To enhance the performance of ultra-high voltage power fittings in severe weather conditions without altering their current structure, the high-strength and toughness aluminum alloys were rationally selected to study the optimization of the die-casting process. This approach aims to improve the overall longevity and function of the power fittings in extreme climates. First of all, the propose of this study is to use the material’s strength–toughness product (STP) concept to evaluate the material stability of the power fitting impact resistance and fatigue toughness in order to determine the appropriate material selection. Secondly, the location of the mold’s sprue and gate was optimized through finite element simulation to prevent gas volume and flow defects during the casting process. This improves the material’s toughness and anti-fatigue failure characteristics of the product. Then, vacuum equipment and a vacuum valve auxiliary system were added based on the existing die-casting machine, and the mold structure was optimized to enable the vacuum die-casting process. Finally, a water-based boron nitride environmentally friendly mold release agent was used to solve demolding difficulties with an A356 aluminum alloy and improve mold lubrication and surface quality. The production of quad-bundled spacers using A356 and vacuum die casting has resulted in parts with a tensile strength of at least 250 MPa and an elongation of no less than 7%. This improvement has laid a foundation for enhancing the operational reliability of existing overhead transmission line fittings.
To address the difficulty of directly measuring the internal conductor temperature and the complex influence of external environmental factors on gas-insulated switchgear (GIS), a three-dimensional thermal–fluid multiphysics coupling model was developed for a 110 kV three-phase common-enclosure GIS disconnect switch. The model incorporates contact resistance heating, natural convection of SF6 gas, wind speed, and solar radiation. The effects of contact resistance and environmental factors on the temperature field distribution were systematically investigated. The results show that an increase in contact resistance significantly raises the conductor temperature, while higher wind speeds effectively reduce the temperature rise of the equipment. Solar radiation substantially increases the enclosure temperature, whereas ambient temperature has little influence on temperature rise. Based on the enclosure temperature rise, a conductor temperature-rise prediction model and a multi-factor correction model were established. Validation results indicate that all models achieved coefficients of determination greater than 0.98, with prediction errors controlled within ±2 °C. The proposed method enables the accurate prediction of conductor temperature under complex environmental conditions and provides technical support for condition monitoring and overheating fault diagnosis of GIS equipment.
We investigate the explosive-rupture behavior of porcelain hollow bushings using a representative 500 kV SF6 incident as the reference case. Finite-element simulations are performed for both the static response and the rupture process. Results show that internal SF6 pressure drives the maximum equivalent (von Mises) stress to the flange, while strain localizes near the bushing mid-span. These findings highlight the cement–grout potting between the porcelain shell and flange, the waterproofing treatment, and the mid-span bonded joint as key manufacturing control points. Dynamic simulations further indicate that comparing the explosive-equivalent energy of the SF6 pressure impulse with the gas expansion (burst) energy enables diagnosis of the failure mode. From the viewpoint of fragment kinetic energy, the analysis indirectly verifies that rupture is initiated by intrinsic porcelain defects and subsequent crack propagation. The simulated fragment morphology and ground dispersion agree with field observations from the actual event, underscoring the critical role of microcracks in brittle fracture. Accordingly, optimizing firing processes to reduce internal cracks and voids—via raw-material control and firing-temperature optimization—is essential for reliability improvement and life extension. The results provide a practical reference for the design and long-term operation of porcelain bushings.
With the development of UHV transmission technology, large-tonnage disc-type suspension porcelain insulators have been widely used. Insulators with cylindrical heads have the advantages of light weight and high strength compared with traditional insulators with conical heads. Cement is an important part of disc-type suspension porcelain insulators. The drying shrinkage of cement can lead to sliding between cement and porcelain. It can also transform the stress distribution of the porcelain, thus influencing the overall long-term mechanical performance of the insulators. In this paper, the effect of the shrinkage of cement on the stress distribution of porcelain insulators was studied by simulation. In addition, the effect of the drying shrinkage rates of cement on insulators with cylindrical and conical heads were compared. The simulation results show that cylindrical-head insulators can better resist the stress change caused by cement shrinkage than the conical-head insulators, which was beneficial to the long-term performance of the insulators. Based on the tensile stress of porcelain parts, the recommended range of the drying shrinkage rate of cement for insulators with cylindrical heads was presented. The research results are of practical value for the selection of cement.
This study primarily simulates the flashover phenomenon between the metal fittings (rods) and the skirt surface (plates) of insulators when water droplets traverse between them under heavy rain conditions. High-speed cameras recorded droplet deformation and breakdown processes, while electric field simulation software modeled the air gap’s electric field distribution. The effects of air gap length, axial position of the water droplet, droplet conductivity, droplet diameter, and voltage polarity on the DC breakdown voltage were analyzed. Results indicate that a larger air gap leads to a greater reduction in droplet breakdown voltage and lower electric field uniformity. The breakdown voltage is essentially independent of changes in the axial position of the droplet and the droplet’s conductivity. The breakdown voltage exhibits no significant correlation with droplet diameter. Droplets rarely break down when voltage is applied to the electrodes, indicating that flashover at the low-voltage end of insulators during rainfall occurs infrequently. This research holds significant importance for elucidating the flashover mechanisms of water droplets at both ends (high-voltage and low-voltage) of the insulators and for guiding the design of external insulation for power equipment.
Sustained winds can induce vibration and fretting wear at the hardware connections of quad-bundle conductors fitted with Stockbridge dampers. We developed a coupled dynamic model to characterize the unsteady flow field, aerodynamic loads, structural response, load transfer, and interface wear of this system. Numerical simulations resolved the instantaneous velocity and vorticity fields around the four sub-conductors and quantified their aerodynamic forces, displacements, accelerations, and dynamic tension. A local contact model combined with Archard’s law was then used to calculate interface forces, relative slip, and cumulative wear. Pronounced wake interference produced nonuniform aerodynamic loading among the sub-conductors. Sub-conductor C3 had the largest along-wind aerodynamic-force RMS (1.836 N), while the along-wind displacement RMS values of C1–C4 were 9.95, 6.63, 10.59, and 5.68 cm, respectively. Along-wind motion dominated vertical motion. The tension of C3 varied from 24.883 to 25.445 N over 2–12 s. Dampers D2 and D4 showed the largest displacement and acceleration responses. Cumulative slips at the damper clamp–conductor interface were 10.797, 15.013, 10.645, and 14.989 μm for D1–D4, respectively, and wear was concentrated at this interface. These results link wake interference to damper-interface loading and provide a basis for optimizing damper placement and assessing transmission-line reliability under sustained winds.