Resistance heat aided friction stir welding (RFSW) was utilized in this experiment with the combined effects of friction heating and resistance heating by adding the direct electric current (0-160 A) to the AZ31B magnesium alloy butt joint. The welded joints were described by optical microscope observations. Analysis of the grain boundary character distribution by optical microscope showed that the weld zone defects decreased, and smoother and more compact joint appearance was accessed by combining the direct electric current with the conventional FSW. In addition, raising the value of electric current promoted the joint quality and refined the grain size in the weld nugget zone (WNZ) and thermo mechanically affected zone (TMAZ) dramatically. However, since there are more grain growth and secondary recrystallization in HAZ of RFSW joints, the average grain size is larger than that of conventional FSW joints. The travel speed of 30 mm/min and the current value of 160A were optimum options within the parameters investigated in this work.
High aspect ratio tungsten nanowires have been prepared by selective dissolution of Nickel-aluminum-tungsten (NiAl−W) alloys which were directionally solidified at growth rates varying from 2 to 25 μm/s with a temperature gradient of 300 K·cm−1. Young’s modulus and electrical resistivity of tungsten nanowires were measured by metallic mask template method. The results show that the tungsten nanowires with uniform diameter and high aspect ratio are well aligned. The length of tungsten nanowires increases with prolongation of etching time, and their length reaches 300 μm at 14 h. Young’s modulus of tungsten nanowires is estimated by Hertz and Sneddon models. The Sneddon model is proper for estimating the Young’s modulus, and the value of calculating Young’s modulus are 260–460 GPa which approach the value of bulk tungsten. The resistivity of tungsten nanowires is measured and fitted with Fuchs−Sondheimer (FS) + Mayadas−Shatzkes (MS) model. The fitting results show that the specific resistivity of W nanowires is a litter bigger than the bulk W, and its value decreases with decreasing diameter.
CO2 laser cladding is a type of green remanufacturing technology, which is of many technical advantages in repairing and remanufacturing industry, especially for some large-scale key mining equipment or parts due to its characteristics of high quality, high efficiency and environmental protection (e.g. energy and material saving). In this paper, the chute plate of coal mining scraper is fixed and remanufactured by CO2 laser cladding technique. Ni60, WC, Ni35, IG55 and other composite powders are selected to design and build the gradient functional structure for chute plate in order to improve the reproduced lifetime. A lot of high power low cost CO2 laser cladding tests are carried out on the matrix material (AISI 1040 steel plate) of old attrite chute plate. The optical microscope, SEM, XRD, microhardness test and wear experiment are adopted to analyze the relationships among the laser cladding process, the overlaying composite material, gradient functional structure and mechanical properties of the remanufacturing scraper’s chute plate. The research results show that laser power and scanning speed are the dominant cladding process parameters, which have a significant influence on the geometric dimension (including width and height), dilution rate and hardness of the deposited layer. These composite powders (especially including the rare earth metals) are the key factor to form the gradient functional structure. The laser cladding Ni60 + WC/Ni35/AISI1040 composite gradient functional structure has a reasonable toughness and strength of the transition layer structure, and a high hardness and wear-resistant surface functional layer, so the fixed and remanufactured product has formed good ductile plasticity and wear resistance properties as a result of the gradient functional structure. The unique Ni60 + WC/Ni35/AISI1040 gradient functional structure makes sure that the chute plate of mining scraper has excellent comprehensive performance, which is satisfied with the service requirements of mechanical parts or equipment in the harsh working environment of the mining industry. This research work provides technological guidance for the fix and remanufacturing chute plate, and achieves the goal of low cost, high efficiency and long life reproduced chute plate of mining scraper.
Molten pool uniformity is a prerequisite for wire and arc additive manufacture to achieve a uniform surface appearance. The thermal boundary is a key indicator to evaluate the thermodynamic state of the molten pool. This paper focuses on thermal analysis through finite element simulation and characterizes the thermal evolution of a molten pool during bottom-up deposition. The peak temperature of the substrate plate increases from 375.7 °C to 623.1 °C when peak current increases from 120 A to 180 A. The temperature gradient decreases from 40 °C/mm to 30 °C/mm. Weld speed increases from 0.15 m/min to 0.25 m/min; the temperature gradient is kept at about 30 °C/mm. Dimensionless thermal conductivity, Ge number, is proposed and defined as the criteria to estimate layer size variation. For Ip = 140 A, the average value of the Ge number is 87.7, and it shows the best numerical stability. Dimensionless thermal conductivity, Ge, is proposed and defined as the criteria to estimate the occurrence of layer size variation. Prolonging heating time and increasing cycle frequency, Ge number shows favorable stability during bottom-up deposition. The experimental results are consistent with analytical conclusions, which proves the validity of the Ge number as an indicator of deposition stability.
1 November 2020 in The International Journal of Advanced Manufacturing Technology
In order to adapt to the development trend of a lightweight automobile and meet the safety requirements of key automotive parts, it is necessary to study the relationship between microstructure and mechanical properties of the dissimilar and different thickness materials welded joint. In this work, a dissimilar welded joint of high strength vehicle steel ASSAPH440 with 2.0 mm thickness/galvanized cold rolled sheet DC52D+ZF45 with 2.6 mm thickness formed by CO2 laser welding was studied. The microstructure of the welded joint was analyzed by metallographic structure and mechanical properties were discussed in terms of their tensile strength and microhardness. The results indicated that a high-quality welded joint with an average tensile strength of 643 MPa and an elongation of 22.7% was obtained at a welding speed of 30 mm s−1 and the laser power of 2200 w in CO2 laser welding, the tensile strength of laser welded joint was more than that of the both based metals. The center of the welding seam was composed of slender lath martensite with a few small white pieces of ferrite. The microstructure of the Heat Affected Zone (HAZ) on the DC52D+ZF45 side was smaller than that of the HAZ on the ASSAPH440 side, and its mechanical properties were superior. The highest microhardness was obtained at the center of the cross section of the welding seam, and the microhardness of the welding seam on the DC52D+ZF45 side was higher than that of the welding seam on the ASSAPH440 side. The tensile fracture appeared at the base metal of DC52D+ZF45 steel as a result of the strength of ASSAPH440 was more than that of DC52D+ZF45. The performance of the laser welded joint met the technical requirements of automobile manufacturing engineering.