Ferritic high-Si ductile cast irons replace an unstable mixed ferrite-pearlite matrix with a unique combination of high elongation, strength and hardness (ideal for automotive drive train components) and resistance to oxidation and corrosion at high temperatures (automotive exhaust and turbocharger systems). The present paper analyses the graphite parameters of 4.5%Si, un-inoculated ductile cast iron (4.7%CE, 0.035%Mgres) as an effect of the casting section size. The structure is characterized by 10.5–11.2% graphite and 464–975 nodules/mm2, at more than 70% ferrite and no carbides, including at 3 mm wall thickness. The lower the wall thickness is, the higher the nodule count is and, consequently, the higher the ferrite amount is. The Roundness Graphite Shape Factor (RSF = 0.65–0.68) illustrates the presence of Slightly Irregular Spheroidal Graphite (Form V ISO 945). There is a big difference between the graphite nodularity evaluated according to ISO 16112:2017 [CGI] (NG1 = 79–86%) and according to ISO 945-4-2019 (DI) (NG2 = 65.2–74.6%), both of them based on RSF. Graphite Nodularity (NG3), calculated with the ISO 945-4-2019 [DI] formula, but replacing RSF with SSF, Sphericity Graphite Shape Factor, has an intermediary position. The higher the imposed minimum RSF or SSF is, the lower the Graphite Nodularity (NG4, NG5): 80–90% for min. 0.50 (minimum Form IV or Intermediate Graphite), 60–80% for min. 0.60–0.65 (minimum Form V graphite) and 35–70% for min. 0.80 (minimum Form VI graphite). The SSF is more representative than the RSF for Si-alloyed ductile cast iron, so it is recommended to use a graphite nodularity calculus considering SSF instead of the RSF formula (stipulated by ISO 945-4-2019), with SSF replacing RSF.
In recent years, high-Si ductile cast irons (3–6% Si) have begun to be used more and more in the automotive and maritime industries, but also in wind energy technology and mechanical engineering. Si-alloyed ferrite has high strength, hardness and oxidation and corrosion resistance, but it has low ductility, toughness and thermal conductivity, with graphite as an important influencing factor. In this study, 4.5% Si uninoculated ductile iron solidified in thin wall castings (up to 15 mm section size) via a permanent (metal) mold versus a sand mold, was evaluated. Solidification in a metal mold led to small size, higher graphite particles (less dependent on the section size). The graphite particles’ real perimeter was 3–5% higher than the convex perimeter, while the values of these parameters were 41–43% higher in the sand mold. Increasing the casting section size led to an increased graphite perimeter, with it being much higher for sand mold. The graphite particles’ shape factors, involving the maximum and minimum size, were at a lower level for metal mold solidification, while by involving the difference between Pr and Pc, is higher for the metal mold. The shape factor, including the graphite area and maximum size, had higher values in the metal mold, sustaining a higher compactness degree of graphite particles and a higher nodularity regarding metal mold solidification (75.5% versus 67.4%). The higher was due to the graphite compactness degree level (shape factor increasing from 0.50 up to 0.80), while the lower was due to the graphite nodularity for both the metal mold (39.1% versus 88.5%) and the sand mold (32.3% versus 83.1%). The difference between the metal mold and sand mold as the average graphite nodularity increased favored the metal mold.
The solidification cooling curve itself as well as its first derivative, and related temperatures, reported to the calculated equilibrium temperatures in stable and metastable solidification systems, are used to predict the solidification characteristics of the cast iron. Silicon, as the most representative cast iron element, and inoculation, as graphitizing metallurgical treatment, have a major influence on the transition from the liquid to the solid state. Six experimental programs are performed, with Si content typically for non-alloyed (<3.0% Si), low (3.0–3.5% Si) and medium alloyed (4.5–5.5% Si) ductile cast irons, as Si-content increasing, and inoculation simultaneous effects. Silicon is an important influencing factor, but the base and minor elements also affect the equilibrium eutectic temperatures, much more in the Fe-C-Si-Xi stable system (15–20 °C) than in the metastable system (5–10 °C), comparing with their calculation based only on a Si effect (Fe-C-Si system). The highest positive effect of inoculation is visible in non-Si alloyed cast irons (2.5% Si): 9–15 °C for the eutectic reaction and 3 to 4 times increased at the end of solidification (37–47 °C). Increased Si content decreases inoculation power to 7–9 °C for low alloying grade (up to 3.5% Si), with the lowest contribution at more than 4.5% Si (0.3–2.0 °C). 2.5–3.5% Si ductile cast irons are more sensitive to high solidification undercooling, especially at the end of solidification (but with a higher efficiency of inoculation), compared to 4.5–5.5% Si ductile cast irons, at a lower undercooling level, and at lower inoculation contribution, as well.
The main objective of the present paper is to evaluate by thermal (cooling curve) analysis the solidification pattern and the occurrence of the layer of degenerate graphite at the surface of ductile iron castings (3.15% Si, typically as 450-18 grade, ISO 1563/2011), with or without a mold coating, including S or O, and different agents (carbonic material, iron powder), supposed to act to block their diffusion into the iron melt. It is found that the mold coating materials temperately influence the parameters of the solidification cooling curves and, more visibly, the occurrence and the thickness of the undesired skin layer. Different graphite morphologies comparable to the casting body are present, at a large range of thicknesses, from 50 up to 200 µm. The sulfur presence in the mold coating will promote a higher skin thickness compared to oxygen (up to 50% by oxygen and 2.5–3.3 times for sulfur action), despite the fact that in the casting body, the graphite nodularity undergoes a limited decrease (from 85% up to 82%–83% level). Carbonic material or iron powder supplementary addition decreases these undesired effects, but the solidification undercooling compared to the equilibrium system is increased. It is found that carbonic material is more efficient at limiting oxygen than iron powder is at limiting the negative effects of sulfur on the casting skin thickness. More experiments are necessary to quantify their capacity to block the oxygen or sulfur transfer into the iron melt.
Having established that sulphur presence in the mould materials appears to have an important contribution in graphite degeneration at least in the casting surface layer, a research program is undertaken to explore the possible beneficial effect of sulphur diffusion blocking at the metal–mould interface. Test samples, with and without a thin steel sheet (up to 3 mm thickness) application on the inner surface of the mould cavity, before iron melt pouring, are considered for structure analysis. A higher nodulizing potential (0.048% Mgres, 0.015% Ceres, and 0.006% Lares) decreases the occurrence of surface graphite degeneration in castings obtained in rigid chemically bonded resin sand moulds, using P-toluol sulfonic acid (PTSA) hardener (S-including), but it is not enough to avoid this phenomenon (200–400 μm skin in present experimental conditions). The casting skin appears to have different values, depending on the evaluation technique (un- and Nital-etching direct measurement, or graphite parameters variation on the casting section). In the presence of a thin steel sheet at the metal–mould interface, the casting skin thickness decreases or is just excluded. It is supposed that it acts as a barrier, blocking S-diffusion from the mould media into the iron melt. Without this S-diffusion, the graphite degeneration in the casting surface layer could be avoided, or at least diminished. For industrial application, the increasing of residual content of nodulizing elements is a limited solution, and it is recommended to use barriers to block S transfer on the mould/metal surface, such as dense coatings or coatings with desulphurization capacity.
28 December 2022 in Journal of Thermal Analysis and Calorimetry