Herein, we report the impact of plasma on gold nanoparticles synthesis. We used an atmospheric plasma torch fed with an aerosolized tetrachloroauric(III) acid trihydrate (HAuCl4·3H2O) solution. The investigation showed that using pure ethanol as a solvent for the gold precursor enabled a better dispersion compared to a water-containing solution. We demonstrated here that the deposition parameters are easy to control, presenting the influence of solvent concentration and deposition time. The advantage of our method is that no capping agent was used. We assume that plasma creates a carbon-based matrix around the gold nanoparticles preventing them to agglomerate. The XPS results revealed the impact of using plasma. Metallic gold was detected in the plasma-treated sample, whereas the no-plasma sample revealed only Au(I) and Au(III) contributions originating from the HAuCl4 precursor. Detailed HRTEM, EDS mapping, and SAED analyses led to more insights into the structure.
Antiferroelectrics have been recently sparking interest due to their potential use in energy storage and electrocaloric cooling. Their main distinctive feature is antiferroelectric switching, i.e., the possibility to induce a phase transition to a polar phase by an electric field. Here, we investigate the switching behavior of the model antiferroelectric perovskite PbZrO3 using thin films processed by chemical solution deposition in different geometries and orientations. Both out-of-plane and in-plane switching configurations are investigated. The critical field is observed to be highly dependent on the direction of the electric field with respect to the film texture. We show that this behavior is qualitatively consistent with a phase transition to a rhombohedral polar phase. We finally estimate the importance of crystallite orientation and film texturation in the variations observed in the literature.
The catalytic activity of cobalt and iron nanoparticles for the growth of carbon nanotubes (CNTs) was studied by a specific reproducible and up-scalable fabrication method. Co and Fe catalysts were deposited over SiO2 nanoparticles by a wet-impregnation method and two different annealing steps were applied for the catalyst formation/activation. The samples were calcined at an optimal temperature of 450 °C resulting in the formation of metal oxide nano-islands without the detection of silicates. Further reduction treatment (700 °C) under H2 successfully converted oxide nanoparticles to Co and Fe metallic species. Furthermore, the catalytic efficiency of both supported-metal nanoparticles at 2 and 5% in weight of silica was evaluated through the growth of CNTs. The CNT structure, morphology and size dispersion were tailored according to the metal catalyst concentration.