This study performed accelerated corrosion tests on reinforced concrete (RC) specimens reinforced with transverse steel bars to evaluate the concrete cracking and rebar strain behaviors caused by rebar corrosion. Seven RC specimens were created with variable compressive strengths, rebar diameters, and concrete cover thicknesses. To mimic in-situ conditions, the accelerated corrosion tests applied a current to the longitudinal bar and transverse bar for different periods of time to create an unbalanced chloride ion distribution. These tests evaluated the amount of rebar corrosion, corrosion cracking properties, and transverse bar strain behavior. The corrosion rate of the transverse bar was faster than that of the longitudinal bar, and cracking first occurred in the concreate around the transverse bar in the specimens with low concrete compressive strength and thin concrete cover. Corrosion cracking and rebar strain were greatly affected by the behavior of the corrosion products that resulted from the pore volume and cracking properties of the cement paste.
This study focused on the quick initial setting time and the expansion strain that occurs during the early aging of α-calcium sulfate hemihydrate (αHH) and examined the setting, compressive strength, and shrinkage strain of αHH-replaced cement mortar. The results show that the initial setting time significantly decreased with an increase in the αHH replacement ratio. Drastic occurrence of ettringite was observed early in the aging of cement mortar when αHH was substituted into the cement; however, the ettringite was not converted to monosulfate with increasing age and thus was not favorable for the development of the compressive strength. When αHH was substituted into cement, using Portland blast-furnace slag cement (PSC) was more advantageous than using ordinary Portland cement (OPC) for the development of the compressive strength. Meanwhile, the expansion of early age αHH can decrease the shrinkage strain of cement mortar. The generation of ettringite is more effective when αHH is substituted into PSC than into OPC and is thus more effective in suppressing the shrinkage strain.
This study evaluates the fracture properties and rear-face strain distribution of nonreinforced and hooked steel fiber-reinforced concrete panels penetrated by projectiles of three different nose shapes: sharp, hemispherical, and flat. The sharp projectile nose resulted in a deeper penetration because of the concentration of the impact force. Conversely, the flat projectile nose resulted in shallower penetrations. The penetration based on different projectile nose shapes is directly related to the impact force transmitted to the rear face. Scabbing can be more accurately predicted by the tensile strain on the rear face of concrete due to the projectile nose shape. The tensile strain on the rear face of the concrete was reduced by the hooked steel fiber reinforcement because the hooked steel fiber absorbed some of the impact stress transmitted to the rear face of the concrete. Consequently, the strain behavior on the rear face of concrete according to the projectile nose shape was confirmed.
In this study, the effect of fine blast furnace slag powder (SP) and limestone powder (LSP) as a mineral admixture in shotcrete using monocalcium aluminate (CA) as a quick-setting accelerator was evaluated. The shotcrete was prepared with up to 25 wt.% substitutions of mineral admixture, i.e., (SP and LSP), and then the CA accelerator was incorporated by 5 wt.% of binders. To examine the optimal mixing ratio for mineral admixture in shotcrete, penetration resistance, compressive strength, XRD analysis, and MIP analysis were performed on the mortar. On the other hand, compressive strength test, chloride diffusion coefficient, and freeze–thaw resistance were conducted on concrete to evaluate the field applicability of shotcrete. The study revealed the addition of LSP improved setting time and early compressive strength while the addition of SP increased long-term compressive strength. With the addition of both SP and LSP, the early and long-term strength was increased due to the influence of the properties of each admixture. Furthermore, the addition of SP and LSP improves the resistance of shotcrete to chloride ions and freeze–thaw.
In this study, high-strength concrete containing hooked-end steel or amorphous metallic fibers was fabricated, and the electrical conductivity and electromagnetic shielding effectiveness were evaluated after 28 and 208 days based on considerations of the influences of the moisture content. Amorphous metallic fibers, which have the same length and length/equivalent diameter ratio as hooked-end steel fibers, were favored for the formation of a conductive network because they can be added in large quantities owing to their low densities. These fibers have a large specific surface area as thin plates. The electromagnetic shielding effectiveness clearly improved as the electrical conductivity increased, and it can be expected that the shielding effectiveness will approach the saturation level when the fiber volume fraction of amorphous metallic fibers exceeds 0.5 vol.%. Meanwhile, it is necessary to reduce the amount of moisture to conservatively evaluate the electromagnetic shielding performance. In particular, when 0.5 vol.% of amorphous metallic fibers was added, a shielding effectiveness of >80 dB (based on a thickness of 300 mm) was achieved at a low moisture content after 208 days. Similar to the electrical conductivity, excellent shielding effectiveness can be expected from amorphous metallic fibers at low contents compared to that provided by hooked-end steel fibers.
About Me
Chungnam National University
Department of Architectural Engineering
Chungnam National University
Department of Architectural Engineering