Key Laboratory for Special Functional Materials of Ministry of Education, National & Local Joint Engineering Research Center for High-efficiency Display and Lighting Technology, School of Nanoscience and Material Engineering
Auto-generated profile, based on publicly available information
Mian Wei
Key Laboratory for Special Functional Materials of Ministry of Education, National & Local Joint Engineering Research Center for High-efficiency Display and Lighting Technology, School of Nanoscience and Material Engineering
In this study, we report that the carrier mobility of 2%-La-doped BaSnO3 (LBSO) films on (001) SrTiO3 and (001) MgO substrates strongly depends on the thickness, whereas it is unrelated to the film/substrate lattice mismatch (+5.4% for SrTiO3 and −2.3% for MgO). The films exhibited large differences in lattice parameters, lateral grain sizes (∼85 nm for SrTiO3 and ∼20 nm for MgO), surface morphologies, threading dislocation densities, and misfit dislocation densities. However, the mobility dependences on the film thickness in both cases were almost the same, saturating at ∼100 cm2 V−1 s−1, while the charge carrier densities approached the nominal carrier concentration (=[2% La3+]). Our study clearly indicates that the carrier mobility of LBSO films strongly depends on the thickness. These results would be beneficial for understanding the carrier transport properties and fruitful to further enhance the mobility of LBSO films.
La-doped SrSnO3 (LSSO) is known as one of the deep-ultraviolet (DUV)-transparent conducting oxides with an energy bandgap of ∼4.6 eV. Since LSSO can be grown heteroepitaxially on more wide bandgap substrates such as MgO (Eg ∼ 7.8 eV), LSSO is considered to be a good candidate for a DUV-transparent electrode. However, the electrical conductivity of LSSO films is below 1000 S cm−1, most likely due to the low solubility of the La ion in the LSSO lattice. Here, we report that high electrically conducting (>3000 S cm−1) LSSO thin films with an energy bandgap of ∼4.6 eV can be fabricated by pulsed laser deposition on a MgO substrate followed by a simple annealing in vacuum. From the X-ray diffraction and the scanning transmission electron microscopy analyses, we found that lateral grain growth occurred during the annealing, which improved the activation rate of the La ion, leading to a significant improvement of the carrier concentration (3.26 × 1020 cm−3) and Hall mobility (55.8 cm2 V−1 s−1). The present DUV-transparent oxide semiconductor would be useful as a transparent electrode for developing optoelectronic devices, which transmit and/or emit DUV-light.
The electron mobility value of observed from La-doped (LBSO) single crystals has a great potential in optoelectronic applications, but LBSO films exhibit much lower mobilities. Threading dislocations from the film/substrate mismatch are believed to be the main source of this phenomenon, but previous experiments suggest that they do not fully explain the mobility suppression. In this paper, we examined the thickness dependence of electrical and thermal transport properties of LBSO films fabricated in different oxidation environments. The results show that oxygen deficiency also affects the electron mobility of LBSO films, and the mobility suppression in LBSO films is dominated by different mechanisms depending on the thicknesses. LBSO films with different oxygen vacancy contents were fabricated using the pulsed laser deposition technique. The films deposited under higher oxidative conditions exhibited lower oxygen deficiency levels and superior transport properties whereas the threading dislocation densities remained unchanged. The highest mobility value observed in this paper was , which is comparable to LBSO films fabricated on thick buffer layers. Our paper provides a broader perspective on understanding the mobility of LBSO films and confirms that threading dislocations are not the only factor.
8 December 2020 in ACS Applied Electronic Materials