In this study, we report that the carrier mobility of 2%-La-doped BaSnO3 (LBSO) films on (001) SrTiO3 and (001) MgO substrates strongly depends on the thickness, whereas it is unrelated to the film/substrate lattice mismatch (+5.4% for SrTiO3 and −2.3% for MgO). The films exhibited large differences in lattice parameters, lateral grain sizes (∼85 nm for SrTiO3 and ∼20 nm for MgO), surface morphologies, threading dislocation densities, and misfit dislocation densities. However, the mobility dependences on the film thickness in both cases were almost the same, saturating at ∼100 cm2 V−1 s−1, while the charge carrier densities approached the nominal carrier concentration (=[2% La3+]). Our study clearly indicates that the carrier mobility of LBSO films strongly depends on the thickness. These results would be beneficial for understanding the carrier transport properties and fruitful to further enhance the mobility of LBSO films.
La-doped SrSnO3 (LSSO) is known as one of the deep-ultraviolet (DUV)-transparent conducting oxides with an energy bandgap of ∼4.6 eV. Since LSSO can be grown heteroepitaxially on more wide bandgap substrates such as MgO (Eg ∼ 7.8 eV), LSSO is considered to be a good candidate for a DUV-transparent electrode. However, the electrical conductivity of LSSO films is below 1000 S cm−1, most likely due to the low solubility of the La ion in the LSSO lattice. Here, we report that high electrically conducting (>3000 S cm−1) LSSO thin films with an energy bandgap of ∼4.6 eV can be fabricated by pulsed laser deposition on a MgO substrate followed by a simple annealing in vacuum. From the X-ray diffraction and the scanning transmission electron microscopy analyses, we found that lateral grain growth occurred during the annealing, which improved the activation rate of the La ion, leading to a significant improvement of the carrier concentration (3.26 × 1020 cm−3) and Hall mobility (55.8 cm2 V−1 s−1). The present DUV-transparent oxide semiconductor would be useful as a transparent electrode for developing optoelectronic devices, which transmit and/or emit DUV-light.
The exact intrinsic carrier effective mass of a well-studied transparent oxide semiconductor is unknown because the reported values are scattered from to . This paper identifies the intrinsic of , by the thermopower modulation clarification method and determines the threshold of the degenerate/nondegenerate semiconductor. At the threshold, the thermopower values of both the La-doped and thin-film transistor structures are , the bulk carrier concentration is , and the two-dimensional sheet carrier concentration is . When the Fermi energy is located above the parabolic shaped conduction band bottom, the mobility is rather high. In contrast, below the threshold exhibits a very low carrier mobility, most likely because the tail states suppress the carrier mobility. The present results are useful to further develop -based oxide electronics.