3 June 2021 in Polymers
Verified
Journal Article
Open access
PDF file
Mujtahid KaavessinaMujtahid Kaavessina
Mujtahid Kaavessina
SDSperisa Distantina
Sperisa Distantina
Esa ShohihEsa Shohih
Esa Shohih
In this research, a low molecular weight poly(lactic acid) (or PLA) synthesized from direct polycondensation was melt compounded with urea to formulate slow-release fertilizer (SRF). We studied the influence of the molecular weight (MW) of PLA as a matrix and the urea composition of SRF towards release kinetics in water at 30 °C. The physical appearance of solid samples, the change in urea concentration, and acidity (pH) of water were monitored periodically during the release test. Three studied empirical models exhibited that diffusion within the matrix dominated the urea release process, especially when the release level was less than 60%. Thus, a lower MW of PLA and a higher urea content of SRF showed a faster release rate. For the entire length of the release experiment, a combination of diffusion and degradation mechanisms exhibited the best agreement with the experimental data. The hydrolytic degradation of PLA may begin after 96 h of immersion (around 60% release level), followed by the appearance of some micro-holes and cracks on the surface of the SRF samples. Generally, this research revealed the good release performance of urea without residues that damage the soil structure and nutrient balance.

22 March 2022 in Polymers
Verified
Journal Article
Open access
PDF file
MZMohammad Zainudin
Mohammad Zainudin
KDKuncoro Diharjo
Kuncoro Diharjo
Mujtahid KaavessinaMujtahid Kaavessina
Mujtahid Kaavessina
DSDjoko Setyanto
Djoko Setyanto
U UBAIDILLAHU UBAIDILLAH
U UBAIDILLAH
It is difficult to obtain suitable fire resistance and mechanical properties for glass-fiber-reinforced polymer (GFRP) roof material in industrial applications. Although some efforts to improve the fire resistance properties of GFRP have been carried out, in practice this sometimes degrades the mechanical properties. Therefore, the base materials, such as filler and reinforcing fiber, must be appropriately combined to simultaneously improve both fire resistance and mechanical properties. The present study examines improvements in GFRP roof material by investigating the effect of aluminium trihydrate (ATH) as a filler and the combination of a chopped strand mat (CSM) with woven roving (WR) and stitched mat (STM) fibers as the reinforcement in a composite GFRP roof structure. The roof samples were prepared following industrial machine standards using the specified materials. The mechanical properties of GFRP were evaluated using tensile, flexural and impact tests, following ASTM D638, ASTM D790 and ASTM D256 standards, respectively. The fire properties were examined through fire tests following the ASTM D635 standard. The results show that the GFRP roof composed of CSM/WR fibers had a 40% higher tensile strength (103.5 MPa) compared with the GFRP roof without CSM fibers (73.8 MPa). The flexural strength of the GFRP roof with CSM/WR fibers was also 57% higher than the roof without fibers, with a ratio of 315.61 MPa to 201 MPa. With the use of CSM/WR fibers, the fire resistance also increased by 23%, resulting in a ratio of 4.31 mm/min to 5.32 mm/min. These results demonstrate that the combination of CSM/WR fibers as a reinforcement would be an excellent option for producing an improved GFRP roof with better industrial properties, especially when producing improved GFRP roofs using a continuous lamination machine.

1 January 2018 in AIP Conference Proceedings
Verified
Conference Paper
Closed access
PDF file
MZMohammad Zainudin
Mohammad Zainudin
KDKuncoro Diharjo
Kuncoro Diharjo
Mujtahid KaavessinaMujtahid Kaavessina
Mujtahid Kaavessina
DSDjoko Setyanto
Djoko Setyanto
There is much consideration of roof selection as a protector of a building against the outside weather, such as lightweight, strong stiff, corrosion resistant and guarantee for the availability of products. Based on these considerations, glass fiber reinforced polymer (GFRP) roof is a roof which can fulfill the requirement. The objective of this research is to investigate the degradation of physical and mechanical properties of GFRP roof exposed in outside weather. This GFRP roof composite was produced using a sheet molding compound (SMC) supplied by PT Intec Persada, Tangerang, Indonesia. There are two kinds GFRP roofs evaluated in this research that are GFRP roof exposed within 7 years and new GFRP roof that has not been exposed. The GFRP roofs were cut manually for preparing the specimens for hardness test, tensile test, SEM and FTIR test. The results show that the GFRP roof exposed within 7 years had the degradation of properties compared to the new GFRP roof. The exposed GFRP roof had lower strength and hardness compared to the new GFRP roof. The SEM observation indicates that exposed GFRP roof had the debonding of fiber on the surface, and in contrast, there are no debonding of fiber in the new GFRP roof surface. It can be recommended that the exposed GFRP roof may be repaired to enhance its performance and can re-increase its properties using the coating.

9 March 2017 in MATEC Web of Conferences
Verified
Journal Article
Open access
PDF file
Mujtahid KaavessinaMujtahid Kaavessina
Mujtahid Kaavessina
SDSperisa Distantina
Sperisa Distantina
FAFadilah
Fadilah
MATEC Web of Conferences, open access proceedings in Materials science, Engineering and Chemistry

1 January 2016 in AIP Conference Proceedings
Verified
Conference Paper
Closed access
Mujtahid KaavessinaMujtahid Kaavessina
Mujtahid Kaavessina
SDSperisa Distantina
Sperisa Distantina
ACAchmad Chafidz
Achmad Chafidz
FAFadilah
Fadilah
SASaeed M. Al-Zahrani
Saeed M. Al-Zahrani
Poly (lactic acid)/elastomer blends were prepared via direct injection molding with the different weight fractions of elastomer, namely: 0, 10, 20 and 30 wt%. Degradation test of poly (lactic acid) (PLA) was performed by burial in the soil. The physical appearance and thermal properties of the tested specimens were monitored periodically. The presence of elastomer tended to significantly increase the degradability of PLA after buried for 27 weeks. With 30 wt% elastomer, the color and the surface of specimens become more white and rougher due to the degradation. Differential scanning calorimetry (DSC) was used to evaluate thermal properties and crystallinity of all samples. It was found that the melting temperature decreased as the amount of elastomer increased. The crystallinity showed that the degradation of PLA is occurred firstly in amorphous phase.