Alexey Kulebyakin

Dr. Alexey Kulebyakin

orcid

Research Focus & Metrics

Academic Career Length

19Years (2008-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 June 2020 in Journal of Luminescence
Verified
Journal Article
Closed access
Dmitrii AgarkovDmitrii Agarkov
Dmitrii Agarkov
Mikhail BorikMikhail Borik
Mikhail Borik
TVTatyana V. Volkova
Tatyana V. Volkova
GKGalina Korableva
Galina Korableva
AKAlexey Kulebyakin
Alexey Kulebyakin
NTNataliya Tabachkova
Nataliya Tabachkova

6 June 2023 in Membranes
Verified
Journal Article
Open access
PDF file
Dmitrii AgarkovDmitrii Agarkov
Dmitrii Agarkov
Mikhail BorikMikhail Borik
Mikhail Borik
BKBoris Komarov
Boris Komarov
GKGalina Korableva
Galina Korableva
AKAlexey Kulebyakin
Alexey Kulebyakin
NTNataliya Tabachkova
Nataliya Tabachkova
The effect of high-temperature aging for 4800 h at a temperature of 1123 K on the crystal structure and the conductivity of (ZrO2)0.90(Sc2O3)0.09(Yb2O3)0.01 and (ZrO2)0.90(Sc2O3)0.08(Yb2O3)0.02 single-crystal membranes were studied. Such membrane lifetime testing is critical to the operation of solid oxide fuel cells (SOFCs). The crystals were obtained by the method of directional crystallization of the melt in a cold crucible. The phase composition and structure of the membranes before and after aging were studied using X-ray diffraction and Raman spectroscopy. The conductivities of the samples were measured using the impedance spectroscopy technique. The (ZrO2)0.90(Sc2O3)0.09(Yb2O3)0.01 composition showed long-term conductivity stability (conductivity degradation not more than 4%). Long-term high-temperature aging of the (ZrO2)0.90(Sc2O3)0.08(Yb2O3)0.02 composition initiates the t″ → t′ phase transformation. In this case, a sharp decrease in conductivity of up to 55% was observed. The data obtained demonstrate a clear correlation between the specific conductivity and the change in the phase composition. The (ZrO2)0.90(Sc2O3)0.09(Yb2O3)0.01 composition can be considered a promising material for practical use as a solid electrolyte in SOFCs.

13 November 2022 in Crystals
Verified
Journal Article
Open access
PDF file
Mikhail BorikMikhail Borik
Mikhail Borik
АЧАртём Сергеевич Числов
Артём Сергеевич Числов
AKAlexey Kulebyakin
Alexey Kulebyakin
Elena LomonovaElena Lomonova
Elena Lomonova
MFMilovich Filipp
Milovich Filipp
NTNataliya Tabachkova
Nataliya Tabachkova
The mechanical properties, phase composition and luminescence of (ZrO2)1−x(Sm2O3)x (x = 0.02–0.06) crystals synthesized using directional melt crystallization were studied. The regularities of changes in the phase composition of the crystals depending on samaria concentration were analyzed. Optical spectroscopy showed that Sm ions were incorporated into the ZrO2 crystal lattice in the form of Sm3+. The microhardness of the crystals was shown to increase with Sm2O3 concentration and reached 12.45 GPa for (ZrO2)0.94(Sm2O3)0.06 crystals. The highest fracture toughness of 14.2 MPa∙m1/2 was observed for the crystals containing 3.7 mol.% Sm2O3. The experimental results were analyzed in order to understand the effect of phase composition on the mechanical properties of the crystals. The effect of ionic radii of stabilizing oxide cations (i.e., Y3+, Gd3+ and Sm3+) on the mechanical properties of the materials on the basis of partially stabilized zirconia was also discussed.

1 August 2023 in Membranes
Verified
Journal Article
Open access
PDF file
Dmitrii AgarkovDmitrii Agarkov
Dmitrii Agarkov
Mikhail BorikMikhail Borik
Mikhail Borik
EBEkaterina Buzaeva
Ekaterina Buzaeva
GKGalina Korableva
Galina Korableva
AKAlexey Kulebyakin
Alexey Kulebyakin
DZDenis Zakharov
Denis Zakharov
This paper presents the results of studying the phase composition, luminescent characteristics, and ionic conductivity of ceramic scandium-stabilized solid solutions of zirconium dioxide containing 9 and 10 mol% Sc2O3. Ceramic samples were prepared by sintering powders obtained by grinding melted solid solutions of the same composition. A comparative analysis of the obtained data with similar characteristics of single crystals has been carried out. Differences in the phase composition of ceramics and initial single crystals were found. The effect of the structure and properties of grain boundaries on the ionic conductivity of ceramic samples is discussed. It is shown that the differences in the ionic conductivity of ceramic samples and crystals are mainly due to changes in the structure and phase composition.

1 July 2021 in Journal of Alloys and Compounds
Verified
Journal Article
Closed access
SASergey A. Artemov
Sergey A. Artemov
Mikhail BorikMikhail Borik
Mikhail Borik
AKAlexey Kulebyakin
Alexey Kulebyakin
IKIrina E. Kuritsyna
Irina E. Kuritsyna
NLNatalya Larina
Natalya Larina
TVTatyana V. Volkova
Tatyana V. Volkova

12 April 2022 in Modern Electronic Materials
Verified
Journal Article
Open access
PDF file
Dmitrii AgarkovDmitrii Agarkov
Dmitrii Agarkov
Mikhail BorikMikhail Borik
Mikhail Borik
GKGalina Korableva
Galina Korableva
AKAlexey Kulebyakin
Alexey Kulebyakin
Elena LomonovaElena Lomonova
Elena Lomonova
NTNataliya Tabachkova
Nataliya Tabachkova
The phase composition and heat conductivity of (ZrO2)0.9(R2O3)0.1 solid solution single crystals have been studied, where R = (Gd, Yb, Sc, Y), (ZrO2)0.9(Sc2O3)0.09(Gd2O3)0.01 and (ZrO2)0.9(Sc2O3)0.09(Yb2O3)0.01. Single crystals have been grown by directional melt crystallization in a cold skull. The phase composition of the crystals has been studied using X-ray diffraction and Raman spectroscopy. The heat conductivity of the crystals has been studied using the absolute steady-state technique of longitudinal heat flow in the 50–300 K range. We show that at a total stabilizing oxide concentration of 10 mol.% the phase composition of the crystals depends on the ionic radius of the stabilizing cation. The (ZrO2)0.9(Sc2O3)0.1 crystals have the lowest heat conductivity in the 50–300 K range while the (ZrO2)0.9(Gd2O3)0.1 solid solutions have the lowest heat conductivity at 300 K. Analysis of the experimental data suggests that the heat conductivity of the crystals depends mainly on the phase composition and ionic radius of the stabilizing cation. Phonon scattering caused by the difference in the weight of the co-doping oxide cation has a smaller effect on the heat conductivity.