously dispersed in a matrix of fine crystalline β-SiC with an average grain size of 6–10 nm. Concentration of Zr in the fiber varies from 14.88% to 17.45% by mass. Fibers consisting of near-stoichiometric ZrC and SiC with little free carbon can be obtained through pyrolysis decarbonization of the as-cured fiber in hydrogen from room temperature to 1000 °C, and subsequently heat treatment in argon up to 1600 °C for 1 h. High-temperature treatment of these amorphous inorganic fibers leads to crystallization of the binary phases of β-SiC and ZrC. The removal of free carbon under hydrogen results in more rapid growth of β-SiC and ZrC crystals, in which obvious aggregation of the dispersed ZrC particles among the continuous β-SiC matrix can be ascribed to a fast migration of Zr cation.