Titanium-copper (Ti–Cu) coatings have attracted extensive attention in the surface modification of industrial and biomedical materials due to their excellent physical and chemical properties and biocompatibility. Here, Ti–Cu coatings are fabricated using a combination of high-power pulsed magnetron sputtering (HPPMS; also known as high power impulse magnetron sputtering (HiPIMS)) and DC magnetron sputtering followed by vacuum annealing at varied temperatures (300, 400, and 500 °C). X-ray diffraction (XRD), transmission electron microscopy (TEM), and X-ray photoelectron spectroscopy (XPS) data showed that Ti, Cu, and CuTi3 are mainly formed in the coatings before annealing, while Ti3O, Cu2O, and CuTi3 are the main compounds present in the annealed coatings. The cross-sectional TEM micrographs and corresponding EDS results provided evidence that Ti is mainly present on the surface and interfaces of the silicon substrate and the Ti–Cu coatings annealed at 500 °C, while the bulk of the coatings is enriched with Cu. The resistivity of the coatings decreased with increasing the annealing temperature from 300 to 500 °C. Based on self-corrosion current density data, the Ti–Cu coating annealed at 300 °C showed similar corrosion performance compared to the as-deposited Ti–Cu coating, while the corrosion rate increased for the Ti–Cu coatings annealed at 400 and 500 °C. Stable release of copper ions in PBS (cumulative released concentration of 0.8–1.0 μM) for up to 30 days was achieved for all the annealed coatings. Altogether, the results demonstrate that vacuum annealing is a simple and viable approach to tune the Cu diffusion and microstructure of the Ti–Cu coatings, thereby modulating their electrical resistivity, corrosion performance, and Cu ion release behavior.
In this study, TiN films doped with different copper contents (TiCuN) were prepared by using direct current magnetron sputtering method. The effects of Cu doping on composition, structure, and mechanical properties of TiN films were studied by energy-dispersive spectroscopy (EDS), X-ray diffraction (XRD), a Vickers microhardnessmeter, and density functional theory (DFT). The results of experimental and DFT study showed that Cu mainly replaced Ti atoms in TiN to form replacement solid solution doping. When Cu replaced Ti in TiN, a weak Cu-N (bond population varied from 0.06 to 0.11) covalent bond formed; meanwhile, the bonding strength of Ti-N (bond population varied from 0.29 to 0.4) bond adjacent to Cu increased. When Cu content was low, a small number of weak Cu-N bonds were formed, with strengthened Ti-N bond near Cu atom, resulting in an increased hardness of Cu doped TiN films. According to the theory of weak bonds, when the Cu content was increased further, the number of weak Cu-N bonds increased and TiCuN hardness decreased. With an increase in Cu content, it was found the toughness of TiCuN also increased. The results of this study will provide a theoretical and experimental guidance for improving the toughness and deformation resistance of TiN, which has a potential application in the surface modification of medical devices.