This study investigates the feasibility of using bauxite residue (BR) as supplementary cementitious material (SCM) for the cement and concrete industry. It is shown from pastes of BR and calcium hydroxide, that BR is highly pozzolanic in nature. The early hydration of cement pastes with BR is accelerated while long-term strength is reduced probably due to the alkaline nature of BR. To be used as cement replacement material in concrete, attempts have been made to reduce the alkali content of BR, in particular to reduce the chance of alkali-aggregate reactions. Co-calcination of BR with kaolin or washing and cooking of BR with calcium hydroxide or calcium hydroxide and gypsum resulted in considerable reduction of alkali content; up to 75%. At the same time the reactivity of the BR was reduced but still being higher compared to fly ash already used in the cement industry.
Calcium oxide (CaO), also known as burnt lime, is being considered as a possible treatment to reduce the negative impact of sea urchins on tare forests in northern coastal waters and blue-green algal blooms in the surrounding of fish-farms. In this respect, the reaction kinetics of burnt lime in contact with sea water has been elucidated and compared to its behaviour in fresh water. In the first minutes of contact between burnt lime and water, it “slaked” as CaO reacted with water to yield calcium hydroxide (Ca(OH)2). Subsequently, calcium hydroxide reacted with magnesium, sulphate and carbonate from the sea water to yield magnesium hydroxide (Mg(OH)2), calcium sulphate dihydrate (gypsum, CaSO4·2H2O) and calcium carbonate (CaCO3), respectively. In a closed system of 1% CaO in natural sea water (where the supply of sulphate, magnesium and carbonate is limited), more than 90% reacted within the first 5 h. It is foreseen that in an open system, like a marine fjord, it will react even faster. The pH 8 of sea water close to the CaO particle surface will immediately increase to a theoretical value of about 12.5 but will, in an open system with large excess of sea water, rapidly fall back to pH 10.5 being equilibrium pH of magnesium hydroxide. This is further reduced to <9 due to the common ion effect of dissolved magnesium in sea water and then be diluted to the sea water background pH, about 8. Field test dosing CaO particles to sea water showed that the pH of water between the particles stayed around 8.
Calcined clays are gaining increasing interest as future supplementary cementitious materials for the production of blended cements. Besides the mineralogy, the right production conditions can affect the pozzolanic activity of calcined clays. In this paper, the pozzolanic reactivity of two calcined natural clays in dependence of burning temperature, residence time in the furnace, cooling conditions and particle size of the final product is investigated. The highest pozzolanic reactivity was found at calcination temperatures between 600 and 800°C. While different cooling conditions had no identified effect on reactivity, decreased particle size and residence time increased the reactivity.
The effect of calcium nitrate (CN) dosages from 0 to 3% (of cement mass) on the properties of fresh cement paste rheology and hardening processes and on the strength of hardened concrete with two types of limestone-blended composite cements (CEM II A-LL 42.5 R and 42.5 N) at different initial (two-day) curing temperatures (−10 °C to +20 °C) is presented. The rheology results showed that a CN dosage up to 1.5% works as a plasticizing admixture, while higher amounts demonstrate the effect of increasing viscosity. At higher CN content, the viscosity growth in normal early strength (N type) cement pastes is much slower than in high early strength (R type) cement pastes. For both cement-type pastes, shortening the initial and final setting times is more effective when using 3% at +5 °C and 0 °C. At these temperatures, the use of 3% CN reduces the initial setting time for high early strength paste by 7.4 and 5.4 times and for normal early strength cement paste by 3.5 and 3.4 times when compared to a CN-free cement paste. The most efficient use of CN is achieved at −5 °C for compressive strength enlargement; a 1% CN dosage ensures the compressive strength of samples at a −5 °C initial curing temperature, with high early strength cement exceeding 3.5 MPa but being less than the required 3.5 MPa in samples with normal early strength cement.
1 January 2012 in Reviews in Mineralogy and Geochemistry
The world’s Portland cement production is the third largest emitter of anthropogenic CO2 after heating/cooling of houses and transport. If no measures are taken, 1 tonne of CO2 is emitted per tonne of clinker produced, where 60% comes from the raw meal (i.e., decomposition of limestone) and 40% from the fuel (most commonly coal). Limestone is the dominating calcium oxide source of Portland cement clinker consisting of about 60% CaO, and hence the cement plants are located near a limestone deposit as limestone constitutes about 80% of the raw meal fed to the rotating kiln for clinker production. In many areas, good limestone sources are close to depletion for several reasons (e.g., MgO should be < 5% in cement clinker), and the objective of this MSA short course contribution was to see if there are other Ca-bearing natural minerals available that can replace limestone, in particular non-carbonaceous minerals that also will lead to a reduction in CO2 emissions. The conclusion is that there is no material as widespread and abundant as limestone that can replace it on a global basis. However, there are some minerals in large deposits locally that may be utilized when new cement plants are to be localized. The most promising being wollastonite (CaSiO3) that also often occur together with limestone. The second being larnite (Ca2SiO4), but it only occurs in few places. Another mineral, anorthite (CaAl2Si2O8), is too high in alumina to play a significant role in Portland cement clinkering, and is also not of interest in calcium aluminate and calcium sulfoaluminate cements due to too high silica content. As a curiosity, gypsum may replace limestone in Portland cement clinkering, but then sulfur dioxide (SO2) is released rather than CO2, which in turn may be used for production of sulfuric acid. However, the demand of sulfuric acid is much less than the demand of Portland cement on a world basis, so this route is not viable and sulfuric acid can be obtained much cheaper from other routes (e.g., roasting sulfide ore).