This study presents relative humidity (RH) sensing response of resistive sensors composed of nanocomposites with oxidized single-wall carbon nanohorns (SWCNHs) and hydrophilic polymers in different ratios at room temperature. The poly(ethylene glycol)-blockpoly(propylene glycol)-block-poly(ethylene glycol) (PEG-PPG-PEG) and polyvinylpyrrolidone (PVP) materials were selected to be the hydrophilic polymers. Two types of nanocomposites with PVP were synthesized, one using SWCNHs/VP at 1/2 (w/w) ratio and another with SWCNHs/PVP in a 1/1 (w/w) ratio. The sensing structure is composed of a Si substrate, a SiO2 layer, and interdigitated (IDT) electrodes, on which the sensing layer is deposited via the drop-casting method. The sensor has a response comparable to that of a commercially available, state-of-the-art, capacitive relative humidity sensor, being characterized by a rapid response time and excellent stability with time. Two sensing mechanisms are considered and analyzed. The first involves the rapid swelling of the host hydrophilic polymer at higher relative humidity levels. The second involves a decrease in the number of holes due to interaction with water molecules, which act as electron donors.
This paper reports, for the first time, on the electrical percolation threshold in oxidized carbon nanohorns (CNHox)–polyvinylpyrrolidone (PVP) films. We demonstrate—starting from the design and synthesis of the layers—how these films can be used as sensing layers for resistive relative humidity sensors. The morphology and the composition of the sensing layers are investigated through Scanning Electron Microscopy (SEM), Atomic Force Microscopy (AFM), and RAMAN spectroscopy. For establishing the electrical percolation thresholds of CNHox in PVP, these nanocomposite thin films were deposited on interdigitated transducer (IDT) dual-comb structures. The IDTs were processed both on a rigid Si/SiO2 substrate with a spacing of 10 µm between metal digits, and a flexible substrate (polyimide) with a spacing of 100 µm. The percolation thresholds of CNHox in the PVP matrix were equal to (0.05–0.1) wt% and 3.5 wt% when performed on 10 µm-IDT and 100 µm-IDT, respectively. The latter value agreed well with the percolation threshold value of about 4 wt% predicted by the aspect ratio of CNHox. In contrast, the former value was more than an order of magnitude lower than expected. We explained the percolation threshold value of (0.05–0.1) wt% by the increased probability of forming continuous conductive paths at much lower CNHox concentrations when the gap between electrodes is below a specific limit. The change in the nanocomposite’s longitudinal Young modulus, as a function of the concentration of oxidized carbon nanohorns in the polymer matrix, is also evaluated. Based on these results, we identified a new parameter (i.e., the inter-electrode spacing) affecting the electrical percolation threshold in micro-nano electronic devices. The electrical percolation threshold’s critical role in the resistive relative-humidity sensors’ design and functioning is clearly emphasized.
Organic–inorganic ternary nanohybrids consisting of oxidized-single walled carbon nanohorns-SnO2-polyvinylpyrrolidone (ox-SWCNH/SnO2/PVP) with stoichiometry 1/1/1 and 2/1/1 and ox-SWCNH/ZnO/PVP = 5/2/1 and 5/3/2 (all mass ratios) were synthesized and characterized as sensing films of chemiresistive test structures for ethanol vapor detection in dry air, in the range from 0 up to 50 mg/L. All the sensing films had an ox-SWCNH concentration in the range of 33.3–62.5 wt%. A comparison between the transfer functions and the response and recovery times of these sensing devices has shown that the structures with ox-SWCNH/SnO2/PVP = 1/1/1 have the highest relative sensitivities of 0.0022 (mg/L)−1, while the devices with ox-SWCNH/SnO2/PVP = 2/1/1 have the lowest response time (15 s) and recovery time (50 s) for a room temperature operation, proving the key role of carbonic material in shaping the static and dynamic performance of the sensor. These response and recovery times are lower than those of “heated” commercial sensors. The sensing mechanism is explained in terms of the overall response of a p-type semiconductor, where ox-SWCNH percolated between electrodes of the sensor, shunting the heterojunctions made between n-type SnO2 or ZnO and p-type ox-SWCNH. The hard–soft acid–base (HSAB) principle supports this mechanism. The low power consumption of these devices, below 2 mW, and the sensing performances at room temperature may open new avenues towards ethanol sensors for passive samplers of environment monitoring, alcohol test portable instruments and wireless network sensors for Internet of Things applications.
We report the relative humidity (RH) sensing response of a resistive sensor, employing sensing layers, based on a quaternary organic–inorganic hybrid nanocomposite comprising oxidized carbon nanohorns (CNHox), graphene oxide (GO), tin dioxide, and polyvinylpyrrolidone (PVP), at 1/1/1/1 and 0.75/0.75/1/1/1 mass ratios. The sensing structure comprises a silicon substrate, a SiO2 layer, and interdigitated transducer (IDT) electrodes. The sensing film was deposited via the drop-casting method on the sensing structure. The morphology and the composition of the sensing layers were investigated through Scanning Electron Microscopy (SEM), X-ray diffraction (XRD), and RAMAN spectroscopy. The organic–inorganic quaternary hybrid-based thin film’s resistance increased when the sensors were exposed to relative humidity ranging from 0 to 100%. The manufactured devices show a room temperature response comparable to that of a commercial capacitive humidity sensor and characterized by excellent linearity, rapid response and recovery times, and good sensitivity. While the sensor with CNHox/GO/SnO2/PVP at 0.75/0.75/1/1 as the sensing layer has the best performance in terms of linearity and recovery time, the structures employing the CNHox/GO/SnO2/PVP at 1/1/1/1 (mass ratio) have a better performance in terms of relative sensitivity. We explained each constituent of the quaternary hybrid nanocomposites’ sensing role based on their chemical and physical properties, and mutual interactions. Different alternative mechanisms were taken into consideration and discussed. Based on the sensing results, we presume that the effect of the p-type semiconductor behavior of CNHox and GO, correlated with swelling of PVP, dominates and leads to the overall increasing resistance of the sensing layer. The hard–soft acid–base (HSAB) principle also supports this mechanism.