Recovering valuable metals such as Si, Ag, Cu, and Al has become a pressing issue as end-of-life photovoltaic modules need to be recycled in the near future to meet legislative requirements in most countries. Of major interest is the recovery and recycling of high-purity silicon (>99.9%) for the production of wafers and semiconductors. The value of Si in crystalline-type photovoltaic modules is estimated to be ˜$95/kW at the 2012 metal price. At the current installed capacity of 30 GW/yr, the metal value in the PV modules represents valuable resources that should be recovered in the future. The recycling of end-of-life photovoltaic modules would supply >88,000 and 207,000 tpa Si by 2040 and 2050, respectively. This represents more than 50% of the required Si for module fabrication. Experimental testwork on crystalline Si modules could recover a >99.98%-grade Si product by HNO3/NaOH leaching to remove Al, Ag, and Ti and other metal ions from the doped Si. A further pyrometallurgical smelting at 1520ºC using CaO–CaF2–SiO2 slag mixture to scavenge the residual metals after acid leaching could finally produce >99.998%-grade Si. A process based on HNO3/NaOH leaching and subsequent smelting is proposed for recycling Si from rejected or recycled photovoltaic modules.
1 September 2021 in Journal of Hazardous Materials
Tungsten and cobalt can be recovered from cemented tungsten carbide-Co (WC-Co) scraps using a novel process based on roasting of the scraps with Na2CO3 and water leaching of the calcine containing Na2WO4. The process was evaluated at different conditions testing several parameters, including Na2CO3/WC molar ratio 1:1 – 2:1, roasting temperature in the range 400 – 900ºC, roasting time at 1 – 3h, leaching temperature at ambient – 90ºC and leaching time 1 – 3h. Thermodynamic modelling of the roasting and leaching stages using HSC and Stabcal software allowed an understanding of the speciation of the products at different conditions. Subsequent experiments to determine an optimised conditions of both roasting and water leaching were conducted aiming to yield recoveries of both W and Co in solution over 95%. Roasting of the scraps with Na2CO3 at 800ºC in 3h using Na2CO3/WC molar ratio of 1:1 will produce a Na2WO4 which can be easily water leached. Over 95% W was recovered after water leaching the calcines at 60ºC in 3h. Over 94% Co was recovered as soluble CoSO4 using 1M H2SO4 with 1.5M H2SO3 added as a reductant. The double step of CoCO3 precipitation using 1.5M Na2CO3 and conversion to Co(OH)2 using 8M NaOH allows a high purity product (>99.5% purity) to be produced with most of the major impurities as Cr and Fe remaining in the residual Na2CO3 and NaOH liquors. The levels of these major impurities are 0.05% Cr and 0.3% Fe in the final Co hydroxide product.
The processing of Cu, Co, and Zn at the Boleo project in Mexico involves two-stage (oxidation–reduction) leaching to extract a total of 85–88% Cu in 4 h. The first stage is an oxidation leaching using sulphuric acid (120 kg/tonne ore) at an Eh of 900 mV for 2 h. Then, the reduction stage takes place in 2 h with SO2 gas sparging for Mn and Co extraction at an Eh of 350–370 mV. The final extraction rates of metal values are 92% of Mn, 80% of Co, and 60% of Co, respectively, after 4 h of leaching at 70 °C. However, the same metal recoveries were obtained within 2 h using an equal amount of sulphuric acid and the addition of 25 kg of SO2 per tonne of ore in a single stage leaching in this research. In this case, the Fe extracted from the ore as Fe2+/Fe3+ is believed to have acted as an electrochemical couple contiguously leaching the Cu sulphide and Mn oxides, which also increased the Cu recovery as the Cu mineralised mostly intergrowths in these mineral structure matrices. A significant improvement was made in which the leaching time was halved to 2 h compared to 4 h in the previous plant design and current operation, involving the two-stage oxidation–reduction leaching.
12 November 2022 in Journal of Hazardous Materials Advances