This article is a response to the state of the art in monitoring the cooling capacity of quenching oils in industrial practice. Very often, a hardening shop requires a report with data on the cooling process for a particular quenching oil. However, the interpretation of the data can be rather difficult. The main goal of our work was to compare various criteria used for evaluating quenching oils. Those of which prove essential for operation in tempering plants would then be introduced into practice. Furthermore, the article describes monitoring the changes in the properties of a quenching oil used in a hardening shop, the effects of quenching oil temperature on its cooling capacity and the impact of the water content on certain cooling parameters of selected oils. Cooling curves were measured (including cooling rates and the time to reach relevant temperatures) according to ISO 9950. The hardening power of the oil and the area below the cooling rate curve as a function of temperature (amount of heat removed in the nose region of the Continuous cooling transformation - CCT curve) were calculated. V-values based on the work of Tamura, reflecting the steel type and its CCT curve, were calculated as well. All the data were compared against the hardness and microstructure on a section through a cylinder made of EN C35 steel cooled in the particular oil. Based on the results, criteria are recommended for assessing the suitability of a quenching oil for a specific steel grade and product size. The quenching oils used in the experiment were Houghto Quench C120, Paramo TK 22, Paramo TK 46, CS Noro MO 46 and Durixol W72.
Microstructure analysis was performed on rolled bars of high-speed steel after two and three forging cycles, each cycle comprising one upsetting and one drawing out operation. High-speed steels belong to difficult-to-form materials with a narrow forging temperature interval. Forging above the maximum forging temperature may lead to grain coarsening. Below the minimum forging temperature, deformation resistance of the material increases, and the workpiece may fail. Using numerical modelling, special forging dies were designed and effective strain distribution was calculated for an axial cross-section plane in specimens after two and three forging cycles. The purpose of the analysis was to identify the relationship between the amount of effective strain and the shape and size of austenite grain and the volume fraction and density of carbides after forging. The size of prior austenite grains was measured using the linear intercept method which is based on the Snyder-Graff method. Grain shapes were characterized in terms of circularity, which is the difference between the shape in question and a circle. With increasing amount of strain, the grains in the material became finer, as undissolved carbides impeded grain growth. In as-received rolled condition, the austenite grain size was G9. After three forging cycles, it was smaller, G11 (the higher the number, the smaller the grains). Circularity characterizes the complexity of a grain shape. Micrographs of carbide particles were taken using a scanning electron microscope and examined with NIS Elements image analysis software. The majority of carbides were sized between 0.2 and 2 μm. The carbides which are less than 1 μm in size do not shrink in response to increasing strain and their quantity does not change appreciably. Carbides with a size of 1-2 μm show a different behaviour. In the central region of specimens, where strain is the largest, their amounts are much larger than in less-worked regions.