23 September 2019 in Materials
Verified
Journal Article
Open access
PDF file
HDHailiang Du
Hailiang Du
NTNing Tan
Ning Tan
LFLi Fan
Li Fan
JZJiajie Zhuang
Jiajie Zhuang
ZQZhichao Qiu
Zhichao Qiu
Yanhua LeiYanhua Lei
Yanhua Lei
The diffusion coatings were deposited on commercially pure Ti and Ti-6Al-4V alloy at up to 1000 °C for up to 10 h using the pack cementation method. The pack powders consisted of 4 wt% Al (Al reservoir) and 4 wt% NH4Cl (activator) which were balanced with Al2O3 (inert filler). The growth kinetics of coatings were gravimetrically measured by a high precision balance. The aluminised specimens were characterised by means of scanning electron microscopy (SEM), energy dispersive spectrometer (EDS) and X-ray diffraction (XRD). At the early stages of deposition, a TiO2 (rutile) scale, other than aluminide coating, was developed on both materials at <900 °C. As the experimental temperature arose above 900 °C, the rutile layer became unstable and reduced to the low oxidation state of Ti oxides. When the temperature increased to 1000 °C, the TiO2 scale dissociated almost completely and the aluminide coating began to develop. After a triple-layered coating was generated, the coating growth was governed by the outward migration of Ti species from the substrates and obeyed the parabolic law. The coating formed consisted of an outer layer of Al3Ti, a mid-layer of Al2Ti and an inner layer of AlTi. The outer layer of Al3Ti dominated the thickness of the aluminide coating.

1 January 2022 in Science and Engineering of Composite Materials
Verified
Journal Article
Open access
PDF file
QCQizheng Cao
Qizheng Cao
LFLi Fan
Li Fan
HCHaiyan Chen
Haiyan Chen
YHYue Hou
Yue Hou
LDLihua Dong
Lihua Dong
ZNZhiwei Ni
Zhiwei Ni
In order to evaluate the effect of rare earth Y 2 O 3 on the wear and corrosion properties of WC–Ni composite coatings, X-ray diffraction, scanning electron microscopy(SEM), electrochemical polarization curve, electrochemical impedance spectroscopy (EIS), and friction and wear tests were used to analyze the metallographic structure, corrosion characteristics in simulated seawater and friction and wear principle of the composite coatings. Results of SEM revealed that the microstructure of the Y 2 O 3 added coatings was refined with the grains changing smaller and the impurity disappearing. The EIS results proved that the addition of Y 2 O 3 brought a positive influence on the corrosion resistance by reducing the capacitance and increasing the R f and R c . The hardness of the coatings with Y 2 O 3 addition tends to be smooth without wild fluctuation, and the coating with 0.5 wt% Y 2 O 3 owned the hardness values reaching 850 HV. With the addition of rare earth elements, the coefficient of fiction values decreased, reaching the lowest (0.3418) at the content of Y 2 O 3 of 0.5 wt%. The surface of the coating without Y 2 O 3 appears grooved due to the abrasive wear; the coatings with Y 2 O 3 did not suffer serious wear and tear. The coating with 0.5 wt% Y 2 O 3 exhibited the best corrosion resistance and wear resistance properties in all the specimens.

1 January 2022 in High Temperature Materials and Processes
Verified
Journal Article
Open access
PDF file
QCQiZheng Cao
QiZheng Cao
LFLi Fan
Li Fan
HCHaiyan Chen
Haiyan Chen
YXYuRong Xu
YuRong Xu
LDLiHua Dong
LiHua Dong
To investigate the corrosion behavior of WC–Co composite coating, plasma transferred arc (PTA) welding was applied to prepare WC–Co coating on hull steel EH40 for achieving good metallurgical bonding. The phases of coatings were mainly composed of WC particles, solid solution γ-Co, Fe 3 Ni 2 , SiO 2 and Mo 2 C. After electrochemical test, it can be concluded that Co-based coating with 45% WC content has better corrosion resistance in low temperature marine environment for obtaining denser oxide film. Through X-ray photo electron spectroscopy (XPS) analysis, the main corrosion products of immersion were Co(OH) 2 and Co 3 O 4 . These corrosion products aggregate to form a stable corrosion product film, which plays some protective role for the coating. Hard particle WC is also partially oxidized to WO 3 . The pitting hole of 60% WC is the most serious. Pitting corrosion is easy to occur at the interface defects.

1 January 2022 in High Temperature Materials and Processes
Verified
Journal Article
Open access
PDF file
XWXinwang Wang
Xinwang Wang
LFLi Fan
Li Fan
YXYurong Xu
Yurong Xu
HCHaiyan Chen
Haiyan Chen
QCQizheng Cao
Qizheng Cao
YQYujiang Qin
Yujiang Qin
In this paper, four kinds of coatings Ni + 30% WC, Ni + 15% WC, Ni, and Co are prepared on EH40 steel by laser cladding technology. Electrochemical experiment tests at a simulating low-temperature (–40°C) environment in 0.5 mol·L −1 hydrochloric acid (HCl) solution and 3.5 wt% NaCl solution were conducted, and the polarization curve and electrochemical impedance spectroscopy (EIS) impedance spectrum were obtained. The results show that the Ni + 15% WC coating has the smallest corrosion current and 0.5 mol·L −1 HCl solution and 3.5 wt% NaCl solution have the maximum polarization resistance and impedance arc. Coatings will be treated in a 0.5 mol·L −1 HCl solution and 3.5 wt% NaCl solution at –40°C immersion for 30 days; finally, X-ray photoelectron spectroscopy (XPS) and scanning electron microscope (SEM) were used for test passivation films of Ni + 15% WC samples and sample surface morphology after corrosion. XPS results show that Fe, Mo, and Ni elements can form metal oxides in the 0.5 mol·L −1 HCl solution, and Cr, Fe, Mo, Ni, and W elements can form metal oxides in the 3.5 wt% NaCl solution. SEM results display that relatively severe corrosion appeared on the substrate near tungsten carbide in a 0.5 mol·L −1 HCl solution, and coating will be corroded form inside of the coating owing to the corrosive solution will penetrate the substrate. In 3.5 wt% NaCl solution, severe corrosion of the substrate has not been observed; however, the binding part has been obviously corroded.

27 September 2023 in Materials
Verified
Journal Article
Open access
PDF file
LFLi Fan
Li Fan
HCHaiyan Chen
Haiyan Chen
GZGuangkuo Zhu
Guangkuo Zhu
QCQizheng Cao
Qizheng Cao
LDLihua Dong
Lihua Dong
Three groups of spherical WB-reinforced Co-based coatings (Co coating, Co + 15%WB coating, Co + 45%WB coating) were fabricated by laser-cladded technology. The microstructure and constituent phase of spherical WB-reinforced Co-based coatings were examined through scanning electron microscopy (SEM) with energy dispersive spectrometry (EDS) and X-ray diffraction (XRD). The low-temperature tribological properties were analyzed by coefficient of friction, 2D and 3D profiles across the wear track, and wear surface morphology, respectively. The results showed that the phases in the WB-reinforced Co-based coatings are mainly γ-Co, carbides Cr23C6 and Cr7C3, WB, and WO3. Under dry sliding friction at −20 °C, the more spherical WB, the lower the friction coefficient. The wear rate of Co + 45%WB coating was as low as 3.567 × 10−4 mm3/N·m−1, indicating the outstanding wear resistance. Abrasive wear was observed on the rough surface of the WB-added coatings. Compared with dry sliding, due to the plastic deformation of micro-convexes and lubrication function in the 3.5 wt.% NaCl solution, the wear tracks on the surfaces of the three tested coatings were shallower, exhibiting distinct elongated plough grooves.

1 January 2024 in Strength of Materials
Verified
Journal Article
Closed access
PDF file
GZG. K. Zhu
G. K. Zhu
HCH. Y. Chen
H. Y. Chen
LFLi Fan
Li Fan
LHL. L. Han
L. L. Han
YSY. L. Shen
Y. L. Shen
LDL. H. Dong
L. H. Dong