Continuous ceramic fiber comprising silicon carbide–zirconium carbide (SiC–ZrC) binary phases was obtained through melt spinning, electron-beam curing and pyrolysis of a pre-ceramic precursor of polyzirconocenecarbosilanes (PZCS). After pyrolysis and heat treatment, ZrC particles with mean diameters of 15–20 nm were formed and homogeneously dispersed in a matrix of fine crystalline β-SiC with an average grain size of 6–10 nm. Concentration of Zr in the fiber varies from 14.88% to 17.45% by mass. Fibers consisting of near-stoichiometric ZrC and SiC with little free carbon can be obtained through pyrolysis decarbonization of the as-cured fiber in hydrogen from room temperature to 1000 °C, and subsequently heat treatment in argon up to 1600 °C for 1 h. High-temperature treatment of these amorphous inorganic fibers leads to crystallization of the binary phases of β-SiC and ZrC. The removal of free carbon under hydrogen results in more rapid growth of β-SiC and ZrC crystals, in which obvious aggregation of the dispersed ZrC particles among the continuous β-SiC matrix can be ascribed to a fast migration of Zr cation.
Composite ceramic fibers comprising about 80 wt% boron nitride (h-BN) and 20 wt% Si3N4 were fabricated through melt-spinning, electron-beam curing, and pyrolysis up to 1600 °C in atmospheres of NH3 and N2, using a mixture of poly[tri(methylamino)borazine] (PBN) and polysilazane (PSZ). By analyzing the microstructure and composition of the pyrolyzed ceramic fibers, we found the formation of binary phases including crystalline h-BN and amorphous Si3N4. Further investigations confirmed that this heterogeneous microstructure can only be formed when the introduced ratio of Si3N4 is below 30% in mass. The mean modulus and tensile strength of the fabricated composite fibers were about 90 GPa and 1040 MPa, twice the average of the pure h-BN fiber. The dielectric constant and dielectric loss tangent of the composite fibers is 3.06 and 2.94 × 10−3.