A low cost composite material was synthesized for neodymium recovery from dilute aqueous solutions. The in-situ production of the composite containing chitosan and iron(III) hydroxide (ChiFer(III)) was improved and the results were compared with raw chitosan particles. The sorbent was characterized using Fourier transform infrared spectroscopy (FTIR) and scanning electron microscopy-energy dispersive X-ray analyses (SEM-EDX). The equilibrium studies were performed using firstly a batch system, and secondly a continuous system. The sorption isotherms were fitted with the Langmuir, Freundlich, and Sips models; experimental data was better described with the Langmuir equation and the maximum sorption capacity was 13.8 mg g-1 at pH 4. The introduction of iron into the biopolymer matrix increases by four times the sorption uptake of the chitosan; the individual sorption capacity of iron (into the composite) was calculated as 30.9 mg Nd/g Fe. The experimental results of the columns were fitted adequately using the Thomas model. As an approach to Nd-Fe-B permanent magnets effluents, a synthetic dilute effluent was simulated at pH 4, in order to evaluate the selectivity of the sorbent material; the overshooting of boron in the column system confirmed the higher selectivity toward neodymium ions. The elution step was carried out using MilliQ-water with the pH set to 3.5 (dilute HCl solution).
Torrefaction of almond shells and olive stones, which are typically considered agricultural waste in the southern regions of the European Union, was investigated in this work for application as reducing agents in the metallurgical industry. Four different temperatures were tested: 250, 280, 300 and 350 °C. The evolution of the solid yields with the temperature was determined with TGA measurements. This showed that the duration of torrefaction should not exceed 45 min. The kinetic profiles were successfully fitted using the pseudo-first-order rate equation (PFORE). Then, torrefaction for 45 min was systematically carried out at every temperature and for each resource in a laboratory-scale batch device. The raw and torrefied biomasses were characterized using proximate, ultimate and calorific analyses. The carbon/oxygen ratio and the heating values were increased as a result of the torrefaction severity (from 20 MJ/kg for both raw biomasses to 30 MJ/kg at 350 °C). The highest mass losses were obtained at the highest temperature (67.35 and 65.04 %w for almond shells and olive stones, respectively, at 350 °C). The fixed carbon value also increased, being higher than 67 %w for torrefaction at 350 °C. The large-scale torrefaction at 350 °C (45 min) of these biomasses was carried out in a continuous pilot plant. The solids were characterized as well, and their properties were close to those of the biomasses torrefied in the laboratory-scale batch reactor under the same conditions. This thermal treatment provided biochars with all the required properties to be used as reducing materials in metallurgy.