In this article, parameters of Double-Pulse Metal Inert Gas Welding (DP-MIG) was used for minimising a porosity formation in a T-joint fillet weld. AA5083-H112 aluminium alloy (Non-heat treatable series) with the plate thickness of 10 millimetres is base metal for this study. Welding consumables were filler wire ER5356 with a diameter of 1.2 millimetres and shielded by industrial argon gas. Three majorities parameter of DP-MIG were Delta wire feed (m/min), Frequency (Hz) and Duty cycle (%). Measurable signal current pattern and opened porosity on the fractured surface were couple observed to study their relationships. An appropriate image processing technique was employed to quantitative measuring and calculating a size grouping area of several opened porosities overall weld length, precisely. The result found that the optimal was used a low-level of Delta wire feed of 0.8 m/min, a high-level of a frequency of 5.0 Hz, a mid-level of the duty cycle 30 % and a high travel speed 60 cm/min could minimise the porosity formation with complete penetration.
Antibiotic cement spacers (CS) are standard treatment for periprosthetic hip infection. However, complications such as cement spacer fracture and spacer dislocation remain common after surgery. The aim of this study is to investigate the influence of CS geometry design on mechanical strength through finite element analysis and compression load testing. The CS model was generated using the three-dimensional engineering program, and an aluminum molding block was created. The mechanical behavior was analyzed using finite element method (static structural version 2022R1). A compression load test was employed to evaluate both fatigue failure and the ultimate failure load. The femoral neck area experiences the highest Von Mises stress (36.32 MPa) with lowest safety factor (1.37). The femoral head shows the most significant deformation. The designed CS is capable of withstanding repetitive loads of 35-50 kg for a total 600,000 cycles. The ultimate load to failure was 4354 N. The fracture analysis reveals a vertical sharing type at the femora neck and transverse-short oblique type at the proximal stem. The designed CS can withstand the majority of daily activities with 50 % partial weight bearing for patients weighing 70-100 kg. The femoral neck area experiences the highest stress and shear strain. To optimize the geometric design of the CS, the increase in femoral neck-shaft angle and maximizing the femoral neck diameter should be consider.
Periprosthetic femoral fracture (PFF) is well-known complication in cementless hip arthroplasty (HA), especially in the elderly with osteoporosis. To prevent intraoperative PFFs during HA, prophylactic cerclage wiring on the calcar area during femoral broaching and implant insertion is recommended. However, biomechanical data on the benefits of cerclage wiring in osteoporotic bone during impaction are limited and controversial. This study aimed to assess the efficacy of prophylactic double-looped cerclage wiring (PDLCW) during femoral broaching in the osteoporotic bone model with an impaction simulation system. Fifteen osteoporotic femur models were prepared and allocated to three groups; control group (no cerclage), PW group (received PDLCW), and CC+PW group (prepared as having calcar crack and received PDLCW). All femurs were broached under impaction force that sequentially increased until the visible fracture or calcar crack propagation was visible. The primary outcomes were mallet impaction force (MIF-CF) and mallet velocity (MV-CF) at the time of calcar fracture. The secondary outcomes were calcar fracture pattern and subsidence during calcar fracture (S-CF). PW group showed a significant increase in average MIF-CF, by 40.4% and 120.2% (p<0.001) compared to the control and CC+PW groups, respectively. The average MV-CF in PW group was also significantly greater, 13.1% and 64.6% (p<0.001), compared to the control and CC+PW groups, respectively. Control group revealed significantly greater incidence of complete calcar fracture (60% vs. 0% vs. 0%, p = 0.024), and the highest S-CF compared to those in the PW and CC+PW groups (10.6 ± 6.0 mm, 6.7 ± 4.4 mm, and 1.3 ± 2.0 mm, p = 0.020). This study showed that PDLCW significantly improved hoop stress resistance by increasing the calcar fracture threshold related to mallet impaction, decreasing the risk of complete calcar fracture.
This study joins a 20 mm thick 5000-series aluminum alloy using hot-wire insertion combined with narrow-gap laser welding to evaluate the feasibility and welding characteristics of this technique. The findings indicate that weld formation is primarily influenced by the laser energy density and material deposition rate. A strategy for improving weld beads is introduced incorporating a reoriented laser spot during the final pass on narrow-gap joints. This approach improves penetration and produces defect-free joints. The optimal processing conditions result in complete joint formation with four welding passes. Microstructural analysis reveals that the aluminum matrix morphology evolves according to the local thermal history during welding. Measurements show that the weld region is slightly harder than the base metal, whereas slightly lower hardness is observed at the fusion line and inter-pass boundaries, which correlates with the microstructure result.
Laser welding for aluminum alloys has many difficulties. This study joins a 20-mm-thick 5000-series aluminum alloy using hot-wire insertion combined with narrow-gap laser welding to evaluate the feasibility and welding characteristics of this technique. First, an experiment is conducted to analyze weld formation in hot-wire laser welding of aluminum narrow-gap joints. The welds are classified into three categories: lack of fusion, suitable bead formation, and excessive melting. The findings indicate that weld formation is primarily influenced by laser energy density and material deposition rate. Second, a strategy for improving weld beads is introduced that incorporates a reoriented laser spot during the final pass on narrow-gap joints. This approach improves penetration and produces defect-free joints without lack of fusion. The optimal processing conditions result in complete joint formation with four welding passes. Finally, the microstructure and hardness of the aluminum joints are evaluated. Microstructural analysis reveals that the aluminum matrix morphology evolves according to the local thermal history during welding. Measurements show that the weld region is slightly harder than the base metal, whereas slightly lower hardness is observed at the fusion line and inter-pass boundaries, which correlates with the microstructure result.
The aim of this study is to improve cladding process productivity by high production rate with low dilution process by specifying technique as hot-wire GMAW process. The base metal of carbon steel A516 Gr70 was cladded by austenitic stainless steel 309LSi for creating a buttering layer and stainless steel 308LSi for hot-wire filler for topping a cladding layer in a one-pass run. The studied parameters this experiment consist of the feeding ratio of hot wire feeding speed per GMAW wire feeding speed and travel speed. Welding phenomenon during welding was observed by CCD camera with specifying the optical device to see the appropriate condition. The result showed the hot-wire GMAW cladding process could reduce cycle time 3.5 times compare with conventional FCAW cladding process. Moreover, dilution of this process could decrease lower than 15% with acceptable FN 3 on the top of weld surface. Therefore, single pass cladding process achieved by using this method with low dilution by still keep microstructure capability.