Tungsten and cobalt can be recovered from cemented tungsten carbide-Co (WC-Co) scraps using a novel process based on roasting of the scraps with Na2CO3 and water leaching of the calcine containing Na2WO4. The process was evaluated at different conditions testing several parameters, including Na2CO3/WC molar ratio 1:1 – 2:1, roasting temperature in the range 400 – 900ºC, roasting time at 1 – 3h, leaching temperature at ambient – 90ºC and leaching time 1 – 3h. Thermodynamic modelling of the roasting and leaching stages using HSC and Stabcal software allowed an understanding of the speciation of the products at different conditions. Subsequent experiments to determine an optimised conditions of both roasting and water leaching were conducted aiming to yield recoveries of both W and Co in solution over 95%. Roasting of the scraps with Na2CO3 at 800ºC in 3h using Na2CO3/WC molar ratio of 1:1 will produce a Na2WO4 which can be easily water leached. Over 95% W was recovered after water leaching the calcines at 60ºC in 3h. Over 94% Co was recovered as soluble CoSO4 using 1M H2SO4 with 1.5M H2SO3 added as a reductant. The double step of CoCO3 precipitation using 1.5M Na2CO3 and conversion to Co(OH)2 using 8M NaOH allows a high purity product (>99.5% purity) to be produced with most of the major impurities as Cr and Fe remaining in the residual Na2CO3 and NaOH liquors. The levels of these major impurities are 0.05% Cr and 0.3% Fe in the final Co hydroxide product.