20 April 2023 in Journal of Materials Research and Technology
Verified
Journal Article
Open access
LYLingfei Yang
Lingfei Yang
CCChangke Chen
Changke Chen
FYFang Yu
Fang Yu
CCChengcheng Chen
Chengcheng Chen
JLJiangpeng Liu
Jiangpeng Liu
JCJianzhong Cui
Jianzhong Cui

27 June 2024 in Materials
Verified
Journal Article
Open access
PDF file
WSWei Sun
Wei Sun
YZYu Zhang
Yu Zhang
FYFang Yu
Fang Yu
LYLingfei Yang
Lingfei Yang
DSDongfu Song
Dongfu Song
Xiangjie WangXiangjie Wang
Xiangjie Wang
The hot compression simulation testing machine was utilized to conduct compression experiments on an Al-Mg-Si-Mn alloy containing the rare earth element Sc at a deformation temperature ranging from 450 to 550 °C and a strain rate of 0.01 to 10 s−1. The study focused on the hot deformation behavior of the aluminum alloy, resulting in the determination of the optimal range of deformation process parameters for the alloy. The relationship between material flow stress, deformation temperature, and strain rate was described using the Arrhenius relationship containing thermal activation energy based on the stress-strain curve of hot compression deformation of aluminum alloy. This led to calculations for structural factor A, stress index n, and stress level parameters as well as thermal deformation activation energy to establish a constitutive Formula for hot deformation rheological stress of aluminum alloy and calculate the power dissipation factor η. Through this process, an optimized range for the optimal deformation process parameter for aluminum alloy was determined (deformation temperature: 490~510 °C; strain rate: 0.05 s−1) and verified in combination with mechanical properties and microstructure through hot extrusion deformation trial production.

3 January 2023 in Crystals
Verified
Journal Article
Open access
PDF file
Xiangjie WangXiangjie Wang
Xiangjie Wang
YXYajun Xu
Yajun Xu
LYLingfei Yang
Lingfei Yang
CCChengcheng Chen
Chengcheng Chen
ZSZhaoxi Song
Zhaoxi Song
JCJianzhong Cui
Jianzhong Cui
The casting table with lubricating oil and wiper is applied simultaneously to produce super-high-strength 7055 aluminum alloy (Al7055) ingots, and 30 T Al7055 ingots with a diameter of 582 mm were cast successfully. In this study, the microstructure and macrosegregation of the ingots were investigated using an optical microscope (OM). The research results show that the hydrogen content in the liquid metal can be decreased from 0.198 mL/100 g Al to 0.103 mL/100 g Al when three rotors are used in the degassing tank. Compared with the conventional hot-top casting table, the surface quality can be improved by using the casting table with oil lubrication. The temperature gradient between the ingot center and edge can be decreased by using the wiper during the casting process from 320 °C to 150 °C, the cracking tendency caused by the ingot temperature gradient can be decreased, the segregation layer thickness is decreased by about 87%, and the ingot can be homogenized at a high temperature by using the heat of the feed itself.

7 February 2022 in Crystals
Verified
Journal Article
Open access
PDF file
LYLingfei Yang
Lingfei Yang
Xiangjie WangXiangjie Wang
Xiangjie Wang
FYFang Yu
Fang Yu
WSWei Sun
Wei Sun
LLLei Li
Lei Li
JCjianzhong cui
jianzhong cui
Through gradient hot rolling, a transition zone from the initial undeformed to 30% deformed microstructure was obtained in the 6 mm thick 1561 aluminum alloy hot rolled plate. The effect of gradient deformation on the evolution process of structure and texture characteristics to 1561 aluminum alloy were systematically investigated by X-ray diffractometer (XRD), optical microscope (OM), and electron back-scattered diffraction (EBSD) in this paper. The results showed that after gradient hot rolling, the grains were elongated along the rolled direction, and the average grain size decreased from 18.95 μm to 1.19 μm. After annealing, the average grain size decreased from 28.34 μm to 10.69 μm. The fraction of dynamic recrystallization is low in all cases. With the increase in gradient deformation, the fraction of the deformed texture (110) Goss, (110) Brass and fiber texture increased under the action of shear strain, the hardness value of annealed 1561 aluminum alloy ranged from 83.8 HV up to as high as 104 HV, and the electrical conductivity (EC) value increased from 23.5% IACS to 24.3% IACS. Significantly, with the increment of the deformation, the dislocation density increases 2.4 × 1013 m−2 of the annealed hot rolled plates, which should be responsible for the hardness increase. While the structure of the alloy becomes more orderly, the EC increases. Work hardening, fine-grain strengthening and texture all influence the mechanical properties of the gradient hot rolled 1561 aluminum alloy plate.

4 September 2023 in Journal of Materials Science
Verified
Journal Article
Closed access
LYLingfei Yang
Lingfei Yang
FYFang Yu
Fang Yu
CCChengcheng Chen
Chengcheng Chen
YXYajun Xu
Yajun Xu
ZSZhaoxi Song
Zhaoxi Song
XWXiangjie Wang
Xiangjie Wang

26 October 2025 in Materials
Verified
Journal Article
Open access
PDF file
HLHonglei Liu
Honglei Liu
LYLingfei Yang
Lingfei Yang
JLJiangpeng Liu
Jiangpeng Liu
WSWenzhu Shao
Wenzhu Shao
Xiangjie WangXiangjie Wang
Xiangjie Wang
This study examines the microstructure and properties of 7A36 aluminum alloys processed through low-frequency electromagnetic casting (LFEC) with microalloyed Sc. Following secondary hot deformation, the addition of Sc refined the average grain size from 3.8 μm to 0.9 μm and reduced the deformed texture content. In the T6-aged condition, the combined application of Sc and LFEC enhanced the hardness (234 HV to 238 HV), ultimate tensile strength (647 MPa to 693 MPa), and elongation (EL). Fractographic analysis revealed brittle fracture modes dominated by cleavage, with minor intergranular contributions. The corrosion resistance was poorest in the rolled state and superior in the two-stage-aged state. Under two-stage aging, the maximum corrosion depth for the Sc-modified, LFEC-processed alloy decreased from 113.6 to 49.1 μm. The synergistic integration of Sc alloying and LFEC significantly improved both the mechanical properties and corrosion resistance.